Sutubalov A.I., Podzhivotov N.Y., Shershak P.V., Yakovlev N.O. Assessment of the adhesive strength of the fiber–polymer matrix system using the nonparametric bootstrap method // Proceedings of VIAM. 2024. No. 11 (141). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-11-100-112.
Assessment of the adhesive strength of the fiber–polymer matrix system using the nonparametric bootstrap method
Abstract
The article discusses the practical aspects of using the bootstrap method in micromechanics problems to assess the adhesive strength of the fiber–polymer matrix system. The article provides a detailed algorithm for constructing confidence intervals when calculating the bootstrap method. А comparative analysis of the interval estimation of experimental adhesive strength data using the nonparametric (bootstrap) method and a number of parametric methods was carried out. Based on the generated bootstrap samples, a histogram of the frequency distributions of the average values of the adhesive strength of the fiber–polymer matrix system is constructed.
Keywords
micromechanical characteristics, micromechanics, adhesion, confidence intervals, interval estimation, parametric method, bootstrap method
Reference list
- Kablov E.N. Quality control of materials – a guarantee of safety of operation of aviation equipment. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
- Erasov V.S. Modern methods of assessing the physical and mechanical properties of materials. Reports All-Rus. Conf. on testing and research of the properties of materials «TestMat–2012». Moscow: VIAM, 2012, p. 13.
- Morgan P. Carbon Fibers and Their Composites. Boca Raton: Taylor & Francis, 2005, 1153 p.
- MIL-HDBK-17: Composite Materials Handbook: in 5 vols. Virginia: Department of Defense, 2002. Vol. 1: Polymer Matrix Composites Guidelines for Characterization of Structural Materials, 586 р.
- Oreshko E.I., Erasov V.S., Utkin D.A., Avtayeva Ya.V. The equipment for definition of physicomechanical characteristics of materials by press-in method (review). Aviation materials and technologies, 2021, no. 4 (65), paper no. 12. Available at: http://www.journal.viam.ru (accessed: April 24, 2024). DOI: 10.18577/2713-0193-2021-0-4-107-124.
- Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: May 24, 2024). DOI: 10.18577/2713-0193-2023-0-1-61-81.
- Oreshko E.I., Erasov V.S., Yakovlev N.O., Utkin D.A. Methods for determining the mechanical characteristics of materials using indentation (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 10. Available at: http://www.journal.viam.ru (accessed: May 21, 2024). DOI: 10.18577/2713-0193-2021-0-1-104-118.
- Erasov V.S., Sibayev I.G., Sutubalov A.I., Popkova E.A., Gorbovets M.A. Methods of mechanical testing to determine the strength of carbon fibers. Aviation materials and technologies, 2024, no. 2 (75), paper no. 11. Available at: http://www.journal.viam.ru (accessed: April 26, 2024). DOI: 10.18577/2713-0193-2024-0-2-137-148.
- Gulyayev A.I. Fiber-matrix adhesion strength measurement using nanoindentation (review). Trudy VIAM, 2019, no. 3 (75), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 30, 2024). DOI: 10.18577/2307-6046-2019-0-3-68-78.
- Bogdanova Yu.G. Adhesion and its role in ensuring the strength of polymer composites: textbook. Moscow: Moscow State University, 2010, 68 p.
- Gulyaev A.I., Yerasov V.S., Oreshko E.I., Utkin D.A. Analysis of carbon fiber destruction during expulsion of a multifilament cylinder. Klei. Germetiki. Tekhnologii, 2021, no. 1, pp. 28–35.
- Chudnov I.V., Buyanov I.A. Assessment of structural defects of carbon fibers and polymer composite materials based on them. Nauka i obrazovaniye (MGTU im. N.E. Baumana), 2011, no. 11, paper no. 12. Available at: http://www.istina.msu.ru (accessed: May 24, 2024). DOI: 77-30569/281952.
- Gadolina I.V., Lisachenko N.G. Development of a method for constructing confidence intervals for percentiles of a random sample of composite strength using bootstrap modeling. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 11, pp. 73–77.
- Agamirov L.V. Methods of statistical analysis of mechanical tests. Moscow: Intermet Engineering, 2004, 128 p.
- Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 30, 2024). DOI: 10.18577/2713-0193-2024-0-1-121-135.
- Nesterov A.V., Nesterov S.V., Kozak D.A. On checking the deviation of probability distribution from normal distribution in the Matlab computer mathematics system. Nauchnye trudy KubGTU, 2015, no. 6, pp. 1–31.
- Krupin V.G., Pavlov A.L., Popov L.G. Higher mathematics. Probability theory, mathematical statistics, random processes. Collection of problems with solutions: textbook. Moscow: Publ. House MEI, 2013, 408 p.
- Hoang Ph. Handbook of Engineering Statistics. Heidelberg: Springer, 2023, 1135 p.
- Efron B., Tibshirani R. An Introduction to the Bootstrap. London: Chapman Hall, 1993, 436 p.
- Glukhov V.V., Anufriev D.V. Bootstrap procedures for determining accuracy characteristics. Nauchnyy vestnik MGTU GA, 2005, no. 89 (7), pp. 30–35.
- Davison A.C., Hinkley D.V. Bootstrap methods and their application. Cambridge: Cambridge University Press, 2006, 592 p.
- Shershak P.V., Yakovlev N.O., Sutubalov A.I. Standards for testing polymer composite materials. Part 1. Tensile properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 12. Available at: http://www.journal.viam.ru (accessed: May 24, 2024). DOI: 10.18577/2713-0193-2023-0-3-152-166.
- Sidorina A.I. Modification of the surface of carbon reinforcing fillers for polymer composite materials by electrochemical treatment (review). Trudy VIAM, 2022, no. 4 (110), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 30, 2024). DOI: 10.18577/2307-6046-2022-0-4-61-74.
- Erasov V.S., Oreshko E.I. Deformation and destruction as processes of change of volume, the areas of a surface and the linear sizes in loaded bodies. Trudy VIAM, 2016, no. 8, paper no. 11. Available at: http://www.viam-works.ru (accessed: May 28, 2024). DOI: 10.18577/2307-6046-2016-0-8-11-11.
- Popov Yu.O., Koloкoltseva T.V., Gromova A.A., Gusev Yu.A. Influence of operational factors on the main physical and mechanical properties of a fiberglass product VPS-31. Trudy VIAM, 2021, no. 11 (105), paper no. 08. Available at: http://www.viam-works.ru (accessed: May, 24, 2024). DOI: 10.18577/2307-6046-2021-0-11-82-90.
- Lutsenko A.N., Odintsev I.N., Grinevich A.V. et al. Study of material deformation by optical-correlation methods. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 70–86. DOI: 10.18577/2071-9140-2014-0-s4-70-86.
- Ilyichev A.V. Comparison of GOST and ASTM standards for mechanical testing of polymer composite materials for tension. Vse materialy. Entsiklopedicheskiy spravochnik s Prilozheniyem «Kommentarii k standartam, TU, sertifikatam», 2015, no. 8, pp. 2–9.