Pavlukovich N.G., Ivanov M.S., Morozova V.S., Bolshakov V.A., Mekalina I.V. Vibration absorbing materials for aircraft. Part 1. Mechanism and research methods for damping of polymeric materials // Proceedings of VIAM. 2026. No. 3 (157). С. 85–96. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-3-85-96.

Vibration absorbing materials for aircraft

Part 1. Mechanism and research methods for damping of polymeric materials
Pavlukovich N.G., Ivanov M.S., Morozova V.S., Bolshakov V.A., Mekalina I.V.
Abstract

The paper studies the problem of acoustic discomfort in an airplane cabin caused by noise of aerodynamic and structural origin. The main attention is paid to the methods of noise reduction using vibration-absorbing materials based on viscoelastic polymers. Physical mechanisms of vibration energy dissipation, in particular relaxation processes, in polymers are considered. Modern methods of investigation of vibration-absorbing characteristics are described, including dynamic mechanical analysis, analysis of amplitude-frequency and amplitude-time dependencies.

Keywords
aircraft noise, damping, vibration absorption, viscoelastic materials, relaxation, polymer composites, noise reduction tests, vibration-damping materials
Reference list
  1. Sagomonova V.A., Sytyi Yu.V., Kislyakova V.I., Dolgopolov S.S. Investigation of the damping properties of vibration-absorbing materials based on thermoplastic elastomers. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 5–10. DOI: 10.18577/2071-9140-2014-0-s3-5-10.
  2. Smith M.J.T. Aircraft noise. New York, USA: Cambridge University Press, 1989, 369 p.
  3. Dennis L. Huff Noise Reduction Technologies for Turbofan Engines. Ohio, USA: National Aeronautics and Space Administration Glenn Research Center Cleveland, 2007, pp. 1–10.
  4. Bogolepov I.I. Industrial Soundproofing. Leningrad: Sudostroenie, 1986, 367 p.
  5. Khaletskiy Yu.D., Pochkin Ya.S. Reducing Aircraft Engine Fan Noise by Tilting Straightener Blades. Akusticheskiy zhurnal, 2015, vol. 61, no. 1, p. 106.
  6. Gaifullin A.M., Golovkin V.A., Golovkin M.A. et al. An Experimental and Computational Approach to Solving the Problem of Wake Vortex Attenuation. Aerodynamics of Aircraft: Proceedings of the XI School-Seminar. Moscow: TsAGI im. N.E. Zhukovsky, 2000, pp. 34–35.
  7. Vasiliev A.V. On the principles of classification of active compensation systems for low-frequency noise and vibration. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2006, no. 4, vol. 8, pp. 1156–1170.
  8. Nashif A., Jones D., Henderson J. Vibration Damping. Trans. from Engl. Moscow: Mir, 1988, 448 p.
  9. Colombo C., Carradó A., Palkowski H. et al. Impact behaviour of 3-layered metal-polymer-metal sandwich panels. Composite Structures, 2015, no. 133, pp. 140–147.
  10. Sokolova O., Carradó A., Palkowski H. Metal-polymer-metal sandwiches with local metal reinforcements: A study on formability by deep drawing and bending. Composite Structures, 2011, vol. 94, is. 1, pp. 1–7.
  11. Shuldeshov E.M., Kraev I.D., Obraztsova E.P. Materials for sound-proof designs of aircraft engines (review). Trudy VIAM, 2021, no. 7 (101), pp. 59–72. Available at: http://www.viam-works.ru (accessed: July 24, 2025). DOI: 10.18577/2307-6046-2021-0-7-59-72.
  12. Sagomonova V.A., Tselikin V.V. Vibration damping material with perforated constraining layer. Aviation materials and technologies, 2023, no. 3 (72), pp. 125–133. Available at: http://www.journal.viam.ru (accessed: July 16, 2025). DOI: 10.18577/2713-0193-2023-0-3-125-133.
  13. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concentration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  14. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2017-9140-2020-0-1-45-53.
  15. Mikhailin Yu.A. Polymer Composite Materials (Reinforced Plastics, VPKM). Tekhnologiya mashinostroyeniya, 2007, no. 3 (57), pp. 5–18.
  16. Mikhailin Yu.A. Structural Polymer Composite Materials. 2nd ed., rev. and add. St. Petersburg: NOT, 2010, 822 p.
  17. Kuleznev V.N., Shershnev V.A. Chemistry and Physics of Polymers. 2nd ed., rev. and add. Moscow: KolosS, 2007, 367 p.
  18. Bergmann J., Stambke M. Potential of Laser-manufactured Polymer-metal hybrid. Joints Physics Procedia, 2012, no. 39, pp. 84–91.
  19. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), pp. 41–50. Available at: http://www.journal.viam.ru (accessed: July 16, 2025). DOI: 10.18577/2713-0193-2022-01-41-50.
  20. Glushchenkov V.A., Palkowski H., Yusupov R.Y. et al. A non-destructive method for evaluating the adhesion between the layers of metal-polymer-metal composite materials. Materiali in Tehnologije, 2024, vol. 58, is. 1, no. 1, pp. 3–8.
  21. Sagomonova V.A., Dolgopolov S.S., Sorokin A.E., Tselikin V.V. Evaluation of vibration-absorbing material based on polyurethane using possibility for a seal. Trudy VIAM, 2021, no. 10 (104), pp. 28–35. Available at: http://www.viam-works.ru (accessed: July 24, 2025). DOI: 10.18577/2307-6046-2021-0-10-28-35.
  22. Kablov E.N., Sagomanova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Study of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9. DOI: 10.31044/1994-6260-2020-0-3-2-9.
  23. Harhash M., Gilbert R.-R., Hartmann S. et al. Experimental characterization, analytical and numerical investigations of metal/polymer/metal sandwich composites – Part 2: free bending. Composite Structures, 2020, vol. 232, pp. 217–228.