Sudyin Yu.I., Salakhova R.K., Galiullin An.R., Savitsky R.S. Study of surface-energy characteristics of elements of three-layer honeycomb panels // Proceedings of VIAM. 2024. No. 12. Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-12-66-74.

Study of surface-energy characteristics of elements of three-layer honeycomb panels

Sudyin Yu.I., Salakhova R.K., Galiullin An.R., Savitsky R.S.
Abstract

The results of research of surface tension of melt adhesive binder VSK-14-6 using a processor tensiometer are presented. As a result of measuring the wetting edge angles in test liquids, the calculated values of surface free energies (SFE) of the studied solids (polymer-sotoplastic and carbon fiber UMT42S-3K-EP) were obtained, including after treatment with atmospheric pressure plasma. The obtained SFE values were used to evaluate the wetting ability of the solids and their adhesion to the binder.

Keywords
three-layer honeycomb panel, honeycomb filler, carbon fiber, edge wetting angle, Washburne method, atmospheric pressure plasma, adhesion
Reference list
  1. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  2. Kablov E.N. New Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Veshkin E.A., Satdinov R.A., Barannikov A.A. Modern materials for the aircraft cabin. Trudy VIAM, 2021, no. 9 (103), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 25, 2024). DOI: 10.18577/2307-6046-2021-0-9-33-42.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Barannikov A.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. On the issue of production of floor panels from polymer composite materials for aircraft (review article). Izvestiya Samarskogo nauchnogo tsentra RAN, 2017, no. 4 (2), pp. 198–213.
  6. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 25, 2024). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  7. Timoshkov P.N., Kolobkov A.S., Kurnosov A.O., Goncharov V.A. Prepregs based on melt binders and new-generation polymer composite materials based on them for aviation equipment. Proceedings of the V All-Rus. scientific and technical conf. «Polymer composite materials and production technologies of the new generation». Moscow: National Research Center «Kurchatov Institute» – VIAM, 2021, pp. 7–20.
  8. Kablov E.N., Antipov V.V. The role of new-generation materials in ensuring the technological sovereignty of the Russian Federation. Izvestiya Samarskogo nauchnogo tsentra RAN, 2023, vol. 93, no. 10, pp. 907–916.
  9. Kablov E.N. The sixth technological mode. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  10. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 25, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  11. Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
  12. Salakhova R.K., Panarin A.V. Study of surface energy characteristics of glass and carbon fiber by the Washburn method. Voprosy materialovedeniya, 2023, no. 3 (115), pр. 159–169.
  13. Salakhova R.K., Postnov V.I., Kachura S.M., Veshkin E.A. Features of glass fiber sample preparation for measurements on a K-100 tensiometer. Proc. of the V All-Rus. scientific and technical conf. «Polymer composite materials and production technologies of the new generation». Moscow: NRC «Kurchatov Institute» – VIAM, 2021, рр. 126–144.
  14. Zinina I.N., Pimanov M.V. Influence of the surface energy of metal samples on the strength of adhesive joints. Izvestiya MGTU «MAMI», 2011, no. 2 (12), pp. 127–130.
  15. Barannikov A.A., Postnov V.I., Veshkin E.A., Satdinov R.A. Application of atmospheric pressure plasma as a method for preparing the surface of polymer composite materials for bonding. Proc. of the V All-Rus. scientific and technical conf. «Polymer composite materials and production technologies of the new generation». Moscow: NRC «Kurchatov Institute» – VIAM, 2021, pp. 177–195.
  16. Bogdanova Yu. G. Adhesion and its role in ensuring the strength of polymer composites. Moscow: Moscow State University, 2010, 68 р.
  17. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
  18. Shershak P.V., Sutubalov A.I., Yakovlev N.O., Sherstyuk F.A. Standards test methods for polymer matrix composite materials. Part 2. Compression properties. Aviation materials and technologies, 2024, no. 2 (75), paper no. 12. Available at: http://www.journal.viam.ru (accessed: September 25, 2024). DOI: 10.18577/2713-0193-2024-0-2-149-166.