Panteleev M.D., Sviridov A.V., Popov K.N., Zotov S.D. New filler material for welding of foundry heat-resistant nickel alloys VZHL718 and VZHL220 // Proceedings of VIAM. 2025. No. 8 (150). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-8-31-40.
New filler material for welding of foundry heat-resistant nickel alloys VZHL718 and VZHL220
Abstract
The article presents the details of the investigation and of the production of the welding consumable for repairing foundry heat-resistant nickel alloys ВЖЛ718 and ВЖЛ220 cast workpieces. The research of mechanical properties from casting material before and after the repairing is conducted. The results of the research of filler material mechanical properties are discussed. The optimized chemical composition of the filler material is determined and is named Св-ВЖ183.
Keywords
In718, Rene220, foundry nickel alloy, defects’ repairing, repairing of foundry defects, tungsten inert gases welding, filler material, mechanical properties
Reference list
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12.
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 2. Compensation and control of deviations, GIP and heat treatment. Elektrometallurgiya, 2022, no. 2, pp. 2–12.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 3. Adaptation and creation of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 4. Development of heat-resistant materials. Elektrometallurgiya, 2022, no. 5, pp. 8–19.
- Knyazev A.E., Min P.G. Comparison of characteristics of metal powder compositions of VZhL718 alloy, manufactured by PREP and VEGA methods, after selective laser melting. Metallurg, 2024, no. 4, pp. 48–58.
- Min P.G., Vadeev V.E., Kolesnikov S.I., Chemov D.A. The effect of impurities on mechanical and operational properties of the cast nickel-base superalloy VZhM200. Trudy VIAM, 2024, no. 10 (140), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 15, 2025). DOI: 10.18577/2307-6046-2024-0-10-13-23.
- Min P.G., Vadeev V.E., Rogalev A.M., Knyazev A.E. Study of chemical composition, structure and mechanical properties of EP648 alloy at various stages of additive manufacturing. Materialovedenie, 2018, no. 12, pp. 17–22.
- Mostafa A., Rubio I.P., Brailovski V. et al. Structure, Texture and Phases in 3D Printed IN718 Alloy Subjected to Homogenization and HIP Treatments. Metals, 2017, no. 7, pp. 196–219. DOI: 10.3390/met7060196.
- El-Bagoury N., Hessien M.M., Alsawat M. et al. Optimization of Microstructure and Mechanical Properties of Hipped Inconel 718 by Various Heat Treatment Processes. Metallography, Microstructure, and Analysis, 2019, vol. 8, pp. 642–655. DOI: 10.1007/s13632-019-00568-7.
- Loshchinin Yu.V., Pakhomkin S.I., Razmakhov M.G. Phase transformation temperatures and calorimetric analysis of powder compositions of nickel-based superalloys. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-1-79-85.
- Gorbovets M.A., Khodinev I.A., Monin S.A. Influence of average cycle stress on characteristics of low-cycle fatigue of high-temperature nickel alloy VZh175. Aviation materials and technologies, 2023, no. 1 (70), paper no. 10. Available at: http://www.journal.viam.ru (accessed: May 15, 2025). DOI: 10.18577/2713-0193-2023-0-1-126-136.
- Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 15, 2025). DOI: 10.18577/2713-0193-2023-0-3-3-14.
- Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), paper no. 03. Available at: http://www.journal.viam.ru (accessed: May 15, 2025). DOI: 10.18577/2713-0193-2023-0-3-30-41.
- Nickel based filler material: pat. 2373038 Rus. Federation; appl. 02.06.08; publ. 20.11.09.
- Nickel based filler material: pat. 2304499 Rus. Federation; appl. 10.11.05; publ. 20.08.07.
- Heat-resistant nickel-based alloy and product made from this alloy: pat. 2285059 Rus. Federation; appl. 24.03.05; publ. 10.10.06.
- Heat-resistant weldable nickel-based alloy and a product made from this alloy: pat. 2301277 Rus. Federation; appl. 20.12.05; publ. 20.06.07.
- Weldable oxidation resistant nickel-iron-chromium-aluminium alloy: pat. 8506883 US; appl. 12.12.07; publ. 18.06.09.
- Nickel-chromium-iron-aluminium alloy: pat. 4671931 US; appl. 11.05.84; publ. 09.06.87.
- Superalloy repair welding using multiple alloy powders: pat. 8618434 US; appl. 22.03.10; publ. 22.09.11.
- Repaired turbine exhaust strut heat shield vanes and repair methods: pat. 8083465 US; appl. 05.09.08; publ. 11.03.10.