Sevostyanov N.V., Budanova E.S., Khvatov V.D., Fomichev A.N. Tribotechnical features of metal composite materials reinforced with nitrides // Proceedings of VIAM. 2025. No. 2 (144). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-2-100-111.

Tribotechnical features of metal composite materials reinforced with nitrides

Sevostyanov N.V., Budanova E.S., Khvatov V.D., Fomichev A.N.
Abstract

The paper presents the results of experimental determination of friction coefficient and wear rate of nitride-reinforced nickel and copper matrix CMs in friction pairs with different steel grades under varying load and sliding speed. It is shown that irrespective of the matrix material, nitride-reinforced MCMs have a high friction coefficient. At low sliding velocities and load, the adhesion mechanism of friction prevails, but with the increase of these parameters, the share of abrasion mechanism of friction increases. As an additional study, the structures of the investigated MCMs were analyzed.

Keywords
coefficient of friction, wear, metal composite material, nitrides, tribology, antifriction
Reference list
  1. Burkovskaya N.P., Sevostyanov N.V. Cermets for plain bearings (review). Trudy VIAM, 2023, no. 3 (121), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 26, 2024). DOI: 10.18577/2307-6046-2023-0-3-84-94.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik RAN, 2020, vol. 90, no. 4, pp. 331–334.
  3. Nitrides: guidelines for students of mechanical specialties. Comp. A.E. Ivantsov, G.A. Rozhkova. Kazan: KSTU, 2006, 20 p.
  4. Manegin Yu.V., Gulyaev I.A., Kolesnikova O.Yu., Omelchenko A.V. Powder steels and alloys with nitride hardening. Tekhnologiya metallov, 2002, no. 12, pp. 5–12.
  5. Kardonina N.I., Kolpakova A.S. Study of the phase and structural composition of high-nitrogen iron-based powders. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya, 2000, no. 2, pp. 15–18.
  6. Komarova A.I., Vityaz P.A., Komarova V.I. Improving the tribomechanical properties of MAO coatings by modifying them with titanium nitride. VIII Int. scientific and technical. conf. «High technology at the current stage of mechanical engineering development». Moscow, 2016, pp. 89–92.
  7. Kharina G.V., Anakhov S.V. Chemical properties of structural metals and alloys: textbook. Ekaterinburg: RSVPPU, 2019, 152 p.
  8. Mikhailenko Ya.I. Course of general and inorganic chemistry. Moscow: Vysshaya shkola, 1966, 664 p.
  9. Artemyev A.A. Formation of the structure of abrasion-resistant alloys under the influence of ultrafine titanium nitride particles. XIV Rus. annual conference of young researchers and postgraduates «Physical chemistry and technology of inorganic materials». Moscow: IMET RAS, 2017, pp. 7–9.
  10. Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B. Trudy VIAM, 2022, no. 10 (116), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 16, 2024). DOI: 10.18577/2307-6046-2022-0-10-76-89.
  11. Burkovskaya N.P., Sevostyanov N.V., Bolsunovskaya T.A., Efimochkin I.Yu. Improvement of materials for sliding bearings of internal combustion engines (review). Trudy VIAM, 2020, no. 1 (85), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 16, 2024). DOI: 10.18577/2307-6046-2020-0-1-78-91.
  12. Evgenov A.G., Shurtakov S.V., Chumanov I.R., Leshchev N.E. New wear-resistant cobalt-based alloy: effect of silicon and carbon on structure and tribotechnical characteristics. Part 1. Aviation materials and technologies, 2021, no. 4 (65), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 16, 2024). DOI: 10.18577/2713-0193-2021-0-4-59-69.
  13. Starunov A.V., Astakhova M.N., Balakai V.I. New composite material based on nickel-cobalt alloy containing silicon oxide as an alloying component. XII Int. Sci.-prac. conf. «Modern instrumental systems, information technologies and innovations»: in 4 vols. Kursk, 2015, vol. 4, pp. 88–90.
  14. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  15. Smirnov V.M., Shalunov E.P. Properties and structure of composite metal matrix materials based on powder copper obtained by reactive mechanical alloying. VII Int. Conf. «Deformation and destruction of materials and nanomaterials». Moscow: IMET RAS, 2017, pp. 437–439.
  16. Lovshchenko F.G., Lovshchenko G.F., Fedosenko A.S. Regularities of formation of structure and phase composition of mechanically alloyed composite powder materials for gas-thermal spraying methods. Vestnik Belorussko-Rossiyskogo universiteta, 2016, no. 1 (50), pp. 36–47.
  17. Chernigovskaya M.A., Pozdnyakova V.G. On the method for determining the structure of polymer composite materials. Sovremennye tekhnologii i nauchno-tekhnicheskiy progress, 2022, no. 9, pp. 77–78.
  18. Kuksenova L.I., Lapteva V.G., Kolmakov A.G., Rybakova L.M. Friction and Wear Test Methods. Moscow: Intermet Inzhiniring, 2001, 152 p.
  19. Buckley D. Surface Phenomena in Adhesion and Frictional Interaction. Moscow: Mashinostroenie, 1986, 359 p.
  20. Kragelsky I.V., Dobychin M.N., Kombalov V.S. Fundamentals of friction and wear calculations. Moscow: Mashinostroenie, 1987, 526 p.
  21. Litvinov V.N., Mikhin N.M., Myshkin N.K. Physicochemical Mechanics of Selective Transfer during Friction. Moscow: Nauka, 1979, 187 p.
  22. Bely A.V. Structure and Methods of Formation of Wear-Resistant Surface Layers. Moscow: Mashinostroenie, 1991, 208 p.
  23. Rybakova L.M., Kuksenova L.I. Structure and Wear Resistance of Metal. Moscow: Mashinostroenie, 1982, 216 p
  24. Kislyi P.S., Bodnaruk N.I., Borovikova M.S. et al. Cermets. Kyiv: Naukova Dumka, 1985, 272 p.
  25. Kudrya A.V., Sokolovskaya E.A., Perezhogin V.Yu., Ha N.N. Some practical considerations related to computer procedures for image processing in materials science. Vektor nauki Tolyattinskogo gosudarstvennogo universiteta, 2019, no. 4 (50), pp. 35–44.