Turchenko M.V., Lebedeva Yu.E., Chaynikova A.S., Butuzov A.V., Gamazina M.V., Svetogorov К.I., Nerush S.V. Production of hydroxyapatite products using additive technologies // Proceedings of VIAM. 2026. No. 2 (156). С. 94–106. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-2-94-106.

Production of hydroxyapatite products using additive technologies

Turchenko M.V., Lebedeva Yu.E., Chaynikova A.S., Butuzov A.V., Gamazina M.V., Svetogorov К.I., Nerush S.V.
Abstract

This review describes in detail the main methods of additive manufacturing (FDM, CJP, SLA, DLP), which make it possible to obtain three-dimensional structures with complex architecture (scaffolds) based on hydroxyapatite. The analysis of scientific information in the field of 3D printing of ceramics based on hydroxyappatite with subsequent application in regenerative medicine is carried out. The relevance of research in the field of obtaining biomedical products based on hydroxyapatite using additive technologies has been assessed.

Keywords
hydroxyapatite, ceramics, laser stereolithography, layer-by-layer deposition, digital light processing, inkjet printing
Reference list
  1. Gurov D.A., Pavlyukovich N.G., Tsapenko A.N. 3D printing with composite organic filament based on liquid crystal polymers and polyetheretherketone. Aviation materials and technologies, 2024, no. 4 (77), pp. 62–81. Available at: http://www.journal.viam.ru (accessed: October 04, 2025). DOI: 10.18577/2713-0193-2024-0-4-62-81.
  2. Duyunova V.A., Serebrennikova N.Yu., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Methods of forming metal-polymer composite materials (review). Aviation materials and technologies, 2022, no. 1 (66), pp. 65–77. Available at: http://www.journal.viam.ru (ассеssed: October 04, 2025). DOI: 10.18577/2713-0193-2022-0-1-65-77.
  3. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and properties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.18577/2071-9140-2020-0-1-54-63.
  4. Evdokimov S.A., Shchegoleva N.E., Kachaev A.A. Methods for joining ceramic composite materials based on SiC with ceramic and metallic materials (review). Aviation materials and technologies, 2022, no. 3 (68), pp. 75–83. Available at: http://www.journal.viam.ru (accessed: October 04, 2025). DOI: 10.18577/2713-0193-2022-0-3-75-83.
  5. Kablov E.N. Dominant of the National Technological Initiative. Metally Evrazii, 2017, no. 3, pp. 2–6.
  6. Khodorenko V.N., Yasenchuk Yu.F., Gunter V.E. Biocompatible porous permeable materials. Biocompatible materials and implants with shape memory: col. of materials of the All-Rus. conf. Ed. V.E. Gunter. Tomsk: NTL Publ. House, 2003, pp. 9–24.
  7. Method for producing biocompatible porous ceramics based on zirconium dioxide for endoprosthetics: pat. RU2741918C1 Rus. Federation; appl. 29.06.20; publ. 29.01.21.
  8. Safronova T.V., Putlyaev V.I., Ivanov V.K. et al. Powder mixtures based on ammonium hydrophosphate and calcium carbonate for obtaining biocompatible porous ceramics in the CaO–P2O5 system. Novye ogneupory, 2016, vol. 1, no. 9, pp. 45–53.
  9. Kovalko N.Yu., Morozova L.V., Kalinina M.V., Shilova O.A. Synthesis and physicomechanical properties of biocompatible ceramics based on T–ZrO2 for medical purposes. Proc. conf. «Inorganic chemistry – a fundamental basis in materials science of ceramic, glassy, and composite materials». St. Petersburg: Institute of Chemical Synthesis of RAS, 2016, pp. 93–95.
  10. Komlev V.S., Barinov S.M., Sergeeva N.S. et al. Porous apatite biocompatible matrices for cellular technologies for reconstruction of tissue defects in surgery. Doklady Akademii nauk, 2005, vol. 401, no. 1, pp. 49–51.
  11. Mikushina V.A., Sidorenko Yu.N. Multilevel approach to modeling biocompatible porous ceramics. Tomsk: ISPMS SB RAS, 2015, pp. 414–415.
  12. Lambert F., Bacevic M., Layrolle P. et al. Impact of biomaterial microtopography on bone regeneration: Comparison of three hydroxyapatites. Clinical Oral Implants Research, 2017, vol. 28 (10), pp. 201–207. DOI: 10.1111/clr.12986.
  13. Gopi D., Kavitha L., Ramya S., Rajeswari D. Chemical and green routes for the synthesis of multifunctional pure and substituted nanohydroxyapatite for biomedical applications. Engineering of Nanobiomaterials. William Andrew Publishing, 2016, pp. 485–521.
  14. Lin K., Chang J. Structure and properties of hydroxyapatite for biomedical applications. Hydroxyapatite (Hap) for Biomedical Applications. Cambridge: Woodhead Publishing, 2015, pp. 3–19.
  15. Seitz H., Rieder W., Irsen S. et al. Three-dimensional printing of porous ceramic scaffolds for bone tissue engineering. Journal of Biomedical Materials Research, 2005, vol. 72 (2), pp. 3–19. DOI: 10.1002/jbm.b.30291.
  16. Shuai C., Feng P., Yang B. et al. Effect of nano-zirconia on the mechanical and biological properties of calcium silicate scaffolds. International Journal of Applied Ceramic Technology, 2014, vol. 12 (6), pp. 1148–1156. DOI: 10.1111/ijac.12337.
  17. Miftakhov A.R. Nanostructured composites. Research in the field of bioengineering. Proceedings of the XXXX All-Rus. sc. and pract. conf. «Modernization of education in the context of technological and digital innovations: Theory and practice». Rostov-on-Don, 2021, pp. 63–67.
  18. Grishina I.P., Dudareva O.A., Markelova O.A., Lyasnikova A.V. Nanomaterials and composites based on them for bioengineering. Proceedings of the Int. Youth Scientific Conf. «The Future of Science–2013»: in 3 vols. Kursk, 2013, vol. 3, pp. 224–226.
  19. Lu T., Li Y., Chen T. Techniques for fabrication and construction of three-dimensional scaffolds for tissue engineering. International journal of nanomedicine, 2013, vol. 8, pp. 337–350.
  20. Kumar A., Kargozar S., Baino F., Han S. Additive manufacturing methods for producing hydroxyapatite and hydroxyapatite-based composite scaffolds: a review. Frontiers in Materials, 2019, vol. 6, p. 313.
  21. Mondal D., Srinivasan A., Comeau P. et al. Acrylated epoxidized soybean oil/hydroxyapatite-based nanocomposite scaffolds prepared by additive manufacturing for bone tissue engineering. Materials Science and Engineering: C, 2021, vol. 118, p. 111400.
  22. Zarei A., Farazin A. Synergizing additive manufacturing and machine learning for advanced hydroxyapatite scaffold design in bone regeneration. Journal of the Australian Ceramic Society, 2025, vol. 3, pp. 797–813.
  23. Soleymani S., Naghib S.M. 3D and 4D printing hydroxyapatite-based scaffolds for bone tissue engineering and regeneration. Heliyon, 2023, vol. 9, no. 9, pp. 67–74.
  24. Mondschein R.J., Kanitkar A., Williams C.B. et al. Polymer structure-property requirements for stereolithographic 3D printing of soft tissue engineering scaffolds. Biomaterials, 2017, vol. 9, pp. 67–74. DOI: 10.1016/j.biomaterials.2017.06.005.
  25. Barry J.J., Evseev A.V., Markov M.A. et al. In vitro study of hydroxyapatitebased photocurable polymer composites prepared by laser stereolithography and supercritical fluid extraction. Biomaterials, 2008, vol. 4, pp. 1603–1610.
  26. Woesz A., Rumpler M., Stampfl J. et al. Towards bone replacement materials from calcium phosphates via rapid prototyping and ceramic gelcasting. Materials Science and Engineering, 2005, vol. 25, pp. 181–186.
  27. Chen Q., Zou B., Lai Q. et al. A study on biosafety of HAP ceramic prepared by SLA-3D printing technology directly. Materials Science and Engineering, 2019, vol. 98, pp. 327–335.
  28. Le Guéhennec L., Van Hede D., Plougonven E. et al. In vitro and in vivo biocompatibility of calcium-phosphate scaffolds three-dimensional printed by stereolithography for bone regeneration. Journal of Biomedical Materials Research, 2020, vol. 108, pp. 412–425.
  29. Trachtenberg J.E., Placone J.K., Smith B.T. et al. Fabrication and Mechanical Characterization of 3D Printed Vertical Uniform and Gradient Scaffolds for Bone and Osteochondral Tissue Engineering. Biomaterials Science, 2017, vol. 28, pp. 532–554.
  30. Malayeri A., Gabbott C., Reilly G. et al. Fabrication and Evaluation of Custom Scaffolds for Craniofacial Surgery and Tissue Engineering. Regenerative Medicine, 2016, vol. 6, pp. 36.
  31. Michna S., Wu W., Lewis J.A. Biomaterials for bioprinting microvasculature. Biomaterials, 2005, vol. 26, pp. 5632–5639.
  32. Zhou Z., Lennon A., Buchanan F. et al. Binder jetting additive manufacturing of hydroxyapatite powders: Effects of adhesives on geometrical accuracy and green compressive strength. Additive Manufacturing, 2020, vol. 10, pp. 16–45.
  33. Liu Z.B., Liang H.X., Shi T.S. et al. Additive manufacturing of hydroxyapatite bone scaffolds via digital light processing and in vitro compatibility. Ceramics International, 2019, vol. 45, pp. 11079–11086.