Nyafkin A.N., Zhabin A.N., Avtaev V.V. Crack propagation in composite materials of the Al‒SiC system under cyclic loads // Proceedings of VIAM. 2024. No. 3 (133). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-3-63-75.

Crack propagation in composite materials of the Al‒SiC system under cyclic loads

Nyafkin A.N., Zhabin A.N., Avtaev V.V.
Abstract

The review presents the features of fatigue crack propagation in composite materials (CM) based on aluminum alloys reinforced with silicon carbide (SiC) particles with different volume content under cyclic loading conditions. The influence of the volume content and size of SiC particles on the growth rate of a fatigue crack in  CM under the action of cyclic loads is considered. The results of studying the influence of the CM structure on the growth rate and development of cracks during cyclic tests are presented.

Keywords
composite material, SiC particles, particle size, particle volume fraction, fatigue crack growth
Reference list
  1. Kablov E.N. Marketing of materials science, aircraft engineering and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  2. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N. The key problem is materials. Trends and guidelines for innovative development of Russia. Moscow: VIAM, 2015, pp. 458–464.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  6. Kosolapov D.V., Shavnev A.A., Kurbatkina E.I., Nyafkin A.N., Gololobov A.V. Study on structure and properties of dispersion hardened mmc based on aluminium alloy of Al–Mg–Si system. Trudy VIAM, 2020, no. 1 (85), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 12, 2022). DOI: 10.18577/2307-6046-2020-0-1-58-67.
  7. Shavnev A.A., Kurbatkina E.I., Nyafkin A.N., Kosolapov D.V. Technologies for manufacturing dispersion-strengthened metal composite material based on aluminum alloy (review). Materialovedenie, 2022, no. 4, pp. 42–48. DOI: 10.31044/1684-579X-2022-0-4-42-48.
  8. Певчев Д.И., Горбовец М.А., Рыжков П.В., Курбаткина Е.И. Исследование характеристик прочности дисперсноупрочненного металлического композиционного материала марки ВКМ22. Trudy VIAM, 2021, no. 2 (96), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 12, 2022). DOI: 10.18577/2307-6046-2021-0-2-30-38.
  9. Milan M.T., Bowen P. Fatigue сrack growth resistance of SiCp reinforced Al alloys: effects of particle size, particle volume fraction, and matrix strength. Journal of Materials Engineering and Performance, 2004, vol. 13, pp. 612–618. DOI: 10.1361/10599490420638.
  10. Mason J.J., Ritchie R.O. Fatigue crack growth resistance in SiC particulate and whisker reinforced P/M 2124 aluminum matrix composites. Materials Science and Engineering A, 1997, vol. 231, pp. 170–182. DOI: 10.1016/S0921-5093(97)00086-5.
  11. Lia W., Liang H., Chen J. et al. Effect of SiC particles on fatigue crack growth behavior of SiC particulate-reinforced Al‒Si alloy composites produced by spray forming. Procedia Materials Science, 2014, vol. 3, pp. 1694–1699. DOI: 10.1016/j.mspro.2014.06.273.
  12. Xu F.M., Zhu S.J., Zhao J.L. et al. Fatigue crack growth in SiC particulates reinforced Al matrix graded composite. Materials Science and Engineering A, 2003, vol. 360, pp. 191–196. DOI: 10.1016/S0921-5093(03)00397-6.
  13. Uzun H., Lindley T.C., McShane H.B., Rawlings R.D. Fatigue crack growth behavior of 2124/SiC/10p functionally graded materials. Metallurgical and Materials Transactions A, 2001, vol. 32A, pp. 1831–1839. DOI: 10.1007/s11661-001-0159-x.
  14. Chena Z.Z., Tokaji K. Effects of particle size on fatigue crack initiation and small crack growth in SiC particulate-reinforced aluminium alloy composites. Materials Letters, 2004, vol. 58, pp. 2314–2321. DOI: 10.1016/j.matlet.2004.02.034.
  15. Li K., Jin X.D., Yan B.D., Li P.X. Effect of SiC particles on fatigue crack propagation in SiC/Al composites. Composites, 1992, vol. 23, no. 1, pp. 54–58. DOI: 10.1016/0010-4361(92)90286-4.
  16. Bruzzi M.S., McHugh P.E. Micromechanical investigation of the fatigue crack growth behaviour of Al–SiC MMCs. International Journal of Fatigue, 2004, vol. 26, pp. 795–804. DOI: 10.1016/j.ijfatigue.2004.01.007.
  17. Nyafkin A.N., Loshinin U.V., Kurbatkina E.I., Kosolapov D.V. Investigation of influence of silicon carbide fractional composition on thermal conductivity of composite material based on aluminium alloy. Trudy VIAM, 2019, no. 11 (83), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 20, 2022). DOI: 10.18577/2307-6046-2019-0-11-53-59.
  18. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  19. Andrew O.N., Joel O.O., Murray A.O., Eruke U.J. Effect of Compaction on Thermal Conductivity of Aluminium Powder. International Journal of Emerging Engineering Research and Technology, 2018, vol. 6, is. 2, pp. 1–5.
  20. Verma R.K., Mahesh N.S., Anwar M.I. Numerical Analysis of Powder Compaction to Obtain High Relative Density in ‘601AB' Aluminum Powder. SasTech Journal, 2012, vol. 11, is. 1, pp. 79–84.
  21. Sevostianov I., Kachanov M. Nanoparticle reinforced materials: Effect of interphase layers on the overall properties. International Journal of Solids and Structures, 2007, vol. 44, is. 3–4, pp. 1304–1315. DOI: 10.1016/j.ijsolstr.2006.06.020.