Abstract

Technological plasticity, deformation mechanisms and dependence between mechanical properties and the conditions of deformation of titanium alloy VT30 were studied in present work. Samples in cast and forged states were examined. The samples were deformed on a pile driver and press at different temperatures, also forging and stamping were carried out. The results showed that the VT30 alloy has better properties in the forged state. In addition, optimal conditions for pressure treatment of titanium alloy VT30 were obtained.

Keywords
titanium, heat treatment, deformation, plasticity, aviation industry, cooling forming, forging
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  3. Ospennikova O.G. Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  4. Nochovnaya N.A., Shiryaev A.A., Sharapkin D.S. Complex of mechanical and operational properties of rolled blanks from metastable-β-titanium alloy VT47. Aviation materials and technologies, 2022, no. 3 (68), paper no. 05. Available at: http://www.journal.viam.ru (accessed: May 16, 2023). DOI: 10.18577/2713-0193-2022-0-3-50-59.
  5. Moiseev V.N. Beta-titanium alloys and prospects for their development. Metallovedeniye i termicheskaya obrabotka metallov, 1998, no. 12, pp. 11–14.
  6. Brun M.Ya., Belov S.P., Glazunov S.G. et al. Metallurgy of titanium alloys. Moscow: Metallurgiya, 1994, 351 p.
  7. Kablov E.N., Putyrsky S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Study of resistance to fatigue fracture of forgings made of high-strength titanium alloy VT22M, manufactured with final deformation in the (α + β)- and β-regions. Titan, 2021, vol. 70, no. 1, pp. 26–33.
  8. Zaripova R.G., Shundalov V.A., Sharafutdinov A.V. et al. The influence of intense plastic deformation and processing modes on the structure and mechanical properties of titanium alloy VT6. Vestnik Ufimskogo gosudarstvennogo aviatsionnogo tekhnicheskogo universiteta, 2012, no. 7 (52), pp. 17–24.
  9. Skugorev A.V., Kapitanenko D.V., Shishkov S.Yu., Melnikova D.A. Formation of the structure and mechanical properties of high-alloy titanium alloys during isothermal stamping in air. Titan, 2021, vol. 72, no. 3, pp. 34–40.
  10. Burgonova O.Yu., Pantyukhova K.N., Belozerova E.P. Determination of a rational mode of heat treatment of the VT3-1 alloy to increase ductility before pressure treatment. Omskiy nauchnyy vestnik, 2017, no. 3 (153), pp. 44–48.
  11. Razyvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Modern technologies of plastic working of metals. Trudy VIAM, 2015, no. 2, paper no. 03. Available at: http://www.viam-works.ru (accessed: May 12, 2023). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  12. Egorova Yu.B., Davydenko L.V., Belova S.B., Chibisova E.V. Prediction of mechanical properties of forgings from titanium alloys VT6 and VT3-1 depending on the chemical composition and structure. Izvestiya vuzov. Tsvetnaya metallurgiya, 2018, no. 1, pp. 12–21.
  13. Putyrskiy S.V., Yakovlev A.L., Nochovnaya N.A., Krokhina V.A. Research of different heat treatment modes influence on properties of semi-finished products and welded joints from titanium alloy ВТ22М. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 3–10. DOI: 10.18577/2071-9140-2019-0-1-3-10.
  14. Dzunovich D.A., Lukina E.A., Yakovlev A.L. Influence of heat treatment parameters on producibility and mechanical properties of sheets made from high-strength titanium alloy VT23. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-3-3-10.
  15. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 22, 2023). DOI: 10.18577/2713-0193-2022-0-1-30-40.
  16. Aleksandrov V.K., Belov A.F., Bondarev B.I. et al. Metallurgy and processing of titanium and heat-resistant alloys. Moscow: VILS, 1991, 389 p.
  17. Krokhina V.A., Arislanov А.A., Putyrskiy S.V., Anisimova A.Yu. Investigation of the regularities of the formation of the structure of rods made of titanium alloy VT6 depending on various technological schemes of manufacture. Aviation materials and technologies, 2023, no. 4 (73), paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 22, 2023). DOI: 10.18577/2713-0193-2023-0-4-36-44.