Starkov A.I., Isaev A.Yu., Kutsevich K.E. Comprehensive assessment of the impact of operational and climatic tests on the change of strength properties of polymer composite materials based on adhesive prepregs. Part 1. Carbon fiber-reinforced plastic VKU-59 // Proceedings of VIAM. 2024. No. 3 (133). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-3-91-100.
Comprehensive assessment of the impact of operational and climatic tests on the change of strength properties of polymer composite materials based on adhesive prepregs
Part 1. Carbon fiber-reinforced plastic VKU-59
Abstract
A comprehensive assessment of the retention of strength properties of carbon fiber plastic of the VKU-59 brand under tension, compression, bending, interlayer shear at test temperatures of –60, +20, +80 and +105 °C was carried out in the initial state and after climatic influences in a tropical climate chamber for 1 and 3 months, heat and humidity aging for 1 and 3 months, thermal aging for 500 and 1000 hours. The influence of the mycological environment and process fluids on the tensile strength of carbon fiber reinforced plastic in bending and compression was studied. To confirm the viability, samples of VKU-59 carbon fiber plastic were tested in tension and compression after 3 months of storage.
Keywords
carbon fiber-reinforced plastic, adhesive prepreg, adhesive joints, tensile strength, compression strength, flexural strength, interlayer shear strength, influence of external factors
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., proc. and add. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs. 276 p.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Satdinov R.A., Veshkin E.A, Postnov V.I. Assessment of the impact of climatic factors on the performance properties of fiberglass VPS-42P/T-64. Trudy VIAM, 2020, no. 10 (92), paper no. 03. Available at: http://www.viam-works.ru (accessed: October 20, 2023). DOI: 10.18577/2307-6046-2020-0-10-21-29.
- Gulyaev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A. Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics. Trudy VIAM, 2021, no. 2 (96), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 20, 2023). DOI: 10.18577/2307-6046-2021-0-2-39-51.
- Borshchev A.V., Gusev Yu.A. Polymer composite materials in automotive industry. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 34–38. DOI: 10.18577/2071-9140-2014-0-s2-34-38.
- Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kutsevich K.E. Adhesive prepregs and layered materials on their basis. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 19–21.
- Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 20, 2023). DOI: 10.18577/2307-6046-2022-0-5-87-95.
- Mishkin S.I., Zhakova L.S., Klimenko O.N., Vasilchuk E.A. Research of influence of the contents resin in CFRP on their mechanical properties. Trudy VIAM, 2023, no. 2 (120), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 20, 2023). DOI: 10.18577/2307-6046-2023-0-2-77-86.
- Malakhovsky S.S., Panafidnikova A.N., Kostromina N.V., Osipchik V.S. Carbon plastics in the modern world: their properties and applications. Uspekhi v khimii i khimicheskoy tekhnologii, vol. XXXIII, 2019, no. 6, pp. 62–64.
- Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
- Veshkin E.A., Startsev V.O., Postnov V.I., Barannikov A.A. The climate impacts as the assessment of maintainability of products from carbon fiber. Trudy VIAM, 2019, no. 8 (80), paper no. 11. Available at: http://www.viam-works.ru (accessed: October 20, 2023). DOI: 10.18577/2307-6046-2019-0-8-98-108.
- Starkov A.I., Kutsevich K.E., Petrova A.P., Antyufeeva N.V. Development of temperature and time curing regime for prepregs based on adhesive binder with reduced flammability. Trudy VIAM, 2023, no. 3 (121), paper no. 03. Available at: http://www.viam-works.ru (accessed: October 20, 2023). DOI: 10.18577/2307-6046-2023-0-3-29-38.
- Dementyeva L.A., Lukina N.F., Serezhenkov A.A., Kutsevich K.E. Basic properties and purpose of PCM based on adhesive prepregs. Reports XIX Int. sci.-tech. conf. «Designs and technology for producing products from non-metallic materials». Obninsk: ONPP «Technology», 2010, pp. 11–12.
- Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Perov N.S. Design of polymeric materials on the molecular principles. II. The molecular mobility in the cross-linked complex systems. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 30–36. DOI: 10.18577/2071-9140-2017-0-4-30-36.
- Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
- Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
- Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 18, 2023). DOI: 10.18577/2307-6046-2021-0-3-58-67.
- Lukina N.F., Petrova A.P., Muhametov R.R., Kogtyonkov A.S. New developments in the field of adhesive aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 452–459. DOI: 10.18577/2071-9140-2017-0-s-452-459.
- Malysheva G.V., Grashchenkov D.V., Guzeva T.A. Evaluation of technological use efficiency of adhesives and glue prepregs in the manufacture of three-layer panels. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 26–30. DOI: 10.18577/2071-9140-2018-0-4-26-30.