Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S. Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys. Part 2 // Proceedings of VIAM. 2025. No. 6 (148). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-6-13-30.

Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys

Part 2
Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S.
Abstract

The review considers the practical application of the directional solidification technique with a flat front to obtain castings with height-variable chemical composition (gradient castings with macrosegregation) and to solve problems of physical metallurgy of γʹ-strengthened Ni- and Co-based superalloys. Such problems include: determination of the influence of alloying elements Re, Ru, Ta and Al on the γʹ-solvus, solidus and liquidus temperatures of single-crystal nickel-based alloys, optimization of the chemical and phase composition of single-crystal Ni- and Co-based alloys, determination of the influence of alloying elements Al and W on compressive yield strength and heat resistance of cobalt-based alloys.

Keywords
directional solidification, flat growth front, macrosegregation of alloying elements, nickel- and cobalt-based superalloys, solidus temperature, liquidus temperature, yield strength, oxidation resistance
Reference list
  1. Ohno Т., Watanabe R., Tanaka K. Development of a nickel-base single crystal superalloy containing molybdenum by alloy designing method. Journal of the Iron and Steel Institute of Japan, 1988, vol. 74, no. 11, pp. 133–140.
  2. Harada H., Yamagata T., Nakazawa S. Design of high specific-strength nickel-base single-crystal superalloys. High Temperature Materials for Power Engineering 1990: Proceedings of Conference held in Liege: in 2 parts. Dordrecht, Boston, London: Kluwer Academic Publishing, 1990, part 2, pp. 1319–1328.
  3. Samoilov A.I., Morozova G.I., Krivko A.I., Afonicheva O.S. Analytical method for optimization of alloying of heat-resistant nickel alloys. Materialovedenie, 2000, no. 2, pp. 14−17.
  4. Morinaga M., Murata Y., Yukawa H. Recent progress in molecular orbital approach to alloy design. Materials Science Forum, 2004, vol. 449−452, pp. 37−42.
  5. Vigdorovich V.N., Volpyan A.E., Kurdyumov G.M. Directional crystallization and physicochemical analysis. Moscow: Khimiya, 1976, 200 p.
  6. Petrushin N.V., Monastyrskaya E.V. Application of directional crystallization to solving problems of development and optimization of heat-resistant materials. Materialovedenie, 1998, no. 5, pp. 2–10.
  7. Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S. Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys. Part 1. Trudy VIAM, 2025, no. 5 (147), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 16, 2025). DOI: 10.18577/2307-6046-2025-0-5-3-24.
  8. Logunov A.V. Heat-resistant nickel alloys for blades and disks of gas turbines. Rybinsk: Gas turbine technologies, 2017, 854 p.
  9. Epishin A., Petrushin N., Nolze G. et al. Investigation of the γ′-strengthened quaternary Co-based alloys Co−Al−W−Ta. Metallurgical and Materials Transactions A, 2018, vol. 49, no. 9, pp. 4042–4057. DOI: 10.1007/s11661-018-4756-3.
  10. Shalin R.E., Svetlov I.L., Kachanov E.B. et al. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.
  11. Caron P. High γʹ solvus new generation nickel-based superalloys for single crystal turbine blade applications. Superalloys 2000. Minerals, Metals & Materials Society, 2000, pp. 737‒746.
  12. Mills K.C., Youssef Y.M., Li Z., Su Y. Calculation of thermophysical properties of Ni-based superalloys. ISIJ International, 2006, vol. 46, no. 5, pp. 623–632. DOI: 10.2355/isijinternational.46.623.
  13. Kablov E.N., Petrushin N.V. Computer method for designing cast heat-resistant nickel alloys. Cast heat-resistant alloys. Effect of S.T. Kishkin. Moscow: Nauka, 2006, pp. 56−78.
  14. Petrushin N.V., Elyutin E.S., Nazarkin R.M. et al. Segregation of alloying elements in directionally crystallized heat-resistant nickel alloys containing rhenium and ruthenium. Voprosy materialovedeniya, 2015, no. 1 (81), pp. 27–37.
  15. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 15, 2024). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  16. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 15, 2024). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  17. Kablov E.N. Casting heat-resistant alloys. Mechanical engineering: encyclopedia in 40 volumes. Moscow: Mashinostroyenie, 2001, vol. II-3: Non-ferrous metals and alloys. Composite materials, pp. 519−552.
  18. Petrushin N.V., Chabina E.B., Dyachkov L.A. Phase stability of single crystals of heat-resistant nickel alloys Ni−Al−Cr−W−Ta−Mo. Metally, 1996, no. 3, pp. 104–112.
  19. Sato J., Omori T., Oikawa K. et al. Cobalt-base high-temperature alloys. Science, 2006, vol. 312, pp. 90−91. DOI: 10.1126/science.1121738.
  20. Pollock T.M., Dibbern J., Tsunekane M. et al. New Co-based high-temperature alloys. Journal of Metals, 2010, vol. 62, no. 1, pp. 58−63. DOI: 10.1007/s11837-010-0013-y.
  21. Yan H.-Yu., Vorontsov V.A., Coakley J. et al. Quaternary alloying effects and the properties for a new generation of Co-base superalloys. Superalloys 2012: 12th International Symposium on Superalloys. Minerals, Metals & Materials Society, 2012, pp. 705–714.
  22. Bauer A., Neumeier S., Pyczak F. et al. Creep properties of different γʹ-strengthened Co-base Superalloys. Materials Science and Engineering A, 2012, vol. 550, pp. 333–341.
  23. Suzuki A., Pollock T.M. High-temperature strength and deformation of γ/γ′ two-phase Co−Al−W-base alloys. Acta Materialia, 2008, vol. 56, no. 6, pp. 1288−1297.
  24. Yan H.-Yu., Vorontsov V.A., Dye D. Alloying effects in polycrystalline γ′ strengthened Co−Al−W base alloys. Intermetallics, 2014, vol. 48, pp. 44–53. DOI: 1-16/j.intermet.2013.10.022.
  25. Tsunekane M., Suzuki A., Pollock T.M. Singe-crystal solidification of new Co−Al−W-base alloys. Intermetallics, 2011, vol. 19, pp. 636–643. DOI: 10.1016./j.intermet.2010.12.018.
  26. Petrushin N., Hvatzkiy K., Gerasimov V. et al. A single-crystal Co-base superalloy strengthened by γ′ precipitates: structure and mechanical properties. Advanced Engineering Materials, 2016, vol. 17, pp. 755−756. DOI: 10.1002/adem.201500088.
  27. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: University Press, 2006, 372 p. DOI: 10.1017/CBO9780511541285.
  28. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  29. Meher S., Nag S., Tiley J. et al. Coarsening kinetics of γʹ precipitates in cobalt-base alloys. Acta Materialia, 2013, vol. 61, pp. 4266−4276. DOI: 10.1016/j.actamat.2013.03.052.
  30. Lorez-Galilea I., Zenk C., Neumeier S. et al. The thermal stability of intermetallic compounds in an as-cast SX Co-base superalloy. Advanced Engineering Materials, 2014, vol. 17, no. 6, pp. 1–7. DOI: 10.1002/adem.201400249.
  31. Epishin A.I., Petrushin N.V., Link T., Nolze G., Loshinin Yu.V., Gershtein G. Study of thermal stability of the structure of cobalt heat-resistant alloy strengthened by intermetallic precipitates of the γ′-phase. Deformatsiya i razrushenie materialov, 2015, no. 3, pp. 17–22.
  32. Petrushin N.V., Elyutin E.S., Filonova E.V., Nazarkin R.M. High-gradient directional crystallization of Co–Al–W–Ta heat-resistant alloy strengthened by the γʹ-phase Co3(Al, W). Vestnik RFFI, 2015, no. 1 (85), pp. 11–17.
  33. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. Development of technologies and equipment for producing blades of the hot path of gas turbine engines from superalloys with directional and single-crystal structure. Trudy VIAM, 2023, no. 7 (125), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2023-0-7-3-14.
  34. Decker R.F., Sims C.T. Metallurgy of nickel-based alloys. Zharoprochnye splavy. Trans. from Engl. Moscow: Metallurgiya, 1976, pp. 39−82.
  35. Vertogradsky V.A., Kovalev A.I., Loshchinin Yu.V. High-temperature thermal analysis of heat-resistant alloys. Structural and heat-resistant materials for new technology. Moscow: Nauka, 1977, pp. 195–201.
  36. Glatzel U. Microstructure and internal strains of undeformed and creep deformed samples of a Nickel-base superalloy. Berlin: Verlag Dr. Köster, 1994, 80 p.
  37. Nabarro F.R.N. Rafting in superalloys. Metallurgical and Materials Transactions A, 1996, vol. 27, no. 3, pp. 513‒530. DOI: 10.1007/BF02648942.
  38. Xue F., Zhou H., Chen X. et al. Creep behavior of a novel Co−Al−W-base single crystal containing Ta and Ti at 982 °C. Eurosuperalloys 2014 – 2nd European Symposium on Superalloys and their Applications: MATEC Web of conferences. Giens, 2014, vol. 14, p. 15002. DOI: 10.1051/matecconf/20141415002.
  39. Mughrabi H. The importance of sign and magnitude of γ/γʹ lattice misfit in superalloys – with special reference to the new γʹ-hardened cobalt-base superalloys. Acta Materialia, 2014, vol. 81, pp. 21−29. DOI: 10.1016/j.actamat.2014.08.005.
  40. Epishin A.I., Petrushin N.V., Svetlov I.L. et al. Compression and oxidation testing of Co–Al–W–Ta single-crystal specimens directionally solidified with a flat front. Mechanics of Solids, 2024, vol. 59, no. 1, pp. 537–540. DOI: 10.1134/S0025654424602969.
  41. Tomaszewska A., Oleksiak B. Microstructural characteristics of new type γ-γ′ Co−9Al−9W cobalt-based superalloys in as-cast state. Metalurgiya, 2018, vol. 57, no. 1−2, pp. 91−94.
  42. Pyczak F., Bauer A., Göken M. et al. The effect of tungsten content on the properties of L12-hardened Co–Al–W alloys. Journal of Alloys and Compounds, 2015, vol. 632, pp. 110–115. DOI: 10.1016/j.jallcom.2015.01.031.
  43. Mishima Y., Ochiai S., Hamao N. et al. Solid solution hardening of nickel – role of transition metal and B-subgroup solutes. Transactions of the Japan Institute of Metals, 1986, vol. 27, pp. 656−664. DOI: 10.2320/matertrans1960.27.656.
  44. Saal J.E., Wolverton C. Energetics of antiphase boundaries in γ′ Co3(Al,W)-based superalloys. Acta Materialia, 2016, vol. 103, pp. 57−62. DOI: 10.1016/j.actamat.2015.10.007.
  45. Epishin A., Chyrkin A., Nolze G., Midtlyng J., Mayer H.M., Petrushin N., Reimers W. Interdiffusion in the face-centered cubic phase of the Co−Al−W−Ta system between 1090 and 1240 °C. Journal of Phase Equilibria and Diffusion, 2018, vol. 39, pp. 176–185. DOI: 10.1007/s11669-018-0620-9.
  46. Klein L., Bauer A., Neumeier S. et al. High temperature oxidation of γ/γ′-strengthened Co-base superalloys. Corrosion Science, 2011, vol. 53, pp. 2027−2034. DOI: 10.1016/j.corsci.2011.02.033.
  47. Yan H.-Y., Vorontsov V.A., Dye D. Effect of alloying on the oxidation behavior of Co−Al−W superalloys. Corrosion Science, 2014, vol. 83, pp. 382−395. DOI: 10.1016/j.corsci.2014.03.002.