Pavlova T.V., Kashapov O.S., Chuchman O.V., Goncharova L.J. Comparative analysis of mechanical properties of the material of VT6 alloy forgings, manufactured by various methods and production conditions // Proceedings of VIAM. 2025. No. 5 (147). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-5-25-37.
Comparative analysis of mechanical properties of the material of VT6 alloy forgings, manufactured by various methods and production conditions
Abstract
The article presents the mechanical properties of blades forgings from VT6 alloy, manufactured using three methods – a bulk stamping followed by single-stage annealing; a combination of a high-temperature annealing stage with heating for calibration and subsequent aging, as well as the high-temperature thermomechanical treatment method, which consists of heating for stamping, stamping calibration followed by quenching in water and aging. Particular attention in the article is paid to the characteristics of plasticity and impact toughness, as well as fatigue strength, taking into account the current issues of ensuring the reliability of the material of the first stages of compressor blades of aircraft engines.
Keywords
titanium alloys VT6 and Ti6-4, microstructure, mechanical properties, thermomechanical treatment method, compressor blades and disks
Reference list
- Duyunova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), paper no. 02. Available at: http://www.journal.viam.ru (accessed: November 29, 2024). DOI: 10.18577/2713-0193-2023-0-2-23-35.
- Kalashnikov V.S., Reshetilo L.P., Chuchman O.V., Naprienko S.A. Strength and reliability of rods and rotor blade stamps made of heat-resistant industrial titanium alloys and modern pseudo-α-titanium alloy. Trudy VIAM, 2022, no. 2 (108), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 29, 2024). DOI: 10.18577/2307-6046-2022-0-2-13-31.
- Sviridov A.V., Gribkov М.S. Features of repair of welded structures of large thicknesses from titanium alloy VT6ch. Trudy VIAM, 2021, no. 11 (105), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 29, 2024). DOI: 10.18577/2307-6046-2021-0-11-34-43.
- Kablov E.N. Materials and technologies of VIAM for «Aviadvigatel». Permskie aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
- Solonina O.P., Glazunov S.G. Modern heat-resistant titanium alloys and prospects for their application in engines. Moscow: Metallurgiya, 1974, 448 p.
- Ezhov A.O. Periodization of the formation and development of the titanium industry in Russia: historiography of the problem. Vestnik TGU, 2015, no. 11 (151). Available at: https://cyberleninka.ru/article/n/periodizatsiya-stanovleniya-i-razvitiya-titanovoy-promyshlennosti-rossii-istoriografiya-problemy (accessed: December 06, 2024).
- Fedorov A.A., Bespalov A.V., Komarov R.S., Khairutdinova R.R. Superplastic deformation of titanium alloy VT6s as part of composite material VT6s-1201 under high hydrostatic pressures. Tekhnologiya legkikh splavov, 2023, no. 1, pp. 70–79.
- Gadalov V.N., Petrenko V.R., Kutepov S.N., Filonovich A.V., Gubanov O.M., Kalinin A.A. Bimetallic hollow titanium-aluminum panels manufactured by diffusion welding in vacuum. Izvestiya TulGU. Tekhnicheskiye nauki, 2023, no. 9, pp. 640–645.
- Dobrynin D.A. Electrolytic-plasma polishing of titanium alloys VT6 and VT8M-1. Trudy VIAM, 2017, no. 7 (55), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 07, 2024). DOI: 10.18577/2307-6046-2017-0-7-2-2.
- Lekarev A.V., Yurchuk L.I., Merkulova G.A. Study of the influence of alpha-forming on the structure and properties of VT6 alloy. Sibirskiy aerokosmicheskiy zhurnal, 2023, no. 3. Available at: https://cyberleninka.ru/article/n/issledovanie-vliyaniya-alfirovaniya-na-strukturu-i-svoystva-splava-vt6 (accessed: December 07, 2024).
- Zolotov A.M., Chizhik T.A., Smirnov M.O. Construction of third-order recrystallization diagrams of VT6 titanium alloy. Globalnaya energiya, 2017, no. 4, pp. 118–126.
- Egorova Yu.B., Davydenko L.V., Chibisova E.V., Chelpanov A.V., Karataeva E.S. Prediction of mechanical properties of rods made of titanium alloy VT6 with different types of structure. Tekhnologiya legkikh splavov, 2022, no. 3, pp. 30–40.
- Panin P.V., Dzunovich D.A. Effect of cooling rate on phase composition and structure of VT6 titanium alloy after hydrogenating annealing. Trudy VIAM, 2017, no. 10 (58), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 07, 2024). DOI: 10.18577/2307-6046-2017-0-10-4-4.
- Ji H., Zhanshuo P., Xiaomin H. et al. Dynamic recrystallization of Ti‒6Al‒4V titanium alloy based on cellular automata. Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, 2023, vol. 237, pp. 1–18. DOI: 10.1177/09544089221125575.
- Zhang J., Li H., Zhan M. Review on globularization of titanium alloy with lamellar colony. Manufacturing Review, 2020, vol. 7 (18). Available at: https://mfr.edp-open.org (accessed: March 17, 2024). DOI: 10.1051/mfreview/2020015.
- Du S., Song Y., He Y. et al. Evolution of Microstructure and Mechanical Properties of Ti‒6Al‒4V Alloy under Heat Treatment and Multi-Axial Forging. Materials, 2024, vol. 17, p. 1060. DOI: 10.3390/ma17051060.
- Seo S., Jung M., Park J. Microstructure Control for Enhancing the Combination of Strength and Elongation in Ti‒6Al‒4V through Heat Treatment. Metals, 2024, vol. 14, p. 985. DOI: 10.3390/met14090985.
- Jadhav S., Powar A., Patil S. et al. Effect of volume fraction of alpha and transformed beta on the high cycle fatigue properties of bimodal Ti6Al4V alloy. 7th International Conference on Key Engineering Materials (ICKEM 2017). IOP Conf. Series: Materials Science and Engineering, 2017, vol. 201, pp. 1–6. DOI: 10.1088/1757-899X/201/1/012035.
- Oglodkov M.S., Kashapov O.S., Kalashnikov V.S., Kondratieva A.R. Comparative analysis of the characteristics of domestic alloys VT8, VT8M, VT8M-1, VT9 and Ti6242S alloy (USA) as applied to high-pressure compressor blades of aircraft gas turbine engines. Aviation materials and technologies, 2024, no. 1 (74), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 07, 2024). DOI: 10.18577/2713-0193-2024-0-3-35-50.