Startsev V.O. Climate aging of paint coating systems. Part 2. Influence of different climatic zones // Proceedings of VIAM. 2025. No. 6 (148). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-6-86-97.

Climate aging of paint coating systems

Part 2. Influence of different climatic zones
Startsev V.O.
Abstract

The second part of the article series on climatic aging of paint coating systems shows the difference in the change in the color distance of aluminum alloy samples with applied epoxy and fluoropolyurethane enamels with red and gray pigments when exposed to climatic zones of moderate, moderately warm and dry subtropical climates. The article provides the calculation of parameters of the time exponential model describing the change in the color distance. As a result there has been found a significant difference in the change in the color distance in moderate and moderately warm climate from the same indicators of a dry subtropical climate.

Keywords
climatic aging, paint coating, color distance, solar radiation, mathematical modeling, forecasting
Reference list
  1. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex systems of paint and varnish coatings for the protection of metal polymer composite materials, as well as their contact joints from the effects of aggressive factors. Lakokrasochnye materialy i ikh primenenie, 2016, no. 6, рр. 32–35.
  2. Erofeev V.T., Smirnov I.V., Voronov P.V., Afonin V.V., Kablov E.N. et al. Study of the resistance of polymer coatings under the influence of climatic factors of the Black Sea coast. Fundamentalnye issledovaniya, 2016, no. 11, рр. 911–924.
  3. Zhang Ti., Zhang Te., He Y. et al. Corrosion and aging of organic aviation coatings: A review. Chinese Journal of Aeronautics, 2023, vol. 36, no. 4, pp. 1–35.
  4. Lebedev M.P., Startsev O.V., Koval T.V., Veligodskiy I.M. Multiplet relaxation α-transitions in a fluororethane coating after climatic aging. Doklady Rossiyskoy akademii nauk. Khimiya, nauki o materialakh, 2024, vol. 516, no. 1, pp. 45–51.
  5. Startsev O.V., Makhonkov A.Yu., Deev I.S., Nikishin E.F. Study of aging of KMU-4L carbon fiber reinforced plastic after 12 years of exposure on the International Space Station using the method of dynamic mechanical analysis. 2. Effect of plate location in multilayer stacks. Voprosy materialovedeniya, 2013, no. 4, pp. 69–76.
  6. Startsev O.V., Bolonin A.B., Vapirov Yu.M. et al. Improving the viscoelastic properties of acrylic enamel AC-1115. Lakokrasochnye materialy i ikh primenenie, 1986, no. 4, pp. 16–18.
  7. Startsev O.V., Medvedev I.M., Krotov A.S., Panin S.V. Dependence of the surface temperature of samples on the climate characteristics during exposure under natural conditions. Korroziya: materialy, zashchita, 2013, no. 7, pp. 43–47.
  8. Startsev O.V., Koval T.V., Krotov A.S., Veligodsky I.M. Modeling of moisture desorption from carbon fiber with protective coatings after long-term climatic aging. Korroziya: materialy, zashchita: Supplement to the journal «Tekhnologiya metallov», 2024, no. 17, pp. 1–10.
  9. Kuznetsova V.A., Yemelyanov V.V., Shapovalov G.G., Kovrizhkina N.A. Use of modifiers for increase of operational properties of paint coatings on the basis of the epoxy film-forming (review). Trudy VIAM, 2021, no. 12 (106), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 23, 2024). DOI: 10.18577/2307-6046-2021-0-12-63-72.
  10. Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Zheleznyak V.G. Trends in the development of matte wear-resistant paint coatings. Trudy VIAM, 2023, no. 10 (128), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 23, 2024). DOI: 10.18577/2307-6046-2023-0-10-132-144.
  11. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: December 23, 2024). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  12. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: December 23, 2024). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  13. Dao P.H., Nguen A.H., Mac V.P. et al. Aging of waterborne paint based on the acrylic resin emulsion and organic pigment. Vietnam Journal of Science and Technology, 2018, vol. 56, no. 3B, art. 126.
  14. Guerguer M., Naamane S., Edfouf Z. et al. Chemical degradation and color changes of paint protective coatings used in solar glass mirrors. Coatings, 2021, vol. 11, no. 4, art. 476.
  15. Knudsen O.Ø., Skilbred A.W.B., Løken A. et al. Correlations between standard accelerated tests for protective organic coatings and field performance. Materials Today Communications, 2022, vol. 31, art. 103729.
  16. Bierwagen G.P., He L., Li J. et al. Studies of a new accelerated evaluation method for coating corrosion resistance – thermal cycling testing. Progress in Organic Coatings, 2000, vol. 39, no. 1, pp. 67–78.
  17. Li S., Be H., Weinell C.E. et al. A quantitative real-time evaluation of rust creep propagation in coating systems exposed to field testing and cyclic ageing test. Progress in Organic Coatings, 2023, vol. 184, art. 107866.
  18. Pélissier K., Le Bozec N., Thierry D. et al. Evaluation of the Long-Term Performance of Marine and Offshore Coatings System Exposed on a Traditional Stationary Site and an Operating Ship and Its Correlation to Accelerated Test. Coatings, 2022, vol. 12, no. 11, art. 1758.
  19. LeBozec N., Thierry D., Le Calvé P. et al. Performance of marine and offshore paint systems: Correlation of accelerated corrosion tests and field exposure on operating ships. Materials and Corrosion, 2015, vol. 66, no. 3, pp. 215–225.
  20. Momber A.W., Buchbach S., Plagemann P. et al. Edge coverage of organic coatings and corrosion protection over edges under simulated ballast water tank conditions. Progress in Organic Coatings, 2017, vol. 108, pp. 90–92.
  21. Pavlenko V., Manuylov V., Kuzhel V. et al. Research on testing methods for the corrosion resistance of paint coatings. Journal of Mechanical Engineering and Transport, 2024, vol. 18, no. 2, pp. 127–133.
  22. Revin P.O., Makarenko A.V., Harisov R.A. et al. Research of underwater applied coatings for corrosion protection of port facilities. Science and Technologies: Oil and Oil Products Pipeline Transportation, 2022, vol. 12, no. 4, pp. 385–393.
  23. Saha J.K., Mitra P.K., Pau S. et al. Performance of different organic coatings on steel substrate by accelerated and in atmospheric exposure tests. Indian Journal of Chemical Technology, 2010, vol. 17, no. 2, pp. 102–110.
  24. Chu M.T., Do D.T., Sereda V.N. et al. Correlation between climate testing methods and service life prediction for paint systems. International Journal of Corrosion and Scale Inhibition, 2023, vol. 12, no. 3, pp. 1363–1373.
  25. Gao J., Hu W., Wang R. et al. Study on a multifactor coupling accelerated test method for anticorrosive coatings in marine atmospheric environments. Polymer Testing, 2021, vol. 100, art. 107259.
  26. Startsev V.O. Methods for studying the aging of polymer binders. Klei. Germetiki. Tekhnologii, 2020, no. 9, pp. 16–26.
  27. Startsev V.O., Molokov M.V., Startsev O.V. et al. The effect of the aliphatic diluent ETAL-1 on the climatic resistance of epoxy polymers based on ED-20 resin. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 12, рp. 26–36.
  28. Startsev V.O., Kogan A.M., Zeleneva T.O. Climate aging of paint coating systems. Part 1. Effect of long-term exposure on color characteristics. Trudy VIAM, 2025, no. 5 (147), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 19, 2025). DOI: 10.18577/2307-6046-2025-0-5-99-111.
  29. Startsev V.O., Nizina T.A. The modeling of epoxy polymers weathering by the color characteristics measurements. Trudy VIAM, 2015, no. 12, paper no. 10. Available at: http://www.viam-works.ru (accessed: December 23, 2024). DOI: 10.18577/2307-6046-2015-0-12-10-10.