Leonov A.A., Zavarzin S.V., Trofimov N.V. On some features of the influence of the composition of the magnesium anode on its electrochemical behavior in relation to magnesium-ion batteries // Proceedings of VIAM. 2024. No. 6 (136). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-6-18-28.

On some features of the influence of the composition of the magnesium anode on its electrochemical behavior in relation to magnesium-ion batteries

Leonov A.A., Zavarzin S.V., Trofimov N.V.
Abstract

The influence of the composition of the anode made of various casting magnesium alloys on its electrochemical behavior in a solution of 3,5% NaClby galvanostatic electrolysis and electrochemical impedance spectroscopy has been studied. It has been established that the use of rare earth elements (REE) as alloying elements has a beneficial effect on discharge characteristics, which allows increasing the anode efficiency and discharge capacity of the VML26 alloy of the system Mg–REE–Zr compared to the Mg–Al–Zn alloy ML5p.ch. by 15 and 7 %, respectively.

Keywords
magnesium alloys, magnesium-ion battery, rechargeable magnesium battery, anode, electrolyte, discharge characteristics
Reference list
  1. Kulova T.L., Skundin A.M. Problems of development of lithium-ion batteries in the world and Russia. Elektrokhimicheskaya energetika, 2023, vol. 23, no. 3, pp. 111–120.
  2. Leonov A.A., Trofimov N.V. Magnesium ion batteries: prospects and challenges in the field of energy. Trudy VIAM, 2024, no. 3 (133), paper no. 04. Available at: http://www.viam-works.ru (accessed: April 25, 2024). DOI: 10.18577/2307-6046-2024-0-3-41-51.
  3. Morachevsky A.G., Popovich A.A. Magnesium-ion batteries – a new direction of research. Globalnaya energiya, 2019, vol. 25, no. 3, pp. 133–139.
  4. Dominko R., Bitenc J., Berthelot R. et al. Magnesium batteries: Current picture and missing pieces of the puzzle. Journal of power sources, 2020, no. 478, pp. 321–339.
  5. Li Q., Xiong W., Yu S.Y. et al. Effect of Gd content on the discharge and electrochemical behaviors of the magnesium alloy AZ31 as an anode for Mg-air battery. Journal of Materials Science, 2021, vol. 56, pp. 12789–12802. DOI: 10.1007/s10853-021-06135-2.
  6. Li C.S., Sun Y., Gebert F., Chou S.L. Current progress on rechargeable magnesium-air battery. Advanced Energy Materials, 2017, vol. 7, р. 1700869. DOI: 10.1002/aenm.201700869.
  7. Deng M., Wang L.Q., Hoche D. et al. Corrosion and discharge properties of Ca/Ge micro-alloyed Mg anodes for primary aqueous Mg batteries. Corrosion Science, 2020, vol. 177. DOI: 108958.10.1016/j.corsci.2020.108958.
  8. Shi M., Li T., Shang H. et al. A critical review of inorganic cathode materials for rechargeable magnesium ion batteries. Journal of Energy Storage, 2023, no. 68, pp. 216–228.
  9. Zhang T.R., Tao Z.L., Chen J. Magnesium-air batteries: from principle to application. Materials Horizons, 2014, vol. 1, pp. 196–206. DOI: 10.1039/c3mh00059a.
  10. Ma B., Ouyang L., Zheng J. Magnesium-rare earth intermetallic compounds for high performance high power aqueous Magnesium-Air batteries. Journal of Magnesium and Alloys, 2023, vol. 311, pp. 347–361. DOI: 10.1016/j.jma.2023.6.010.
  11. Mana Y., Jaumaux P., Xu Y. et al. Research development on electrolytes for magnesium-ion batteries. Science Bulletin, 2023, no. 68, pp. 1819–1842.
  12. Kablov E.N. Aviation materials science in the 21st century. Prospects and objectives. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS–VIAM, 2002, pp. 23–47.
  13. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  14. Trofimov N.V., Leonov A.A., Duyunova V.A., Uridiya Z.P. Cast magnesium alloys (review). Trudy VIAM, 2016, no. 12, paper no. 01. Available at: http://www.viam-works.ru (accessed: October 20, 2017). DOI: 10.18577/2307-6046-2016-0-12-1-1.
  15. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  16. Wang L., Wang R., Feng Y. et al. Effect of Al and Pb contents on the corrosion electrochemical properties and activation of Mg–Al–Pb alloy anode. Journal of Electrochemical Society, 2017, vol. 164, pp. A438–A446.
  17. Liu X., Liu S., Xue J. Discharge performance of the magnesium anodes with different phase constitutions for Mg-air batteries. Journal of Power Sources, 2018, vol. 396, pp. 667–674. DOI: 10.1016/j.jpowsour.2018.06.085.
  18. Bingjie Ma, Liuzhang Ouyang, Jie Zheng. Magnesium-rare earth intermetallic compounds for high performance high power aqueous Magnesium-Air batteries. Journal of Magnesium and Alloys, 2023, is. 8, pp. 1011–1025. DOI: 10.1016j.jma.2023.06.010.
  19. Wang N., Wang R., Peng C. et al. Discharge and Corrosion Performance of AP65 Magnesium Alloy in Simulated Seawater: Effect of Temperature. Journal of Materials Engineering and Performance, 2014, vol. 23, pp. 4374–4384.
  20. Feng Y., Xiong W., Zhang J.et al. Electrochemical discharge performance of the Mg–Al–Pb–Ce–Y alloy as the anode for Mg–air batteries. Journal of Materials Chemistry A, 2016, is. 22, pp. 8658–8668.
  21. Abramova M.G. Revisiting the confirmation of the identity of the corrosion destruction mechanism of aluminum alloys (review). Part 1. Atmospheric corrosion. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-4-86-94.
  22. Fomina M.A., Zakharov K.E., Yamshchikov E.I., Trofimov N.V. Selection and research of optimal paste formulation for local removal of corrosion products from magnesium alloys as well as the technology of it’s application. Aviation materials and technologies, 2023, no. 4 (73), paper no. 05. Available at: http://www.journal.viam.ru (accessed: May 05, 2024). DOI: 10.18577/2713-0193-2023-0-4-45-54.
  23. Bard A.J., Faulkner L.R. Electrochemical methods. Fundamentals and applications. 2ed. Wiley, 2001, 833 p.
  24. Wang N., Li W., Huang Y. et al. Wrought Mg–Al–Pb–Re alloy strips as the anodes for Mg-air batteries. Journal of power sources, 2019, vol. 436, pp. 957–968. DOI: 10.1016/j.jpowsour.2019.226855.
  25. Chen X., Ning S., Le Q. et al. Effects of external field treatment on the electrochemical behaviors and discharge performance of AZ80 anodes for Mg-air batteries. Journal of Materials Science & Technology, 2020, vol. 38, pp. 47–55.
  26. Feliu S.Jr. Electrochemical impedance spectroscopy for the measurement of the corrosion rate of magnesium alloys: brief review and challenges. Metals, 2020, vol. 10, no. 6, p. 775.