Gvozdev S.S., Kurbatkina E.I., Shcherbakov E.M., Bogachev I.A. Features of granules spheroidization of different fractions of molybdenum-based high-temperature composite material // Proceedings of VIAM. 2025. No. 5 (147). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-5-38-50.

Features of granules spheroidization of different fractions of molybdenum-based high-temperature composite material

Gvozdev S.S., Kurbatkina E.I., Shcherbakov E.M., Bogachev I.A.
Abstract

The article presents the results of research and development on basic technological synthesis parameters of Mo–Si–B system metal composite material (MCM) by EBM and SLS methods. Additionally, the paper provides the investigation of the mechanisms of interface formation and diffusion processes at the interface «matrix–strengthening agent» in the process of synthesis of blanks by EBM and SLS. The powders have been analyzed by scanning electron microscope imaging, the images from which show that the powder granules have a splinter shape.

Keywords
powder sintering, heat resistance, molybdenum-silicon-boron material, metal composite material, selective laser sintering, selective electron-beam melting, powder spheroidization, GTE turbine
Reference list
  1. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 25, 2024). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  2. Startsev N.I., Falaleev S.V. Design of aircraft engine units: turbine and combustion chamber: course of lectures. Samara: SSAU Publ. house, 2007, 102 p.
  3. Tansug G. Synergistic inhibition effect between 4-amino-5-methyl-4H-1,2,4-triazole-3-thiol, citrate ions and polycarboxylate for corrosion protection of C1010 steel in cooling water system. Journal of Adhesion Science and Technology, 2017, vol. 31, is. 18, pp. 2053–2070.
  4. Serpova V.M., Nyafkin A.N., Kurbatkina E.I. Hybrid metal matrix composites based on copper (review). Trudy VIAM, 2022, no. 1 (107), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 28, 2024). DOI: 10.18577/2307-6046-2022-0-1-76-87.
  5. Serpova V.M., Sidorov D.V., Nyafkin A.N., Kurbatkina E.I. Hybrid metal matrix compo-sites based on aluminum alloys (review). Trudy VIAM, 2021, no. 3 (97), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 28, 2024). DOI: 10.18577/2307-6046-2021-0-3-68-77.
  6. Kablov E.N., Shchetanov B.V., Bolshakova A.N., Efimochkin I.Yu., Shcherbakov E.M. Niobium reinforced by α-Al2O3 fibers. Part 1. Two-Component Compositions. Aviation materials and technologies, 2021, no. 3 (64), paper no. 06. Available at: http://www.journal.viam.ru (accessed: October 25, 2024). DOI: 10.18577/2713-0193-2021-0-3-58-77.
  7. Laptev A.B., Akhiyarov R.J., Lapteva A.A., Puzanov A.I., Zagorskikh O.A. Distribution of chloride ions along the flight path of aircraft (Overview). Journal of Physics: Conference Series: III International Conference on Metrological Support of Innovative Technologies (ICMSIT-III-2022). Krasnoyarsk: IOP Publishing Ltd, 2022, vol. 2373, p. 22008. DOI: 10.1088/1742-6596/2373/2/022008.
  8. Movenko D.A., Laptev A.B., Zagorskikh O.A. Composition and Morphology of Hot-Salt Corrosion in Heat-Resistant Nickel Alloys. Inorganic Materials: Applied Research, 2022, vol. 13, no. 6, pp. 1652–1657. DOI: 10.1134/s207511332206017x.
  9. Yukhvid V.I., Andreev D., Sanin V.N., Sachkova N. SHS Metallurgy of Composite Materials Based on the Nb–Si System. Russian Journal of Non-Ferrous Metals, 2018, vol. 59, no. 1, pp. 42–49. DOI: 10.3103/S1067821218010169.
  10. Getsov L.B., Shelyapina N.M., Laptev A.B., Puzanov A.I. Sulfide Oxide Corrosion of Modern Heat-Resistant Alloys. Russian Aeronautics, 2019, vol. 62, no. 4, pp. 689–695. DOI: 10.3103/S1068799819040214.
  11. Getsov L.B., Balandina M.Y., Laptev A.B., Movenko D.A., Puzanov A.I., Pivovarova M.V. Study of metal powder alloy KhN56KVMTYuB for gas turbine engine disks under aggressive action of a mixture of sodium chlorides and sulfates. Metallovedenie i termicheskaya obrabotka metallov, 2021, no. 7 (793), pp. 19–25. DOI: 10.30906/mitom.2021.7.19-25.
  12. Getsov L.B., Balandina M.Y., Grishchenko A.I., Laptev A.B., Puzanov A.I. Rehbinder effect in testing heat-resistant alloys in contact with molten salts. Zavodskaya laboratoriya. Diagnostika materialov, 2021, vol. 87, no. 10, pp. 54–62. DOI: 10.26896/1028-6861-2021-87-10-54-62.
  13. Getsov L.B., Balandina M.Y., Laptev A.B., Movenko D.A. A Study of Metal-Powder Alloy KhN56KVMTYuB for GTE Disks Under Aggressive Impact of Sodium Chlorides and Sulfates. Metal Science and Heat Treatment, 2021, vol. 63, no. 7–8, pp. 363–368. DOI: 10.1007/s11041-021-00696-4.
  14. Iveković A., Omidvari N., Vrancken B. et al. Selective laser melting of tungsten and tungsten alloys. International Journal of Refractory Metals & Hard Materials, 2018, no. 72, pp. 27–32. DOI: 10.1016/j.ijrmhm.2017.12.005.
  15. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: October 28, 2024). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  16. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.
  17. Benarieb I., Antipov V.V., Khasikov D.V., Oglodkov M.S., Savichev I.D., Kuznetsova P.E. Study of structure and properties of sparinly alloyed aluminum alloy of Al–Mg–Sc–Zr system, produced by selective laser melting. Aviation materials and technologies, 2023, no. 4 (73), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 25, 2024). DOI: 10.18577/2713-0193-2023-0-4-23-35.
  18. Mazalov I.S., Mazalov P.B., Suhov D.I., Sulyanova E.A. Influence of hot isostatic pressing parameters on structure and properties of cobalt-based alloys obtained by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 01. Available at: http://www.journal.viam.ru (accessed: October 25, 2024). DOI: 10.18577/2713-0193-2021-0-2-3-14.
  19. Bobrovskiy A.P., Efimochkin I.Yu., Bolshakova A.N., Khudnev A.A. Production of spherical granules of a high-temperature metal composite material based on molybdenum. Trudy VIAM, 2022, no. 1 (107), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 25, 2024). DOI: 10.18577/2307-6046-2022-0-1-44-52.
  20. Berezina E.P., Nikiforov S.A., Gilmutdinov A.Kh. Numerical modeling of gas-powder flows of an installation for plasma spheroidization of metal powders. Matematicheskie metody v tekhnologiyakh i tekhnike, 2024, no. 3, pp. 55–60.