Startsev V.O. Climatic aging of paint coating systems. Part 5. Influence of duration of erosion effect // Proceedings of VIAM. 2025. No. 9 (151). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-9-149-160.

Climatic aging of paint coating systems

Part 5. Influence of duration of erosion effect
Startsev V.O.
Abstract

In the fifth part of the series of articles on the climatic aging of paint coating systems, the features of the change in the color indices of the CIE L*a*b* model under the influence of sand and dust in laboratory conditions are studied. It is shown that for different paint coating systems with the addition of red and gray pigments, the dependences of the change in lightness and chromatic indices differ significantly. For all the studied systems, the contribution of the L, a, b indices to the change in color distance is quantitatively characterized.

Keywords
paint coating, color distance, erosion, mathematical modeling, forecasting
Reference list
  1. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex systems of paint and varnish coatings for the protection of metal polymer composite materials, as well as their contact joints from the effects of aggressive factors. Lakokrasochnye materialy i ikh primenenie, 2016 no. 6, pp. 32–35.
  2. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  3. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: 08.07.2025). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  4. Startsev O.V., Koval T.V., Krotov A.S., Dvirnaya E.V., Veligodsky I.M. Investigation of the properties of carbon fiber reinforced plastic with coatings after 8 and 13 years of aging in moderately warm climate. Part 2. Condition of protective paint and vanish coatings. Trudy VIAM, 2024, no. 11 (141), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 08, 2025). DOI: 10.18577/2307-6046-2024-0-11-113-124.
  5. Startsev V.O., Frolov A.S. Influence of climatic influence on color characteristics of paint and varnish coatings. Lakokrasochnye materialy i ikh primenenie, 2015, no. 3, pp. 16–18.
  6. Wu L., Guo X., Zhang J. Abrasive Resistant Coatings – A Review. Lubricants, 2014, vol. 2, no. 2, pp. 66–89.
  7. Zheng L., Fan J., Gong Q. et al. Sand Erosion Resistance and Failure Mechanism of Polyurethane Film on Helicopter Rotor Blades. Polymers, 2023, vol. 15, no. 22, p. 4386.
  8. Khorshidi F.H., Najafi S.K., Najafi F. et al. Color and Gloss Changes of a Lignin-Based Polyurethane Coating under Accelerated Weathering. Journal of Renewable Materials, 2023, vol. 12, no. 2, pp. 1–10.
  9. Kotnarowska D., Przerwa M., Szumiata T. Resistance to Erosive Wear of Epoxy-Polyurethane Coating Modified With Nanofillers. Journal of Materials Science Research, 2014, vol. 3, no. 2, pp. 52–58.
  10. Zhang Ti., Zhang Te., He Y. et al. Corrosion and aging of organic aviation coatings: A review. Chinese Journal of Aeronautics, 2023, vol. 36, no. 4, pp. 1–35.
  11. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: July 08, 2025). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  12. Zhang S.W., Deguo W., Weihua Y. Investigation of abrasive erosion of polymers. Journal of Materials Science, 1995, vol. 30, no. 18, pp. 4561–4566.
  13. Hernández-Peña A., Gallardo-Hernández E.A., Farfan-Cabrera L.I. et al. Solid particle erosion evaluation of automotive paint coatings under the influence of artificial weathering. Wear, 2023, vol. 532–533, art. 205105.
  14. Wärnheim A., Saarimaa V., Heydari G. et al. Multiscale analysis of pigment effects on weathering of polyester coatings: from nanoscale chemistry to macroscale performance. Materials Degradation, 2025, vol. 9, no. 1, art. 66.
  15. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
  16. Cai G., Zhang D., Jiang D., Dong Z. Degradation of fluorinated polyurethane coating under UVA and salt spray. Part II: Molecular structures and depth profile. Progress in Organic Coatings, 2018, vol. 124, pp. 25–32.
  17. Molina M.T., Cano E., Ramírez-Barat B. Testing protective coatings for metal conservation: the influence of the application method. Heritage Science, 2023, vol. 11, no. 1, art. 94.
  18. Chen J., Li B., Zeng X. et al. Study on the Influence of Accelerated Aging on the Properties of an RTV Anti-Pollution Flashover Coating. Polymers, 2023, vol. 15, no. 3, art. 751.
  19. Pánek M., Reinprecht L. Critical view on the possibility of color changes prediction in the surfaces of painted wood exposed outdoors using accelerated weathering in Xenotest. Journal of Coatings Technology and Research, 2019, vol. 16, no. 2, pp. 339–352.
  20. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: July 08, 2025). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  21. Dao P.H., Nguyen A.H., Mac V.P. et al. Aging of waterborne paint based on the acrylic resin emulsion and organic pigment. Vietnam Journal of Science and Technology, 2018, vol. 56, no. 3B, art. 126.
  22. Guerguer M., Naamane S., Edfouf Z. et al. Chemical degradation and color changes of paint protective coatings used in solar glass mirrors. Coatings, 2021, vol. 11, no. 4, art. 476.
  23. Startsev V.O. Climatic aging of paint coating systems. Part 4. Additivity of the impact of climate factors. Trudy VIAM, 2025, no. 8 (150), paper no. 13. Available at: http://www.viam-works.ru (accessed: August 20, 2025). DOI: 10.18577/2307-6046-2025-8-152-162.
  24. Startsev V.O. Climate aging of paint coating systems. Part 3. Comparison of results of natural and accelerated climatic tests taking into account the effect of seasonality. Trudy VIAM, 2025, no. 7 (149), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 20, 2025). DOI: 10.18577/2307-6046-2025-7-105-118.
  25. Fairchild M.D. Color Appearance Models. Wiley, 2013, 480 p.
  26. Schanda J. Colorimetry: Understanding the CIE System. Wiley, 2007, 398 p.
  27. Ibraheem N.A., Hasan M.M., Khan R.Z., Mishra P.K. Understanding Color Models : A Review. ARPN Journal of Science and Technology, 2012, vol. 2, no. 3, pp. 265–275.
  28. Isupov V.V., Startsev O.V. Numerical methods in dynamic mechanical spectroscopy of polymers. Abstract of reports. Int. Conf. «Mathematical models and numerical methods of continuous media mechanics» dedicated to the 75th anniversary of the outstanding mathematician and mechanic, organizer of science, academician Nikolai Nikolaevich Yanenko. Ed. Yu.I. Shokin. Novosibirsk: Publ. house of the SB of RAS, 1996, pp. 293–294.
  29. Startsev O.V., Perepechko I.I. Molecular mobility and relaxation processes in the epoxy matrix of the composite. 1. Effect of the type of reinforcing filler. Mekhanika kompozitnykh materialov, 1984, no. 3, pp. 387–391.
  30. Kablov E.N., Lebedev M.P., Startsev O.V., Golikov N.I. Climatic tests of materials, structural elements, machinery and equipment in conditions of extremely low temperatures. Proc. of the VI Eurasian Symposium on the Problems of Strength of Materials and Machines for Cold Climate Regions EURASTRENCOLD–2013. Yakutsk, 2013, pp. 5–7.
  31. Startsev O.V., Lebedev M.P., Kychkin A.K. Aging of polymer composite materials in conditions of extremely cold climate. Izvestiya Altayskogo gosudarstvennogo universiteta, 2020, no. 1 (111), pp. 41–51.