Abstract

The article analyzes publications on various methods of modification of water-based acrylic copolymers and provides the advantages and disadvantages of water-based acrylic coatings.  The physical and chemical modification methods that make it possible to change the properties of water-based acrylic copolymers are considered. The paper shows the practical use of these modification methods for increasing water and corrosion resistance, as well as thermal and physical-mechanical properties of water-based acrylic coatings.

Keywords
water-based acrylic copolymer, physical modification, chemical modification, physical-mechanical properties, thermal properties, corrosion resistance, water resistance
Reference list
  1. Karami S., Montahari S., Pishvaei M., Eskandari N. Improvement of thermal properties of pigmented acrylic resin using silica aerogel. Journal of applied polymer science, 2018, vol. 135, no. 1, pp. 1–9. DOI: 10.1002/app.45640.
  2. Du B., Chen F., Luo R., Zhou S., Wu Z. Synthesis and Characterization of Nano-TiO2/SiO2-Acrylic Composite Resin. Advances in Materials Science and Engineering, 2019, vol. 2019, pp. 1–7. DOI: 10.1155/2019/6318623.
  3. Yilmaz O. High performance nanocomposite coatings based on soft core-reactive shell polyacrylic latex/modified halloysite nanotubes. Progress in Organic Coatings, 2019, vol. 127, pp. 266–275. DOI: 10.1016/j.porgcoat.2018.11.026.
  4. Zhong S., Li J., Cai Y., Yi L. Novel surfactant-free waterborne acrylic-silicone modified alkyd hybrid resin coatings containing nano-silica for the corrosion protection of carbon steel. Polymer-Plastics Technology and Materials, 2019, vol. 58, no. 8, pp. 866–878. DOI: 10.1080/03602559.2018.1542711.
  5. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Grigoreva K.N. Research of the influence of the modifying additives nature on the rheological and thermomechanical properties of a photopolymer composition based on epoxy vinyl ester resin. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 31–40. DOI: 10.18577/2071-9140-2019-0-3-31-40.
  6. Wei J., Oyang C., Shan X., Gao Q. Advances in water-resistant modification of aqueous acrylic resins: modification methods, mechanism of action. MATEC Web of Conferences, 2022, vol. 363, pp. 1–9. DOI: 10.1051/matecconf/202236301024.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Yin Y., Jiang B., Zhu X. et al. Investigation of Thermostability of Modified Graphene Oxide/Methylsilicone Resin Nanocomposites. Engineered Science, 2019, vol. 5, pp. 73–78. DOI: 10.30919/es8d762.
  9. Tang L.S., Zhang M., Zhang S.F., Yang J.Z. High performance waterborne aminoacrylic coatings from the blends of hydrosols and latexes. Progress in Organic Coatings, 2004, vol. 49, no. 1, pp. 54–61. DOI: 10.1016/j.porgcoat.2003.08.007.
  10. Yang K., Chen X., Zhang Z. et al. Introducing rigid pyrimidine ring to improve the mechanical properties and thermal-oxidative stabilities of phthalonitrile resin. Polymers for Advanced Technologies, 2019, vol. 31, no. 2, pp. 328–337. DOI: 10.1002/pat.4773.
  11. Bai L., Zheng S., Bao R. et al. Effect of PLA Crystallization on the Thermal Conductivity and Breakdown Strength of PLA/BN Composites. ES Materials & Manufacturing, 2019, vol. 3, pp. 66–72. DOI: 10.30919/esmm5f195.
  12. Xiong K., Wang L., Zhang A. The Mechanical Properties, Compatibility, and Thermal Stabilities of POE-Graft-Methyl Methacrylate and Acrylonitrile(POE-g-MAN)/ Styrene-Acrylonitrile Copolymer (SAN Resin) Blends. Journal of Macromolecular Science, Part B, 2011, vol. 50, no. 7, pp. 1350–1363. DOI: 10.1080/00222348.2010.516178.
  13. Romo-Uribe A., Santiago-Santiago K., Zavala-Padilla G. et al. Waterborne layered silicate/acrylate nanocomposites by in-situ emulsion polymerization: Thermal and mechanical reinforcement. Progress in Organic Coatings, 2016, vol. 101, pp. 59–70. DOI: 10.1016/j.porgcoat.2016.07.014.
  14. Insulating paint for interior and exterior of buildings and method of making same: pat. 4623390A US; appl. 04.11.85; publ. 18.11.86.
  15. Comite A., Cozza E.S., Di Tanna G. et al. Influence of counter ions in electrochemical properties and kinetic parameters of poly tyramine electroactive film. Progress in Organic Coatings, 2015, vol. 78, pp. 124–132.
  16. Jiao C., Sun L., Shao Q. et al. Advances in Waterborne Acrylic Resins: Synthesis Principle, Modification Strategies, and Their Applications. ACS Omega, 2021, vol. 6, pp. 2443–2449. DOI: 10.1021/acsomega.0c05593.
  17. Marchenko S.A., Zheleznyak V.G., Kuznetsova V.A. Application and modification of particles to create superhydrophobic coatings (review). Trudy VIAM, 2023, no. 5 (123), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 05, 2025). DOI: 10.18577/2307-6046-2023-0-5-94-110.
  18. Timperley C.M., Arbon R.E., Bird M. et al. Bis(fluoroalkyl)acrylic and methacrylic phosphate monomers, their polymers and some of their properties. Journal of Fluorine Chemistry, 2003, vol. 121, no. 1, pp. 23–31. DOI: 10.1016/S0022-1139(02)00314-7.
  19. Yang W., Zhu L., Chen Y. et al. Surface topography and hydrophobicity of waterborne fluorinated acrylic/silica hybrid coatings. Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2015, vol. 484, pp. 62–69. DOI: 10.1016/j.colsurfa.2015.07.053.
  20. Xu H., Qiu F., Wang Y. et al. Preparation, Mechanical Properties of Waterborne Polyurethane and Crosslinked Polyurethane-Acrylate Composite. Journal of Applied Polymer Science, 2012, vol. 124, no. 2, pp. 958–968. DOI: 10.1002/app.35127.
  21. Zheng B., Ge S., Wang S. et al. Effect of γ-aminopropyltriethoxysilane on the properties of cellulose acetate butyrate modified acrylic waterborne coatings. Reactive and Functional Polymers, 2020, vol. 154, pp. 1–8. DOI: 10.1016/j.reactfunctpolym.2020.104657.
  22. Jiang Y., Li L., Liu J. et al. Hydrophobic films of acrylic emulsion by incorporation of fluorine-based copolymer prepared through the RAFT emulsion copolymerization. Journal of Fluorine Chemistry, 2016, vol. 183, pp. 82–91. DOI: 10.1016/j.jfluchem.2016.01.010.
  23. Li L., Li X., Shen Y. et al. Hydrophobicity and corrosion resistance of waterborne fluorinated acrylate/silica nanocomposite coatings. e-Polymers, 2021, vol. 21, no. 1, pp. 779–792. DOI: 10.1515/epoly-2021-0079.
  24. Liu M., Mao X., Zhu H. et al. Water and corrosion resistance of epoxy–acrylic–amine waterborne coatings: Effects of resin molecular weight, polar group and hydrophobic segment. Corrosion Science, 2013, vol. 75, pp. 106–113. DOI: 10.1016/j.corsci.2013.05.020.
  25. Bi J., Liu Y., Gao F. et al. Improving water resistance and mechanical properties of waterborne acrylic resin modified by 3,3′,5,5′-tetramethyl-4,4′-biphenyl diglycidyl ether. Surfaces and Interfaces, 2022, vol. 35, pp. 1–34. DOI: 10.1016/j.surfin.2022.102426.
  26. Liang C., Du Y., Wang Y. et al. Intumescent fire-retardant coatings for ancient wooden architectures with ideal electromagnetic interference shielding. Advanced Composites and Hybrid Materials, 2021, vol. 4, pp. 979–988. DOI: 10.1007/s42114-021-00274-5.
  27. Ji S., Gui H., Guan G. et al. Molecular design and copolymerization to enhance the anti-corrosion performance of waterborne acrylic coatings. Progress in Organic Coatings, 2021, vol. 153, pp. 1–12. DOI: 10.1016/j.porgcoat.2021.106140.
  28. Tereshko A.E., Golikov I.V., Indeikin E.A., Krasnobaeva V.S. Modification of acrylic water-dispersed paints and varnishes with petroleum hydrocarbons. Izvestiya vysshikh uchebnykh zavedeniy. Khimiya i khimicheskaya tekhnologiya, 2007, no. 50 (4), pp. 77–80.
  29. Guo X., Ge S., Wang J. et al. Waterborne acrylic resin modified with glycidyl methacrylate (GMA): Formula optimization and property analysis. Polymer, 2018, vol. 143, pp. 155–163. DOI: 10.1016/j.polymer.2018.04.020.
  30. Nosrati R., Olad A., Maryami F. Visible-light induced anti-bacterial and self-cleaning waterborne polyacrylic coating modified with TiO2/polypyrrole nanocomposite; preparation and characterization. Journal of Molecular Structure, 2018, vol. 1163, pp. 174–184. DOI: 10.1016/j.molstruc.2018.02.097.
  31. Poddar M.K., Sharma S., Moholkar V.S. Investigations in two-step ultrasonic synthesis of PMMA/ZnO nanocomposites by in situ emulsion polymerization. Polymer, 2016, vol. 99, pp. 453–469. DOI: 10.1016/j.polymer.2016.07.052.
  32. Sharma S., Poddar M.K., Moholkar V.S. Enhancement of thermal and mechanical properties of poly(MMA-co-BA)/Cloisite 30B nanocomposites by ultrasound-assisted in-situ emulsion polymerization. Ultrasonics Sonochemistry, 2017, vol. 36, pp. 212–225. DOI: 10.1016/j.ultsonch.2016.11.029.
  33. Zahedi F., Amraee I.A. Carboxylated multiwalled carbon nanotubes effect on dynamic mechanical behavior of soft films composed of multilayer polymer structure. Polymer, 2018, vol. 151, pp. 187–196. DOI: 10.1016/j.polymer.2018.07.044.
  34. Tkachuk A.I., Kurshev E.V., Lonskii S.L., Lyubimova A.S. Modification of epoxy binderes with multi-walled carbon nanotubes. Trudy VIAM, 2023, no. 2 (120), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 05, 2025). DOI: 10.18577/2307-6046-2023-0-2-63-76.
  35. Solovyanchik L.V., Kondrashov S.V. The prospects of using carbon nanotubes to impart functional properties to the surface of polymer materials (review). Trudy VIAM, 2021, no. 9 (103), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 06, 2025). DOI: 10.18577/2307-6046-2021-0-9-11-21.
  36. Kryzhanovsky V.K. Technical properties of polymeric materials. St. Petersburg: Professiya, 2003, 203 p.
  37. Rostiashvili V.G., Irzhak V.I., Rosenberg B.A. Glass transition of polymers. Leningrad: Khimiya, 1987, 192 p.
  38. Drake I., Cardoen G., Hughes A. et al. Polyurea-acrylic hybrid emulsions: Characterization and film properties. Polymers, 2019, vol. 181, pp. 1–10. DOI: 10.1016/j.polymer.2019.121761.
  39. Shim J.Y., Park D.M., Kim H.O. The Synthesis of Waterborne Acrylic – Modified Alkyd and its Application. Proceedings of the 24th International Waterborne, High-Solids, and Powder Coatings Symposium, 1997, pp. 159–167.
  40. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  41. Madhusudha A.M., Mohana K.N.S., Hegde M.B. et al. Functionalized graphene oxide-epoxy phenolic novolac nanocomposite: an efficient anticorrosion coating on mild steel in saline medium. Advances Composites and Hybrid Materials, 2020, vol. 3, pp. 141–155. DOI: 10.1007/s42114-020-00142-8.
  42. Zhong S., Li J., Yi L. et al. Cross-linked waterborne alkyd hybrid resin coatings modified by fluorinated acrylate-siloxane with high waterproof and anticorrosive performance. Polymers for Advanced Technologies, 2018, vol. 30, no. 2, pp. 292–303. DOI: 10.1002/pat.4464.
  43. Pham H.H., Winnik M.A. Polymer Interdiffusion vs Cross-Linking in Carboxylic Acid−Carbodiimide Latex Films. Effect of Annealing Temperature, Reactive Group Concentration, and Carbodiimide Substituent. Macromolecules, 2006, vol. 39, no. 4, pp. 1425–1435. DOI: 10.1021/ma051685w.
  44. Liu M., Mao X., Zhu H. et al. Water and corrosion resistance of epoxy–acrylic–amine waterborne coatings: Effects of resin molecular weight, polar group and hydrophobic segment. Corrosion Science, 2013, vol. 75, pp. 106–113. DOI: 10.1016/j.corsci.2013.05.020.
  45. Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021, no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: May 06, 2025). DOI: 10.18577/2713-0193-2021-0-1-71-79.
  46. Zhong Z., Yu Q., Yao H. et al. Study of the styrene–acrylic emulsion modified by hydroxyl-phosphate ester and its stoving varnish. Progress in Organic Coatings, 2013, vol. 76, no. 5, pp. 858–863. DOI: 10.1016/j.porgcoat.2013.02.008.
  47. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.