Sudzhanskaya I.V., Lebedeva Yu.E., Vaganova M.L., Shchegoleva N.E. Parameters affecting on the ionic conductivity of solid electrolytes based on cerium dioxide // Proceedings of VIAM. 2025. No. 1 (143). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-1-60-73.

Parameters affecting on the ionic conductivity of solid electrolytes based on cerium dioxide

Sudzhanskaya I.V., Lebedeva Yu.E., Vaganova M.L., Shchegoleva N.E.
Abstract

Ceramic materials based on cerium dioxide are used as solid electrolytes of solid oxide fuel cells at temperatures below 600 °C. Based on the analysis of the results of existing world studies, it is shown that the ionic conductivity of doped CeO2 depends on the synthesis method, sintering temperature and time, type and concentration of alloying elements, grain size, grain boundaries and etc. Recommendations are proposed for obtaining doped cerium dioxide with an increased ionic conductivity value in the medium-temperature range for the production of solid electrolytes.

Keywords
solid electrolytes, cerium dioxide, ionic conductivity, activation energy, ion radius, blocking effect
Reference list
  1. Lyu Y., Xie J., Wang D., Wang J. Review of cell performance in solid oxide fuel cells. Journal of Materials Science, 2020, vol. 55, pp. 7184–7207.
  2. Gao Z., Mogni L.V., Miller E.C. et al. A perspective on low-temperature solid oxide fuel cells. Energy Environment Science, 2016, vol. 9, p. 1602.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Singh M., Zappa D., Comini E. Review Article: Solid oxide fuel cell: Decade of progress, future perspectives and challenges. International Journal of Hydrogen Energy, 2021, vol. 46, pp. 27643–27674. DOI: 10.1016/j.ijhydene.2021.06.020.
  5. Irshad M., Siraj K., Raza R. et al. A Brief Description of High Temperature Solid Oxide Fuel Cell’s Operation, Materials, Design, Fabrication Technologies and Performance. Applied Sciences, 2016, vol. 6, p. 75.
  6. Mahmud L.S., Muchtar A., Somalu M.R. Challenges in fabricating planar solid oxide fuel cells: A review. Renewable and Sustainable Energy Reviews, 2017, vol. 72, pp. 105–116.
  7. Kablov E.N., Karachevtsev F.N., Shilov A.L. et al. Thermodynamics and vaporization of ceramics based on the Gd2O3–ZrO2 and Gd2O3–HfO2 systems studied by kems. Journal of Alloys and Compounds, 2022, vol. 908, p. 164575. DOI: 10.1016/j.jallcom.2022.164575.
  8. Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering temperature and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
  9. Lebedeva Yu.E., Chainikova A.S., Shchegoleva N.E., Belyachenkov I.O., Turchenko M.V. Synthesis and study of the properties of yttrium oxide sols. Trudy VIAM, 2023, no. 2 (120), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 29, 2024). DOI: 10.18577/2307-6046-2023-0-2-32-41.
  10. Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 29, 2024). DOI: 10.18577/2307-6046-2021-0-4-61-73.
  11. Belyachenkov I.O., Schegoleva N.E., Chainikova A.S., Vaganova M.L., Shavnev A.A. The influ-ence of sintering and modifying additives on the sintering process and the properties of silicon nitride ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 70–78. DOI: 10.18577/20-71-9140-2020-0-1-70-78.
  12. Ramos-Alvarez P., Villafuerte-Castrejo´n M.E., Gonza´lez G. et al. Ceria-based electrolytes with high surface area and improved conductivity for intermediate temperature solid oxide fuel cells. Journal of Materials Sciences, 2017, vol. 52, pp. 519–532.
  13. Anjaneya K.C., Nayaka G.P., Manjanna J. et al. Preparation and characterization of Ce1‒xGdxO2‒d (x = 0,1–0,3) as solid electrolyte for intermediate temperature SOFC. Journal of Alloys and Compounds, 2013, vol. 578, pp. 53–59. DOI: 10.1016/j.jallcom.2013.05.010.
  14. Sudzhanskaya I.V., Nekrasova Yu.S., Kubankin A.S. Effect of the composition of the ceramics (MCeMgSr)O2‒δ (M = Y, Sm) on the microstructure, mechanical and electrical properties for solid electrolyte. Crystals, 2022, vol. 12, p. 1198.
  15. Nakayama M., Martin M. First-principles study on defect chemistry and migration of oxide ions in ceria doped with rare-earth cations. Physical Chemical Chemistry Physics, 2009, vol. 11, pp. 3241–3249.
  16. Anirban S.K., Paul T., Dutta A. Vacancy mediated ionic conduction in Dy substituted nanoceria: a structure-property correlation study. RSC Advances, 2015, vol. 5, pp. 50186–50195.
  17. Anirban S.K., Dutta A. Revisiting ionic conductivity of rare earth doped ceria: Dependency on different factors. International Journal of Hydrogen Energy, 2020, vol. 45, is. 46, pp. 25139–25166. DOI: 10.1016/j.ijhydene.2020.06.119.
  18. Anirban S.K., Banerjee A., Dutta A. Synthesis route dependent structure, conductivity and dielectric properties of Ce0,8Gd0,2O1,9 oxygen ion conductor: A comparative approach. International Journal of Hydrogen Energy, 2020, vol. 46, pp. 8210–8225. DOI: 10.1016/j.ijhydene.2020.12.010.
  19. Kumar S.A., Kuppusami P., Amirthapandian S., Fu Y.-P. Effect of Sm co-doping on structural, mechanical and electrical properties of Gd doped ceria solid electrolytes for intermediate temperature solid oxide fuel cells. International Journal of Hydrogen Energy, 2020, vol. 45, pp. 29690–29704. DOI: 10.1016/j.ijhydene.2019.10.098.
  20. Sudzhanskaya I.V., Vasiliev A.E., Yapryntsev M.N., Nekrasova Yu.S., Oleynik A.N. Influence of the method of obtaining the Ce0.8Y0.2O2‒δ solid solution on its structure and electrophysical properties. Steklo i keramika, 2022, vol. 95, no. 8, pp. 43–51. DOI: 10.14489/glc.2022.08.pp.043-051.
  21. Anjaneya K.C., Nayaka G.P., Manjanna J. et al. Studies on structural, morphological and electrical properties of Ce0,8Ln0,2O2‒δ (Ln = Y3+, Gd3+, Sm3+, Nd3+ and La3+) solid solutions prepared by citrate complexation method. Journal of Alloys and Compounds, 2014, vol. 585, pp. 594–601. DOI: 10.1016/jallcom.2013.09.101.
  22. Momin N., Manjanna J., D’Souza L. et al. Synthesis, structure and ionic conductivity of nanocrystalline Ce1‒xLaxO2‒δ as an electrolyte for intermediate temperature solid oxide fuel cells. Journal of Alloys and Compounds, 2022, vol. 896, p. 163012. DOI: 10.1016/jallcom.2021.163012.
  23. Kim G., Lee N., Kim K.-B. et al. Various synthesis methods of aliovalent-doped ceria and their electrical properties for intermediate temperature solid oxide electrolytes. International Journal of Hydrogen Energy, 2013, vol. 38, is. 3, pp. 1571–1587. DOI: 10.1016/j.ijhydene.2012.11.044.
  24. Anjaneya K.C., Manjanna J., Kumar V.M.A. et al. Rare earth ion doped ceria as electrolytes for solid oxide fuel cell. Advanced Materials Letters, 2016, vol. 7, is. 9, pp. 743–747. DOI: 10.5185/amlett.2016.6070.
  25. Dicmen S., Shuk P., Greenblatt M. Hydrothermal synthesis and properties of Ce1‒xLaxO2‒δ solid solutions. Solid State Ionics, 1999, vol. 126, pp. 89–95.
  26. Brett D.J.L., Atkinson A., Brandon N.P., Skinner S.J. Intermediate temperature solid oxide fuel cells. Chemical Society Reviews, 2008, vol. 37, pp. 1568–1578. DOI: 10.1039/b612060c.
  27. Guo T., Zhang L., Song X. et al. Influences of Gd2Ti2O7 sintering aid on the densification, ionic conductivity and thermal expansion of Gd0,1Ce0,9O0,95 electrolyte for solid oxide fuel cells. Journal of Power Sources, 2014, vol. 262, is. 15, pp. 239–244. DOI: 10.1016/j.jpowsour.2014.03.077.
  28. Zhou Y., Rahaman M.N. Effect of redox reaction on the sintering behavior of cerium oxide. Acta Materials, 1997, vol. 45, no. 9, pp. 3635–3639.
  29. Harrison R.W., Morgan J., Buckley J. et al. Development and comparison of field assisted sintering techniques to density CeO2 ceramics. Journal of European Ceramic Society, 2022, vol. 42, pp. 6599–6607. DOI: 10.1016/j.jeurceramsoc.2022.06.079.
  30. Momin N., Manjanna J., Aruna S.T. et al. Effect on 20 mol % gadolinium doping on oxide ion conductivity of ceria as electrolyte for intermediate temperature solid oxide fuel cells. Ceramics International, 2022, vol. 48, is. 23, pp. 35867–35873. DOI: 10.1016/j.ceramint.2022.08.169.
  31. Tian R., Zhao F., Chen F. Sintering of Samarium doped ceria powders prepared by a glycine-nitrate process. Solid State Ionics, 2011, vol. 192, is. 1, pp. 580–583. DOI: 10.1016/j.ssi.2010.08.003.
  32. Minh N.Q. Ceramic fuel cells. Journal of American Ceramic Society, 1993, vol. 76, pp. 563–588.
  33. Higashi K., Sonoda K., Ono H. et al. Synthesis and sintering of rare-earth-doped ceria powder by the oxalate coprecipitation method. Journal of Materials Resеarch, 1999, vol. 14, pp. 957–967.
  34. Inaba H., Nakajima T., Tagawa H. Sintering behaviors of ceria and gadolinia-doped ceria. Solid State Ionics, 1998, vol. 106, pp. 263–268.
  35. Accardo G., Frattini D., Ham H.C. et al. Improved microstructure and sintering temperature of bismuth nano-doped GDC powders synthesized by direct sol-gel combustion. Ceramics International, 2017, vol. 11, pp. 165. DOI: 10.1016/j.ceramint.2017.11.165.
  36. Baral A.K., Dasari H.P., Kim B.-K., Lee J.-H. Effect of sintering aid (CoO) on transport properties of nanocrystyalline Gd doped ceria (GDC) materials prepared by co-precipitation method. Journal of Alloys and Compounds, 2013, vol. 575, pp. 455–460. DOI: 10.1016/j.jallcom.2013.05.191.
  37. Wu Y.-C., Chen W.-Y. Fabrication and characterization of Ca2+, Sr2+, Ba2+, Sm3+, and La3+ co-doped ceria-based electrolyte powders for low-temperature anode-supported solid oxide fuel cells. International Journal of Hydrogen Energy, 2018, vol. 43, pp. 18453–18476. DOI: 10.1016/j.ijhydene.2018.08.049.
  38. Avilae Paredes H.J., Choi K., Chen C.T., Kim S. Dopant-concentration dependence of grain-boundary conductivity in ceria: a space-charge analysis. Journal of Materials Chemistry, 2009, vol. 19, pp. 4837–4842. DOI: 10.1039/b904583j.
  39. Anjaneya K.C., Nayaka G.P., Manjanna J. et al. Preparation and characterization of Ce1exGdxO2ed (x¼0.1-0.3) as solid electrolyte for intermediate temperature SOFC. Journal of Alloys and Compound, 2013, vol. 578, pp. 53–59.
  40. Kumar S.A., Kuppusami P., Amirthapandian S., Fu Y.-P. Effect of Sm co-doping on structural, mechanical and electrical properties of Gd doped ceria solid electrolytes for intermediate temperature solid oxide fuel cells. International Journal of Hydrogen Energy, 2020, vol. 45, pp. 29690–29704. DOI: 10.1016/j.ijhydene.2019.10.098.
  41. Accardo G., Audasso E., Yoon S.P. Unravelling the synergistic effect on ionic transport and sintering temperature of nanocrystalline CeO2 tri-doped with Li, Bi and Gd as dense electrolyte for solid oxide fuel cells. Journal of Alloys and Compounds, 2022, vol. 898, p. 162880. DOI: 10.1016/j.jallcom.2021.162880.
  42. Ventakaramana K., Madhuri C., Suresh Y. et al. Investigation on micro-structural, structural, electrical and thermal properties of La3+, Sm3+, Gd3+ triple-doped ceria as solid-electrolyte for intermediate temperature-solid oxide fuel cells applications. Journal of Applied Physics, 2019, vol. 126, p. 144901. DOI: 10.1063/1.5113890.
  43. Alaydrus M., Sakaue M., Aspera S.M. et al. A first-principles study on defect association and oxygen ion migration of Sm3+ and Gd3+ co-doped ceria. Journal of Physics: Condensed Materials, 2013, vol. 25, p. 225401. DOI: 10.1088/0953-8984/25/22/225401.
  44. Eguchi K., Setoguchi T., Inoue T., Arai H. Electrical properties of ceria-based oxides and their application to solid oxide fuel cells. Solid State Ionics, 1992, vol. 52, pp. 165–172.
  45. Yeh T.H., Chou C.C. Ionic conductivity investigation in samarium and strontium co-doped ceria system. Physics Scripta, 2007, vol. 129, pp. 303–307.
  46. Tschope A. Grain size-dependent electrical conductivity of polycrystalline cerium oxide II: space charge model. Solid State Ionics, 2001, vol. 139, pp. 267–280.
  47. Bae J., Lim Y., Park J.-S. et al. Thermally-induced dopant segregation effects on the space charge layer and ionic conductivity of nanocrystalline gadolinia-doped ceria. Journal of Electrochemical Society, 2016, vol. 163, pp. 919–996. DOI: 10.1149/2.1201608jes.
  48. Tian C., Chan S.W. Ionic conductivities, sintering temperatures and microstructures of bulk ceramic CeO2 doped with Y2O3. Solid State Ionics, 2000, vol. 134, pp. 89–102.
  49. Kim D.K., Cho Pe.S., Lee Je.H. et al. Mitigation of highly resistive grain – boundary phase in gadolinia – doped ceria by the addition of SrO. Electrochemical Solid-State Letters, 2007, vol. 10, pp. 91–95.
  50. Park S.Y., Cho P.S., Lee S.B. et al. Improvement of grain-boundary conduction in SiO2-doped GDC by BaO addition. Journal of Electrochemical Society, 2009, vol. 156, is. 8, pp. 891–896. DOI: 10.1149/1.3139074.