Min P.G., Vadeev V.E., Kolesnikov S.I., Chemov D.A. The effect of impurities on mechanical and operational properties of the cast nickel-base superalloy VZhM200 // Proceedings of VIAM. 2024. No. 10 (140). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-10-13-23.

The effect of impurities on mechanical and operational properties of the cast nickel-base superalloy VZhM200

Min P.G., Vadeev V.E., Kolesnikov S.I., Chemov D.A.
Abstract

The results of the study of the effect of sulfur, phosphorus, silicon and nitrogen impurities on the main properties of the high-temperature nickel alloy VZhM200 for blades casting with a directional structure of the PD-8 gas turbine engine: long-term, fatigue strength and short-term mechanical properties are presented. It was found that with an increased content of these impurities in the alloy, the time to destruction decreases at T = 1000 °C at bases of 100, 500 h and plasticity at T = 20 °C. It was also found that the number of cycles to failure was reduced when tested for high-cycle fatigue at T = 900 °C in the alloy with the addition of silicon and nitrogen.

Keywords
cast heat-resistant nickel-base superalloy, directional crystallization, impurities, mechanical properties, long-term strength, fatigue
Reference list
  1. Tikhonov A.I., Kraev V.M., Siluyanova M.V. Prospects for the Development of Russian Aviation Engine Building Based on a Unified Gas Generator. STIN, 2023, no. 6, pp. 71–74.
  2. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), paper no. 01. Available at: http://www.journal.viam.ru (accessed: September 02, 2024). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  3. Konstantinov I.V. Ensuring technological sovereignty of the aviation industry using the SUKHOI SUPERJET NEW aircraft as an example. Scientific achievements and innovative approaches: theory, methodology, practice: collection of scientific papers based on the materials of the VIII International scientific and practical conf. Anapa, 2022, рp. 99–103.
  4. More than 40 PD-8 engines are planned to be produced in 2024. Available ai: https://tass-ru/ekonomika/18995881 (accessed: September 02, 2024).
  5. Min P.G., Kablov D.E., Sidorov V.V., Vadeev V.E. Patterns of impurity behavior in the production of single-crystal heat-resistant nickel alloys and the development of effective methods for their refining. Prospects for the development of metallurgical technologies: abstracts VII Conf. of young specialists. Moscow, 2016, рp. 36–37.
  6. Sidorov V.V. The effect of impurities and surface-active additives on the formation of the structure and properties of high-heat-resistant casting alloys: thesis abstract, Dr. Sc. (Tech.). Moscow, 1989, 50 p.
  7. Pridancev M.V. The effect of impurities and rare earth elements on the properties of alloys. Moscow: Metallurgizdat, 1962, 208 p.
  8. Zhuanggi Hu, Hongwei Song. Effect of Phosphorus on Microstructure and Creep Property of IN718 Superalloy. Journal of material Science Technology, 2005, vol. 21, pp. 73–76.
  9. Chao Yuan, Fengshi Yin. Effect of Phosphorus on Microstructure and High Temperature Properties of a cast Ni-base Superalloy. Journal of Material Science Technology, 2002, vol. 18, no. 6, pp. 555–557.
  10. Holt R.T., Wallace W. Impurities and trace elements in nickel-base superalloys. International metals reviews, 1976, vol. 21, no. 1, pp. 1–24.
  11. Sun C., Huang R.F., Guo J.T., Hu Z.Q. Sulphur distribution in K24 cast nickel-base superalloy and its influence on mechanical properties. High Temperature Technology, 1988, vol. 6 (3), pp. 145–148.
  12. Tigrova G.D., Korkka S.I., Grebtsova T.M. Effect of silicon on the phase composition of nickel-based alloys. Metallovedenie i termicheskaya obrabotka metallov, 1980, no. 4, pp. 38–41.
  13. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Features of the technology of smelting and pouring modern foundry high-heat-resistant nickel alloys. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyenie, 2011, no. SP2, pp. 68–78.
  14. Kablov D.E. Regularities of nitrogen behavior in the production of single crystals of heat-resistant nickel alloys and improving their performance properties: thesis abstract, Cand. Sc. (Tech.). Moscow, 2012, 17 p.
  15. Kablov D.E., Sidorov V.V., Min P.G. Regularities of nitrogen behavior during production of single crystals of heat-resistant nickel alloys and its influence on their operational properties. Metallovedenie i termicheskaya obrabotka metallov, 2014, no. 1, pp. 8–12.
  16. Epishin A.L., Svetlov I.L., Petrushin N.V., Loshchinin Yu.V., Link T. Segregation in Single-Crystal Nickel-Base Superalloy. Defect and Diffusion Forum, 2011, vol. 309–310, pp. 121–126.
  17. Sarioglub C., Stinner C., Blanchere J.R. et al. The Control of Sulfur Content in Nickel-Base, Single Crystal Superalloys and Its Effect on Cyclic Oxidation Resistance. Superalloys-1996, 1996, pp. 71–80.
  18. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Production of cast bar (blend) preparations from modern cast high-heat resisting nickel alloys. All-Rus. Sci.-techn. conf. «Problems and perspectives of development of metallurgy and mechanical engineering with use of complete basic researches and research and development», Ekaterenburg, 2011, pp. 31–38.
  19. Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), paper no. 02. Available at: http://www.journal.viam.ru (accessed: September 02, 2024). DOI: 10.18577/2071-9140-2021-0-3-11-18.
  20. Heat resisting cast alloy on the basis of nickel and the product which has been executed of it: pat. 2740929 Rus. Federation; appl. 20.04.20; publ. 21.01.21.
  21. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  22. Gerasimov V.V., Visik E.M., Kolyadov E.V. On directional crystallization of large-sized castings on the UVNK-15 unit. Liteynoe proizvodstvo, 2013, no. 3, pp. 22–24.
  23. Gerasimov V.V., Kolyadov E.V. Technical characteristics and technological capabilities of the UVNK-9A and VIP-NK units for producing single-crystal castings from heat-resistant alloys. Liteynoe proizvodstvo, 2012, no. 11, pp. 33–37.
  24. Yakimovich P.V., Alekseev A.V. Determination of sulfur in casting heat-resistant nickel alloys by GD-MS. Trudy VIAM, 2020, no. 1, paper no. 11. Available at: http://www.viam-works.ru (accessed: September 02, 2024). DOI: 10.18557/2307-6046-2020-0-1-101-108.
  25. Sidorov V.V., Morozova G.I., Petrushin N.V., Kuleshova E.A., Kulebyakina A.M., Dmitrieva L.I. Phase composition and thermal stability of cast heat-resistant nickel alloy with silicon. Metally, 1990, no. 1, pp. 94–98.
  26. Yaoxiao Zhu, John Radavich, Zhi Zheng et al. Development and Long-Time Structural Stability of a Low Segregation Hf Free Superalloys – DZ 125L. Superalloys-2000, 2000, pp. 329–339.
  27. Mc Vay R.V., William P., Meier G.H., Pettit F.S. Oxidation of Low Sulfur Single Crystal Nickel-base Superalloys. Superalloys-1992, 1992, pp. 807–816.
  28. Tammy M. Simpson and Allen R. Price. Oxidation improvements of low sulfur processed supperalloys. Superalloys-2000, 2000, pp. 387–392.
  29. Mitchel A. Nitrogen in Superalloys. High Temperature Materials and Processes, 2005, vol. 24, no. 2, pp. 101–109.
  30. Sims C., Hagel V. Heat-resistant alloys. Moscow: Metallurgiya, 1976, 566 p.
  31. Gorbovets M.A., Hodinev I.A., Karashaev M.M., Ryzhkov P.V. Low cycle dwell fatigue testing of heat resistant metallic materials (review). Trudy VIAM, 2022, no. 5 (111), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 10, 2024). DOI: 10.18577/2307-6046-2022-0-5-123-137.
  32. Kablov D.E., Belyaev M.S., Sidorov V.V., Min P.G. The influence of sulfur and phosphorus impurities on low cycle fatigue of single crystals of ZhS36-VI alloy. Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 25–28. DOI: 10.18577/2071-9140-2015-0-4-25-28.