Sevalnev G.S., Krasulya А.А. Study of abrasive wear of high-carbon iron-based alloy with increased nickel content after electroless boriding at low temperature // Proceedings of VIAM. 2025. No. 5 (147). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-5-88-98.

Study of abrasive wear of high-carbon iron-based alloy with increased nickel content after electroless boriding at low temperature

Sevalnev G.S., Krasulya А.А.
Abstract

In the article the microstructure, phase composition and resistance of Ni-Resist cast iron to abrasive wear without treatment and after low-temperature electrolysis-free boriding were studied. The results of the study showed that boriding using the experimental composition made it possible to form a diffusion layer with a hardness of up to 1800 HV 0,1, to increase abrasive resistance at an attack angle of 30°, while increasing the attack angle to 60 and 90° has led to a decrease in abrasive resistance.

Keywords
iron-based alloy, corrosion-resistant cast iron Ni-Resist, boriding, hardness, wear resistance, abrasion resistance, angle of attack
Reference list
  1. Ostrovsky V.G. Reliability of energy-efficient equipment «Novomet» with an increased content of mechanical impurities. Inzhenernaya praktika, 2011, no. 5, pp. 58–61.
  2. Ageev Sh.R., Savelyev K.V. How the open stage works: operation of mechanized wells in complicated conditions. Inzhenernaya praktika, 2014, no. 2, pp. 20–23.
  3. Yakimov S.B., Shportko A.A. On the influence of the concentration of abrasive particles on the service life of electric centrifugal pumps with working stages made of Ni-resist type 1 material at the fields of OJSC NK Rosneft. Territoriya Neftegaz, 2016, no. 3, pp. 84–99.
  4. Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2024-0-2-3-14.
  5. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: November 24, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  6. Bannykh I.O., Ashmarin A.A., Betzofen S.Ya. et al. Optimization of chemical composition and parameters of thermomechanical processing of TRIP steels based on new methods of X-ray tensiometry, texture and phase analysis. Metally, 2022, no. 6, pp. 66–72.
  7. Blinov V.M., Lukin E.I., Blinov E.V. et al. Tensile Fracture of Austenitic Corrosion-Resistant Steels with an Overequilibrium Nitrogen Content and Various Vanadium Contents. Russian Metallurgy (Metally), 2021, vol. 2021, is. 10, pp. 1265–1269. DOI: 10.1134/S0036029521100062.
  8. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  9. Voznesenskaya N.M., Tonysheva O.A., Eliseev E.A. Modern structural steels of cryogenic purpose and influence of some alloying elements on their properties (review). Trudy VIAM, 2020, no. 1, paper no. 01. Available at: http://www.viam-works.ru (accessed: November 24, 2024). DOI: 10.18577/2307-6046-2020-0-1-3-14.
  10. Tsikh S.G., Krasulya A.A., Pomelnikova A.S., Filimonov A.V. Low-temperature liquid boriding of Ni-resist cast iron. Uprochnyayushchie tekhnologii i pokrytiya, 2020, no. 10, pp. 468–472.
  11. Krukovich M.G., Prusakov B.A., Sizov I.G. Plasticity as the Key to the Durability of Boronized Lays. Springer series of Material Sciences. Plasticity of Boronized Layers, 2016, vol. 237, pp. 65–80.
  12. Burnyshev I.N., Valiakhmetova O.M., Mutagarova S.A. On the issue of boriding of steels. Vestnik Izhevskogo gosudarstvennogo tekhnicheskogo universiteta, 2007, no. 4, pp. 124–127.
  13. Chernov Ya.B., Filatov E.S., Karimov K.R., Chebykin V.V. Galvanic-thermodiffusion boriding of steels. Trudy Kolskogo nauchnogo tsentra RAN, 2015, no. 5 (31), pp. 300–303.
  14. Covert R., Morrison J., Roehrig K. Properties and Applications of Ni-Resist and Ductile Ni-Resist Alloys. Toronto: Nickel Development Institute, 1998, 38 p.
  15. Vinogradov V.N., Sorokin G.M., Kolokolnikov M.G. Abrasive wear. Moscow: Mashinostroenie, 1990, 224 p.
  16. Vinogradov V.N., Sorokin G.M., Shreiber G.K. Shock-abrasive wear of drill bits. Moscow: Nedra, 1975, 167 p.
  17. Mednikov A.F., Tkhabisimov A.B. Results of studies of abrasive resistance of 15Kh11MF steel at elevated temperatures. Hydraulic and heat engineering systems and units: reports XXVII Int. scientific-technical conf. Moscow: Mir nauki, 2023, pp. 161–166.
  18. Ryzhenkov A.V., Mednikov A.F., Grigoriev S.V. et al. Results of field studies of corrosion and abrasive resistance of ion-plasma coating formed on samples of tubular heating surfaces of a biofuel boiler. Teploenergetika, 2023, no. 10, pp. 34–44.
  19. Tkhabisimov A., Mednikov A., Zilova O. Studies of the Solid Particle Erosion Resistance of 30 L Steel with Different Types of Surface Modification. Metals, 2023, vol. 13, no. 12, p. 1978. DOI: 10.3390/met13121978.
  20. Method for determining the modulus of elasticity of a surface-modified layer of a metal sample: pat. BY21660C1; appl. 31.08.15; publ. 30.04.17.