Abstract

In cast blades made of heat-resistant nickel alloys with an equiaxed structure for gas turbine units and engines, one of the main defects is shrinkage porosity, which is a stress concentrator, and reduces the properties of the material and the reliability of the blades. In the second part, the results of testing modern methods for minimizing porosity in the manufacture of large-sized blades of gas turbine units at the leading engine-building enterprises of the industry are presented.

Keywords
large-sized cast turbine blades, fine-grained structure, equiaxed structure, porosity, casting feed, casting modes, gas turbine units
Reference list
  1. Kolyadov E.V., Visik E.M., Gerasimov V.V., Bityutskaya O.N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), pp. 15–24. Available at: http://www.journal.viam.ru (accessed: June 06, 2025). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  2. Visik E.M., Bityutskaya O.N., Gerasimov V.V., Pilipenko А.А., Moiseev А.S. Features of production of large casting turbine blades by directional crystallization of nickel corrosion resistеnt superalloy. Aviation materials and technologies, 2025, no. 2 (79), pp. 3–12. Available at: http://www.journal.viam.ru (accessed: June 06, 2025). DOI: 10.18577/2713-0193-2025-0-2-3-12.
  3. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: June 06, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  4. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), pp. 3–16. Available at: http://www.journal.viam.ru (accessed: June 06, 2025). DOI: 10.18577/2713-0193-2023-0-1-3-16.
  5. Kablov E.N. Cast Blades of Gas Turbine Engines: Alloys, Technologies, Coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
  6. Veynik A.I. Casting Calculation. Moscow: Mashgiz, 1964, 403 p.
  7. Kats E.L. Technological Fundamentals of Solidification Control during Gas Turbine Blade Casting: thesis, Doctor Sc. (Tech.). Moscow, 1986, 555 p.
  8. Zhuravlev V.A. On the Macroscopic Theory of Alloy Crystallization. Izvestiya AN SSSR. Ser.: Metally, 1975, no. 5, pp. 93–99.
  9. Zhuravlev V.A., Bakumenko S.P., Ilyin G.A. et al. Formation of defects during crystallization of alloys in a two-dimensional region with a short-lived internal heat current. Izvestiya AN SSSR. Ser.: Metally, 1982, no. 3, pp. 172–173.
  10. Timofeev G.I. Mechanics of alloys during crystallization of ingots and castings. Moscow: Metallurgy, 1977, 160 p.
  11. Leibenzon L.S. Movement of natural liquids and gases in a porous medium. Moscow; Leningrad: Gostekhizdat, 1947, 244 p.
  12. Sobolev V.V., Trofimov P.M. Study of solidification conditions and formation of axial porosity in continuous ingots of club-shaped cross-section. Stal, 1982, no. 4, pp. 28–31.
  13. Katz E.L., Spiridonov E.V. Feeding mechanism for castings made of alloys with a wide range of crystallization temperatures. Trudy NIAT, 1972, no. 2, pp. 2–17.
  14. Spiridonov E.V., Katz E.L. Features of shrinkage compensation in castings made of high-strength alloys. Magnesium alloys in industry. Eds. A.T. Tumanov, M.B. Altman. Moscow: ONTI VIAM, 1972, pp. 65–69.
  15. Przybyl J. Theory of foundry processes. Moscow: Mir, 1967, 328 p.
  16. Veynik A.I. Theory of casting solidification. Moscow: Mashgiz, 1960, 435 p.
  17. Balandin G.F. Fundamentals of the Theory of Casting Formation: in 2 parts. Moscow: Mashinostroenie, 1976, part 1, 328 p.
  18. Neustruev A.A., Pantyukhin V.P. Method for Calculating the Solidification Sequence of Shaped Castings. Mathematical Modeling of Solidification Processes of Metals and Alloys. Novosibirsk: SB AS USSR, 1983, pp. 120–126.
  19. Yakovlev E.I., Berestevich A.I., Sobolev A.A., Zhabrev S.B. Manufacturing of Large-Size Cast Blades for Gas Turbine Units with a Regulated Equiaxed Structure. Liteynoe proizvodstvo, 2018, no. 8, pp. 24–27.
  20. Yakovlev E.I., Berestevich A.I., Zhabrev S.B. Formation of a Regulated Structure of Large-Sized Cast Blades for Gas Turbine Units. Tsvetnye metally, 2018, no. 5, pp. 86–90.
  21. Yakovlev E.I. Production of Castings from Heat-Resistant Nickel Alloys with a Fine-Grained Equiaxed Structure and Reduced Porosity. Liteynoe proizvodstvo, 2022, no. 6, pp. 2–5.