Bespalov A.S., Salimov I.E., Lonskii S.L., Kurshev E.V., Ponomarenko S.A. Investigation of the composition and structure of a thermal insulation coating based on a polymer matrix and hollow microspheres // Proceedings of VIAM. 2026. No. 1 (155). С. 174–185. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-1-174-185.

Investigation of the composition and structure of a thermal insulation coating based on a polymer matrix and hollow microspheres

Bespalov A.S., Salimov I.E., Lonskii S.L., Kurshev E.V., Ponomarenko S.A.
Abstract

Liquid thermal insulation compositions based on a polymer matrix and the additions of gas filled or evacuated microspheres are considered, and the main prospects and scope of application of thin film thermal insulation material obtained from these liquid compositions is shown. The microstructure and X-ray spectral analysis of a typical thin-film thermal insulation coating and microspheres included in its composition were studied by pyrolytic gas chromate-mass spectrometry, the composition of the polymer component of the material was determined, and the structure of microspheres was studied by X-ray diffraction.

Keywords
liquid thermal insulation, thermal insulation coating, microspheres, pyrolytic gas chromate-mass-spectrometry, polymer matrix composition
Reference list
  1. Zagorodnyuk L.Kh., Sumskoy D.A., Zolotykh S.V. Effective thermal protection system using a low-density thermal insulation solution. Vestnik Sibirskogo gosudarstvennogo avtomobilno-dorozhnogo universiteta, 2019, vol. 16, no. 3 (67), pp. 324–333.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Foamed polyimides. Trudy VIAM, 2015, no. 4, paper no. 09. Available at: http://www.viam-works.ru (accessed: May 17, 2025). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  4. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concentration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41‒49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  5. Kan A.Ch., Zhelezina G.F., Kulagina G.S., Ayupov T.R. Fire safety of structural organic plastics reinforced with aramid fabrics. Aviation materials and technologies, 2022, no. 4 (69), pp. 51–60. Available at: http://www.journal.viam.ru (accessed: May 17, 2025). DOI: 10.18577/2713-0193-2022-0-4-51-60.
  6. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), pp. 119–126. Available at: http://www.journal.viam.ru (accessed: May 17, 2025). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  7. Babashov V.G., Varrik N.M., Karaseva T.A. Porous ceramic for filtration of metal melts and hot gases (rеview). Trudy VIAM, 2020, no. 8 (90), pp. 54–63. Available at: http://www.viam-works.ru (accessed: May 17, 2025.) DOI: 10.18577/2307-6046-2020-0-8-54-63.
  8. Istomin A.V., Kolyshev S.G. Processing of wastes high-temperature heat-protective material. Trudy VIAM, 2021, no. 1 (95), pp. 97‒104. Available at: http://www.viam-works.ru (accessed: May 17, 2025.). DOI: 10.18577/2307-6046-2021-0-1-97-104.
  9. Osnos S.P. Application of materials based on basalt fibers in the aerospace industry. Kompozitnyy mir, 2015, no. 4 (61), pp. 72–79.
  10. Bespalov A.S., Salimov I.E., Yudin A.V. Imparting highly hydrophobic properties to a high-porous ceramic material with low-concentration solutions of fluoroparaffin in a supercritical carbon dioxide environment. Aviation materials and technologies, 2025, no. 1 (78), pp. 39‒48. Available at: http://www.journal.viam.ru (accessed: May 17, 2025). DOI: 10.18577/2713-0193-2025-0-1-39-48.
  11. Lermontov S.A., Sipyagina N.A., Malkova A.N., Buznik V.M., Bespalov A.S., Grashchenkov D.V., Baranchikov A.E. Hierarchical porous composite ceramic material modified by hydrophobic methyltrimethoxysilane-based aerogel. Journal of porous materials, 2021, vol. 28, no. 4, pp. 1237–1244. DOI: 10.1007/s10934-021-01075-3.
  12. Kondrashov E.K., Nefedov N.I., Vereninova N.P., Kushch P.P., Kichigina G.A., Kiryukhin D.P., Buznik V.M. Modification of fluorocopolymer coatings by telomers to improve their hydrophobicity. Polymer Science. Series D, 2016, vol. 9, no. 2, pp. 212–218.
  13. Buznik V.M. The state of domestic fluoropolymer chemistry and possible development prospects. Rossiyskiy khimicheskiy zhurnal, 2008, vol. 52, no. 3, pp. 7–12.
  14. Venevitin A.A., Asminin V.F. Improving the functional properties of heat-insulating coatings based on hollow microspheres. Current areas of scientific research in the 21st century: theory and practice, 2013, no. 5, pp. 171–178.
  15. Zhdanov N.N., Garipov R.M., Levin A.S. The influence of functionalized monomers on the properties of acrylstyrene dispersion and heat-protective coating based on it. Vestnik tekhnologicheskogo universiteta, 2016, vol. 19, no. 23, pp. 65–67.
  16. Kurshev E.V., Lonskiy S.L., Deev I.S. Application of scanning electron microscopy and X-ray spectral microanalysis to study non-metallic composite materials. Proc. of the VIII All-Rus. Conf. on Testing and Research of Material Properties «TestMat»: in 4 parts. Moscow: VIAM, 2016, part 2, pp. 1–13.
  17. Deev I.S., Kobets L.P. Structure formation in filled thermosetting polymers. Kolloidnyy zhurnal, 1999, vol. 61, no. 5, pp. 650–660.
  18. Bousfield B. Surface Preparation and Microscopy of Materials. John Wiley & Sons Ltd, 1992, 342 p.
  19. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading. Trudy VIAM, 2014, no. 7, paper no. 06. Available at: http://www.viam-works.ru (accessed: May 13, 2025). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  20. Trathnigg B. Size-exclusion chromatography of polymers. Encyclopedia of Analytical Chemistry. Ed. R.A. Meyers. Chichester: Wiley, 2000, pp. 8008–8034.
  21. Grundy P.J., Jones G.A. Electron Microscopy in the Study of Materials. Edward Arnold Publishers Ltd, 1976, 194 p.
  22. Ponomarenko S.A., Shimkin A.A. Chromatographic methods of analysis: application possibilities in the aviation industry (review). Zavodskaya laboratoriya. Diagnostika materialov, 2017, no. 83 (4), pp. 5–13.
  23. Applied Pyrolysis Handbook. 2nd ed. Ed. T.P. Wampler. CRC Press, 2006, 304 p.
  24. Lebedev A.T. Mass Spectrometry in Organic Chemistry: A Textbook. Moscow: Binom. Knowledge Laboratory, 2003, 493 p.
  25. Zhdanov N.N. Development of Heat-Protective Coatings Based on Acrylic-Styrene Copolymers and Hollow Glass Microspheres: thesis, Cand. Sc. (Thech.). Kazan, 2017, 123 p.
  26. Loginova N.A. Determination of the Efficiency of Thin-Film Thermal Insulation Coatings as Applied to Heating Systems: thesis, Cand. Sc. (Thech.). Moscow, 2010, 133 p.