Abstract

The article considers the main directions of application of catalysts for oil refining processes, including those for the import substitution. Some properties of a high-porous material based on oxide fiber are demonstrated, revealing the prospect of using this class of material as catalyst carrier. The water front movement in a fibrous high-porous material has been studied by the magnetic resonance imaging (MRI process). It has been shown that thermal activation of the fiber surface increases the sorption capacity of the material.

Keywords
fibrous high-porous material, catalyst, sorption capacity, specific surface area
Reference list
  1. Kapustin V.M., Ivanov A.V. Production of catalysts for oil refining and petrochemistry in Russia. Neftegaz.RU, 2023, no. 9 (141). Available at: https://magazine.neftegaz.ru/articles/
  2. importozameshchenie/795285-proizvodstvo-katalizatorov-dlya-neftepererabotki-i-neftekhimii-v-rossii (accessed: January 25, 2025).
  3. Abatayeva A.U., Alangiraeva H.D. Import substitution is a priority direction for the development of the catalyst industry. Vestnik magistratury. Khimicheskie nauki, 2022, no. 10–3 (133), pp. 8–11.
  4. Review of the oil refining catalyst market in Russia and the CIS countries. INFOMINE Research Group. Available at: https://infomine.ru/files/catalog/644/file_644_eng.pdf (accessed: January 25, 2025).
  5. Oil refineries of Russia and the CIS countries: reference book. Moscow: OMT-Consult, 2018, 155 p.
  6. Catalog of oil refineries and gas processing plants (OR/GPP). LNG projects facilities of the CIS. Energybase. Available at: https://clck.ru/TKVdn (accessed: January 25, 2025).
  7. Noskov A.S. Scientific and technical level of researches and import substitution perspective in the field of industrial catalysts. Herald of the Russian Academy of Sciences, 2022, vol. 92. no. 10. рр. 940–949.
  8. Leffler W.L. Oil refining. 2nd ed., rev. trans. from Engl. Moscow: Olimp-Business, 2004, 224 p.
  9. Method for processing gasolines from thermal processes and a catalyst for its implementation: pat. 2469070 Rus. Federation; appl. 13.10.11; publ. 10.12.12.
  10. Bodryi A.B., Rakhmatullin E.M., Ilibaev R.S., Garieva G.F. On new granular catalysts for catalytic cracking. Kataliz v promyshlennosti, 2014, no. 5, p. 20.
  11. Ivanchina E.D., Ivashkina E.N., Nazarova G.Yu. et al. Development of a kinetic model of the catalytic cracking process. Kataliz v promyshlennosti, 2017, no. 6, pp. 477–486.
  12. Chorkendorff I., Naimantsvedreit H. Modern Catalysis and Chemical Kinetics. Trans. from Engl. Dolgoprudny: Intellekt, 2010, 500 p.
  13. Stiles E.B. Carriers and Supported Catalysts. Theory and Practice. Moscow: Khimiya, 1991, 240 p.
  14. Ryabov V.D. Chemistry of Oil and Gas: Textbook for Universities. Moscow: «Tekhnika» GUMA GROUP, 2018, 288 p.
  15. Solodova N.L., Terentyeva N.A. Current status and development trends of catalytic cracking of petroleum feedstocks. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, vol. 15, no. 1, pp. 141–147.
  16. Gilmutdinov A.T., Khisamova L.Z. Review of modern catalysts used in catalytic cracking processes. Ufa: Ufa State Petroleum Tech. Univ., 2019, pp. 11–13.
  17. Sedghi R.B.F., Kapustin V.M., Gerzeliev I.M., Tretyakov V.F. Study of the effect of ZSM-5 additives to cracking catalysts to increase the yield of light olefins and propylene. Kataliz v promyshlennosti, 2012, no. 6, pp. 33–38.
  18. Doronin V.P., Lipin P.V. Promising developments: cracking catalysts and additives to them. Kataliz v promyshlennosti, 2018, no. 5, pp. 82–87.
  19. Oil and gas processing technology. Tehnoinfa. Available at: http://www.tehnoinfa.ru/
  20. pererabotkaneftiigaza/21.html (accessed: January 31, 2025).
  21. Akhmetov S.A. Technology of deep oil and gas processing: textbook for universities. Ufa: Gilem, 2002, 672 p.
  22. Parkash S. Handbook of oil refining. Trans. from Engl. Eds I.A. Belyaev, V.N. Lyndin. Moscow: Premium Inzhiniring, 2012, 759 p.
  23. Lamberov A.A., Egorova S.R. Industrial implementation of developments from the experience of cooperation with PJSC NIZHNEKAMSKNEFTEKHIM. Kataliz v promyshlennosti, 2022, no. 2, pp. 76–86. DOI: 10.18412/1816-0387-2022-2-76-86.
  24. Wang Zh., Gao J., Chang K. et al. Manufacturing of open-cell aluminum foams via infiltration casting in super-gravity fields and mechanical properties. RSC Advances, 2018, vol. 8, pp. 15933–15939. DOI: 10.1039/C7RA13689G.
  25. Antipov V.V., Varrik N.M., Maksimov V.G., Lugovoy A.A., Babashov V.G., Shavnev A.A. Study of mechanical and thermal characteristics of a porous ceramic material based on mullite. Trudy VIAM, 2023, no. 6 (124), paper no. 04. Available at: http://www.viam-works.ru (accessed: January 23, 2025). DOI: 10.18577/2307-6046-2023-0-6-38-45.
  26. Babashov V.G., Butakov V.V., Kolyshev S.G., Maksimov V.G. Research of the unevenness of distribution of the strength properties of high-temperature thermal insulation materials. Trudy VIAM, 2021, no. 6 (100), paper no. 12. Available at: http://www.viam-works.ru (accessed: January 23, 2025). DOI: 10.18577/2307-6046-2021-0-6-123-134.
  27. Morozov E.V., Koptyug I.V., Bouznik V.M. NMR Imaging as an instrument for study and diagnostics of composite materials and articles on their base. Aviacionnye materialy i tehnologii, 2014, no. S1, pp. 17–29. DOI: 10.18577/2071-9140-2014-0-s1-17-29.
  28. Avilova I.A., Bouznik V.M., Volkov V.I., Zhelezina G.F., Morozov E.V., Raskutin A.E., Falaleev O.V. Study of interaction of polymer composite materials with water using nuclear magnetic resonance methods. Aviacionnye materialy i tehnologii, 2014, no. S1, pp. 30–36. DOI: 10.18577/2071-9140-2014-0-s1-30-36.
  29. Koptyug I.V. MRI of mass transport in porous media: Drying and sorption processes. Progress in Nuclear Magnetic Resonance Spectroscopy, 2012, vol. 65, pp. 1–65. DOI: 10.1016/j.pnmrs.2011.12.001.
  30. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concen-tration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-20200-0-2-41-49.
  31. Kablov E.N., Babashov V.G., Balinova Y.A., Maksimov V.G. Phase transformations in a composite material with an organic matrix filled with zirconium dioxide fibers. High Temperature, 2021, vol. 59, no. 1, pp. 55–61.
  32. Babashov V.G., Varrik N.M., Karaseva T.A. Porous ceramic for filtration of metal melts and hot gases (rеview). Trudy VIAM, 2020, no. 8 (90), paper no. 6. Available at: http://www.viam-works.ru (accessed: January 23, 2025). DOI: 10.18577/2307-6046-2020-0-8-54-63.
  33. Morozov E.V., Buznik V.M., Bespalov A.S., Grashchenkov D.V. Magnetic resonance imaging of water absorption by highly porous ceramic materials. Doklady akademii nauk, 2019, vol. 484, no. 5, pp. 563–567. DOI: 10.31857/S0869-56524845563-567.
  34. Sahimi M. Flow and Transport in Porous Media and Fractured Rock: From Classical Methods to Modern Approaches. Second Edition. Wiley-VCH, 2011, 733 p. DOI: 10.1002/9783527636693.