Antipov V.V., Venediktova M.A., Pushnitsa А.S., Kotelnikova D.D., Popov А.V. Investigation of the possibility of increasing the temperature range of fire retardant materials // Proceedings of VIAM. 2024. No. 10 (140). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-10-74-83.
Investigation of the possibility of increasing the temperature range of fire retardant materials
Abstract
The article describes the results of research (physical, fire and thermophysical) properties of the flame retardant material based on fluorosiloxane rubber with different systems of functional additives. The work is aimed at extending the temperature range (up to 200 °С) of fire retardant materials operation, in environments that allow contact with fuel. Research confirms the efficiency of phosphate-nitrogen intumescent system, due to the formation of a durable protective carbon backbone under the influence of high temperatures, preventing the spread of fire.
Keywords
flame-retardants, fluorosiloxane rubbers, thermal conductivity, density, flammability
Reference list
- Goncharova P.Yu., Babkin O.E., Sirotinina M.V. Formulation principles for creating effective fire-retardant UV-curable intumescent compositions. Innovative materials and technologies in design. St. Petersburg, 2016, pp. 42–48.
- Gabdulin R.Sh. Effective methods of fire protection of building structures. Bezopasnost, 2011, no. 1, pp. 48–49.
- Yakovlev A.D., Yakovlev S.A. Functional-purpose paint and varnish coatings. St. Petersburg: Khimizdat, 2016, 272 p.
- Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Fire safety assessment of polymeric materials for aviation purposes: analysis of the state, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
- Mouritz A.P., Gibson A.G. Fire properties of polymer composite materials. Dordrecht: Springer Science & Business Media, 2007, pp. 59–63.
- Lyon R.E. Fire-safe aircraft cabin materials. Fire & Polymers, ACS Symposium Series, 1995, no. 559, pp. 618–638.
- Avduevsky V.S., Galitseysky B.M., Glebov G.A. Fundamentals of Heat Transfer in Aviation and Rocket-Space Engineering. Ed. V.K. Koshkin. Moscow: Mashinostroenie, 1975, 623 p.
- Khalturinsky N.A., Popova T.V., Berlin A.A. Combustion of Polymers and the Mechanism of Action of Flame Retardants. Uspekhi Khimii, 1984, vol. 53, no. 2, pp. 326–346.
- Aseeva R.M., Zaikov G.E. Combustion of Polymer Materials. Moscow: Nauka, 1981, 280 p.
- Krasnov L.L., Kirina Z.V. Materials Ensuring the Reliability of Structural Elements in Fire Conditions. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 10, pp. 48–52.
- Venediktova M.A., Krasnov L.L., Kirina Z.V. Some aspects of the application of fire-protective coatings (review). Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 1–2, paper no. 06. Available at: http://www.materialsnews.ru (accessed: September 07, 2024).
- Venediktova M.A., Evdokimov A.A., Krasnov L.L., Petrova A.P. Research of possibility of application of fireproof paste for increase of fire safety of designs from polymeric composite materials. Trudy VIAM, 2021, no. 9 (103), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 07, 2024). DOI: 10.18577/2307-6046-2021-0-9-67-75.
- Zybina O.A., Varlamov A.V., Chernova N.S., Mnatsakanov S.S. On the role and transformations of components of fire-retardant intumescent paint and varnish compositions in the process of thermolysis. Zhurnal prikladnoy khimii, 2009, vol. 82, no. 4, pp. 1445–1449.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg, 2016, рp. 25–26.
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, рp. 907–916.
- Shetz M. Silicone rubber. Moscow: Khimiya, 1975, 400 p.
- Dolgov O.N., Voronkov M.G., Grinblat M.P. Organosilicon liquid rubbers and materials based on them. Leningrad: Khimiya, 1975, 112 p.
- The Big Handbook of the Rubber Manufacturer: in 2 parts. Eds. S.V. Reznicenko, Yu.L. Morozov. Moscow: Tekhinform, 2012, part 1, 2, 1385 p.
- Rubber and Rubber. Science and Technology; trans. from Engl. Eds. A.A. Berlin, Yu.L. Morozov. Dolgoprudny: Intellect, 2011, 768 p.
- Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Technology of Elastomeric Materials. Moscow: Istok, 2009, 502 p.
- Krasheninnikova M.V. Fire-retardant intumescent materials based on organosoluble film formers. Lakokrasochnye materialy i ikh primenenie, 2006, no. 12, pp. 14–16.
- Pavlovich A.V., Vladenkov V.V., Izyumsky V.N., Kilchitskaya S.L. Fire-retardant intumescent coatings. Lakokrasochnaya promyshlennost, 2012, no. 5, pp. 22–27.
- Zaikov G.E. Combustion, destruction and stabilization of polymers. St. Petersburg: Scientific foundations and technologies, 2008, 421 p.
- Kodolov V.I. Flammability and fire resistance of polymeric materials. Moscow: Khimiya, 1976, 98 p.
- Kodolov V.I. Flame retardants for polymeric materials. Moscow: Khimiya, 1980, 156 p.
- Potapova A.I., Bobrova I.I., Evdokimov A.A., Venediktova M.А. Prescription techniques for creating elastomeric compositions with reduced flammability. Trudy VIAM, 2024, no. 1 (131), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 07, 2024). DOI: 10.18577/2307-6046-2024-0-1-60-77.
- Kondrashov S.V., Solovyanchik L.V., Larionov S.A., Volny O.S. Investigation of the effect of flame retardants on the flammability and fluidity of the melt of aliphatic polyamides. Trudy VIAM, 2022, no. 2 (108), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 07, 2024). DOI: 10.18577/2307-6046-2022-0-2-52-63.
- Garashchenko A.N., Kulkov A.A., Strakhov V.L. The effect of the service life on the flame-retardant efficiency of the bulging coatings and the fire resistance of structures. Aviation materials and technologies, 2022, no. 2 (67), paper no. 09. Available at: http://www.journal.viam.ru (accessed: September 07, 2024). DOI: 10.18577/2713-0193-2022-0-2-97-110.
- Barbotko S.L., Volnyy O.S., Shurkova E.N. Creation of the phenomenological model describing change of the characteristic of combustibility (duration of residual burning) depending on thickness of polymeric material. Trudy VIAM, 2018, no. 10 (70), paper no. 12. Available at: http://www.viam-works.ru (accessed: September 07, 2024). DOI: 10.18577/2307-6046-2018-0-10-107-116.