Marchenko S.A., Zheleznyak V.G., Kuznetsova V.A., Timoshina E.A. Dependence of ice adhesion on the hydrophobic properties of polymer coatings, applied of pneumatic spraying method // Proceedings of VIAM. 2024. No. 2 (132). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-2-76-83.

Dependence of ice adhesion on the hydrophobic properties of polymer coatings, applied of pneumatic spraying method

Marchenko S.A., Zheleznyak V.G., Kuznetsova V.A., Timoshina E.A.
Abstract

The work focused on determining the dependence of the anti-icing properties of coatings on hydrophobic properties. The coatings were applied by pneumatic spraying and did not have a clearly structured roughness structure. For the study, polymer coatings of various chemical natures were selected based on: organosilicon copolymer, copolymer of vinylidene fluoride and chlorotrifluoroethylene, fluoropolyurethane, epoxy varnish, acrylic copolymer, poly-dieneurethane with epoxy end groups and fluorosiloxane rubber. The dependences of ice adhesion on the contact angle of wetting, roughness and freezing time of water were determined.

Keywords
hydrophobic polymer coatings, ice adhesion, contact angle, water freezing time, anti-icing coatings, pneumatic spraying
Reference list
  1. Frohboese P., Anders A. Effects of icing on wind turbine fatigue loads. Journal of Physics: Conference Series, 2007, vol. 75, p. 012061.
  2. Parent O., Ilinca A. Anti-icing and de-icing techniques for wind turbines: critical review. Cold Regions Science and Technology, 2011, vol. 65, pp. 88–96.
  3. Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  4. Kablov E.N. Structural and functional materials are the basis of economic, scientific and technical development of Russia. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
  5. Gent R., Dart N., Cansdale J. Aircraft icing. Philosophical Transactions of the Royal Society of London A: Mathematical, Physical and Engineering Sciences, 2000, vol. 358 (1776), pp. 2873–2911.
  6. Buznik V.M., Kablov E.N., Koshurina A.A. Materials for complex technical devices for Arctic applications. Scientific and technical problems of Arctic development. Moscow: Nauka, 2015, pp. 275–285.
  7. Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
  8. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  9. Wang H., He G., Tian Q. Effects of nano-uorocarbon coating on icing. Applied Surface Science, 2012, vol. 258:18, pp. 7219–7224.
  10. Shen Y., Tao J., Tao H. et al. Anti-icing potential of superhydrophobic Ti6Al4V surfaces: ice nucleation and growth. Langmuir, 2015, vol. 31, pp. 10799–10806.
  11. Liu J., Janjua Z.A., Roe M. et al. Super-hydrophobic/icephobic coatings based on silica nanoparticles modified with self-assembled monolayers. Nanomaterials, 2016, vol. 6, p. 232.
  12. Tourkine P., Le Merrer M., Quere D. Delayed freezing of water-repellent material. Langmuir, 2009, vol. 25, pp. 7214–7216.
  13. Varanasi K., Deng T., Smith J.D. et al. Frost formation and ice adhesion on superhydrophobic surfaces. Applied Physics Letters, 2010, vol. 97, art. 234102.
  14. Kablov E.N., Solovyanchik L.V., Kondrashov S.V. et al. Electrically conductive hydrophobic polymer composite materials based on oxidized carbon nanotubes modified with tetrafluoroethylene telomers. Rossiyskie nanotekhnologii, 2016, vol. 11, no. 11–12, pp. 91–97.
  15. Antonini C., Innocenti C., Horn T. et al. Understanding the effect of superhydrophobic coatings on energy reduction in anti-icing systems. Cold Regions Science and Technology, 2011, vol. 67, pp. 58–67.
  16. Li J., Zhou Y., Wang W. et al. Superhydrophobic copper surface textured by laser for delayed icing phenomenon. Langmuir, 2020, vol. 36 (5), pp. 1075–1082.
  17. Golovin K., Kobaku S., Lee D. et al. Designing durable icephobic surfaces. Science advances, 2016, vol. 2, pp. 1–12.
  18. Diao Y., Harada T., Myerson A. et al. The role of nanopore shape in surface-induced crystallization. Nature Materials, 2011, vol. 10, pp. 867–871.
  19. Guo P., Zheng Y., Wen M. et al. Icephobic/Anti-Icing properties of Micro/Nanostructured surfaces. Advanced Materials, 2012, vol. 24, pp. 2642–2648.
  20. Tian X., Verho T., Ras R. Surface wear. Moving superhydrophobic surfaces toward real-world applications. Science, 2016, vol. 352, p. 142.
  21. Yang S., Xia Q., Zhu L. et al. Research on the icephobic properties of fluoropolymer-based materials. Applied Surface Science, 2011, vol. 257, pp. 4956–4962.
  22. Peng C., Xing S., Yuan Z., Jiayu X. Preparation and anti-icing of superhydrophobic PVDF coating on a wind turbine blade. Applied Surface Science, 2012, vol. 259, pp. 764–768.
  23. Tarasova P.N., Sleptsova S.A., Laukkanen S., Dyakonov A.A. Sealing materials based on polytetrafluo-roethylene for aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 05. Available at: http://www.journal.viam.ru (ассеssed: October 30, 2023). DOI: 10.18577/2713-0193-2022-0-1-51-64.
  24. Bragg M., Broeren A., Blumenthal L. Iced-airfoil aerodynamics. Progress in Aerospace sciences, 2005, vol. 41 (5), pp. 323–362.
  25. Kondrashov S.V., Pykhtin A.A., Solovyanchik L.V., Bolshakov V.A., Pavlyuk B.Ph., Badamshina E.R., Dzhalmukhanova A.S., Karpov S.V. Research of dependence of adhesion of ice to polyurethane coatings from their physicomechanical properties. Trudy VIAM, 2019, no. 3 (75), paper no. 10. Available at: http://www.viam-works.ru (accessed: December 17, 2023). DOI: 10.18577/2307-6046-2019-0-3-87-95.
  26. Marchenko S.A., Zheleznyak V.G., Kuznetsova V.A. Ice adhesion. Methods of determination (review). Trudy VIAM, 2022, no. 9 (115), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 17, 2023). DOI: 10.18577/2307-6046-2022-0-9-143-160.