Shiryaev A.A., Arislanov A.A., Putyrskiy S.V., Vostrikov N.F. Experience of using additive manufacturing waste in the production of porous semi-finished products from titanium alloys VT1-00 and VT6 // Proceedings of VIAM. 2025. No. 4 (146). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-4-14-27.

Experience of using additive manufacturing waste in the production of porous semi-finished products from titanium alloys VT1-00 and VT6

Shiryaev A.A., Arislanov A.A., Putyrskiy S.V., Vostrikov N.F.
Abstract

The article presents the results of studies of the structure and physical and mechanical properties of porous half-blanks manufactured by sintering in vacuum furnaces from powder of VT1-00 and VT6 titanium alloys. It is shown that the designed mode provides the level of mechanical properties and the degree of porosity of semi-finished products sufficient for use in the aerospace industry, energy and food industries. Samples of products were manufactured from porous semi-finished products of titanium alloys VT1-00 and VT6 using high-temperature soldering technology to form permanent joints.

Keywords
titanium alloys, cellular semi-finished products, heat treatment, microstructure, X-ray computed tomography, mechanical properties
Reference list
  1. Banhart J. Manufacture, characterisation and application of cellular metals and metal foams. Progress in Materials Science, 2001, vol. 46, pp. 559–632.
  2. Khokhlov M.A., Ishchenko D.A. Structural ultra-light porous metals (review). Avtomaticheskaya svarka, 2015, no. 3–4, pp. 60–65.
  3. Cabezas-Villa J.L., Olmos L., Bouvard D. et al. Processing and properties of highly porous Ti6Al4V mimicking human bones. Journal of Materials Research, 2018, vol. 33, pp. 650–661. DOI: 10.1557/jmr.2018.35.
  4. Tang E., Zhang X., Han Y. Experimental research on damage characteristics of CFRP/aluminum foam sandwich structure subjected to high velocity impact. Journal of Materials Research and Technology, 2019, vol. 8 (5), pp. 4620–4630.
  5. Valanezhad A., Savabi O., Nejatidanesh F. et al. The Effect of Vacuum Leak Rate on Sintering of Porous Titanium Scaffold. e-Journal of Surface Science and Nanotechnology, 2019, vol. 17, pp. 184−188. DOI: 10.1380/ejssnt.2019.184.
  6. Oh I.-H., Nomura N., Hanada S. Microstructures and Mechanical Properties of Porous Titanium Compacts Prepared by Powder Sintering. Materials Transactions, 2002, vol. 43, no. 3, pp. 443–446.
  7. Kato K., Yamamoto A., Ochiai S. et al. Cell Proliferation, Corrosion Resistance and Mechanical Properties of Novel Titanium Foam with Sheet Shape. Materials Transactions, 2012, vol. 53, no. 4, pp. 724–732.
  8. Parveez B., Jamal N.A., Anuar H. et al. Microstructure and Mechanical Properties of Metal Foams Fabricated via Melt Foaming and Powder Metallurgy Technique: A Review. Materials, 2022, vol. 15, art. 5302. DOI: 10.3390/ma15155302.
  9. Jain H., Mondal D.P., Gupta G. et al. Microstructure and high temperature compressive deformation in lightweight open cell titanium foam. Manufacturing Letters, 2021, vol. 27, pp. 67–71.
  10. Jha N., Mondal D.P., Majumdar J.D. et al. Highly porous open cell Ti-foam using NaCl as temporary space holder through powder metallurgy route. Materials and Design, 2013, vol. 47, pp. 810–819.
  11. Ye B., Dunand D.C. Titanium foams produced by solid-state replication of NaCl powders. Materials Science and Engineering A, 2010, vol. 528, pp. 691–697.
  12. Bolzoni L., Ruiz-Navas E.M., Zhang D., Gordo E. Modification of Sintered Titanium Alloys by Hot Isostatic Pressing. Key Engineering Materials, 2012, vol. 520, pp. 63–69.
  13. Nakamura T., Gnyloskurenko S.V., Sakamoto K. et al. Development of New Foaming Agent for Metal Foam. Materials Transactions, 2002, vol. 43, no. 5, pp. 1191–1196.
  14. Yue X.-Z., Matsuo K., Kitazono K. Compressive Behavior of Open-Cell Titanium Foams with Different Unit Cell Geometries. Materials Transactions, 2017, vol. 58, no. 11, pp. 1587–1592.
  15. Yue X.-Z., Fukazawa H., Maruyama K. et al. Effect of Post Heat Treatment on the Mechanical Properties of Porous Ti‒6Al‒4V Alloys Manufactured through Powder Bed Fusion Process. Materials Transactions, 2019, vol. 60, no. 1, pp. 74–79.
  16. Nakajima H. Fabrication, properties, and applications of porous metals with directional pores. Proceedings of Japan Academy, Series B, 2010, vol. 86, no. 9, pp. 884–899.
  17. Li J.P., Li S.H., Van Blitterswijk C.A., de Groot K. A novel porous Ti6Al4V: Characterization and cell attachment. Journal of Biomedical Materials Research, Part A, 2005, vol. 73A, is. 2, pp. 223–233. DOI: 10.1002/jbm.a.30278.
  18. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  19. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference book. Moscow: VILS-MATI, 2009, 520 p.
  20. Titanium and titanium alloys. Fundamentals and applications. Ed. C. Leyens, M. Peters. Wiley–VCH, 2003, 513 p.
  21. Ageev S.V., Gurshov V.L. Hot isostatic pressing in powder matallurgy. Metalloobrabotka, 2015, no. 4 (88), pp. 56–60.
  22. Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. Practical guide to metallography of titanium-based alloys and its intermetallics: tutorial. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
  23. Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  24. Yakovlev A.L., Arislanov A.A., Putyrsky S.V., Nochovnaya N.A. Study of mechanical properties and structure of large-sized semi-finished products made of VT6ch titanium alloy. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-4-12-18.
  25. Krokhina V.A., Arislanov А.A., Putyrskiy S.V., Anisimova A.Yu. Investigation of the regularities of the formation of the structure of rods made of titanium alloy VT6 depending on various technological schemes of manufacture. Aviation materials and technologies, 2023, no. 4 (73), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 07, 2024). DOI: 10.18577/2713-0193-2023-0-4-36-44.
  26. Putyrskiy S.V., Plokhikh А.I., Arislanov А.A., Naprienko S.A., Anisimova A.Yu. Study of structure and mechanical properties of the laminar structure material based on titanium alloys VT1-0 and VT47. Aviation materials and technologies, 2023, no. 2 (71), paper no. 03. Available at: http://www.journal.viam.ru (accessed: October 07, 2024). DOI: 10.18577/2713-0193-2023-0-2-36-50.
  27. Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanasyev-Khodykin A.N. Study of finely dispersed solder powders for diffusion vacuum brazing obtained by melt atomization. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie, 2011, no. SP2, pp. 79–87.
  28. Kablov E.N., Lukin V.I., Ospennikova O.G. Welding and brazing in the aerospace industry. Reports All-Russian scientific-practical conf. «Welding and Safety». Yakutsk: IPTPS SB RAS, 2012, рp.21–30.