Senenko S.A., Bogachev I.A., Shoshev F.L. Effect of the fractional composition of the metal-powder composition of the VT6 alloy on the surface roughness, structure and mechanical properties of the printed material obtained by selective electron beam melting // Proceedings of VIAM. 2024. No. 6 (136). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-6-29-41.

Effect of the fractional composition of the metal-powder composition of the VT6 alloy on the surface roughness, structure and mechanical properties of the printed material obtained by selective electron beam melting

Senenko S.A., Bogachev I.A., Shoshev F.L.
Abstract

The technological properties of metal-powder compositions of VT6 alloy of different fractional composition are investigated. Synthesized samples were obtained by selective electron beam melting from metal-powder compositions of various fractions according to the standard parameters. The structure and surface roughness of the printed samples were studied. The widest possible range of fractions of the metal powder composition suitable for use in the process of selective laser electron beam melting without reducing the characteristics of the printed material has been determined.

Keywords
metal-powder composition, selective electron beam fusion, additive technologies, structure, surface roughness
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Study of the structure and properties of heat-resistant alloys based on titanium aluminides with gadolinium microadditives. Materialovedenie, 2017, no. 3, pp. 3–10.
  3. Khorev A.I. Titanium alloys for aerospace technology and the prospects for their development. Aviacionnye materialy i tehnologii, 2002, is: Promising aluminum, magnesium and titanium alloys for aerospace technology, pp. 11–32.
  4. Inozemtsev A.A., Bashkatov I.G., Koryakovtsev A.S. Titanium alloys in products developed by Aviadvigatel OJSC. Modern titanium alloys and problems of their development. Moscow: VIAM, 2010, pp. 43–46.
  5. Korner C. Additive manufacturing of metallic components by selective electron beam melting – a review. International Materials Reviews, 2016, vol. 61, no. 5, pp. 361–377.
  6. Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. Practical guide to metallography of alloys based on titanium and its intermetallic compounds: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
  7. Murr L.E., Gaytan S.M. Electron beam melting. Comprehensive materials processing, 2014, vol. 10, pp. 135–161.
  8. Wentao Y., Wenjun G., Ya Q. et al. Multi-physics modeling of single/multiple-track defect mechanisms in electron beam selective melting. Acta Materialia, 2017, vol. 134, pp. 324–333.
  9. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference book. Moscow: VILS–MATI, 2009, 520 p.
  10. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  11. Tang H.P., Qian M., Liu N. et al. Effect of powder reuse times on additive manufacturing of Ti–6AI–4V by selective electron beam melting. Journal of the minerals, metals & materials society, 2015, vol. 67 (3), pp. 555–563.
  12. Guoqing C., Binggang Z., Wei L., Jicai F. Crack formation and control upon the electron beam welding of TiAl-based alloys. Intermetallics, 2011, vol. 19, pp. 1857–1863.
  13. Dudikhin D.D., Saprykin A.A. Methods for producing of spherical powders for additive laser technologies. Masters Journal, 2016, no. 1, pp. 51–55.
  14. Knyazev A.E., Vostrikov A.V. Sieving of powders additive and powder manufacturings (review). Trudy VIAM, 2020, no. 11 (93), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 14, 2023). DOI: 10.18577/2307-6046-2020-0-11-11-20.
  15. Vrancken B., Thijs L., Kruth J.-P., Van Humbeeck J. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties. Journal of Alloys and Compounds, 2012, vol. 541, pp. 177–185.
  16. Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.
  17. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  18. Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  19. ASTM F2924-14. Standard Specification for Additive Manufacturing Titanium-6 Aluminum-4 Vanadium with Powder Bed Fusion. Available at: https://www.astm.org (accessed: October 12, 2023). DOI: 10.1520/F2924-14.
  20. Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 1. Trudy VIAM, 2020, no. 6–7 (89), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 13, 2023). DOI: 10.18577/2307-6046-2020-67-3-10.
  21. Burkovskaya N.P., Bobrovsky A.P., Efimochkin I.Yu., Bolshakova A.N. Spheroidization of powder compositions based on refractory metals (review). Part 1. Trudy VIAM, 2023, no. 1 (119), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 11, 2023). DOI: 10.18577/2307-6046-2023-0-1-128-138.