Sevalnev G.S., Nefedkin D.Yu., Dulnev K.V., Skorikova M.A. Study of the characteristics of maraging steel under tribotechnical loading // Proceedings of VIAM. 2024. No. 10 (140). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-10-3-12.

Study of the characteristics of maraging steel under tribotechnical loading

Sevalnev G.S., Nefedkin D.Yu., Dulnev K.V., Skorikova M.A.
Abstract

Metallographic and durometric studies and wear tests under dry sliding friction conditions of maraging steel 21NKMT after various types of heat treatment were carried out. It has been established that the samples after quenching and single aging have the lowest wear rate, while the samples after two-times aging have the highest hardness of 630 HV. The use of two-fold aging and overaging of 21NKMT steel leads to an increase in wear intensity by 12–33%.

Keywords
maraging steels, hardness, wear resistance, grain size, aging, friction coefficient, precipitation particles, intermetallides
Reference list
  1. Korobova E.N., Sevalnev G.S., Gromov V.I., Leonov A.V. Steels for the manufacture of roller bearings for special purposes (review). Trudy VIAM, 2021, no. 11 (105), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 05, 2024). DOI: 10.18577/2307-6046-2021-0-11-3-11.
  2. Gloeckner P., Rodway C. The evolution of reliability and efficiency of aerospace bearing systems. Engineering, 2017, vol. 9, no. 11, pp. 962–991.
  3. Krishna S.C., Tharian K.T., Chakravarthi K.V.A. et al. Heat treatment and thermo-mechanical treatment to modify carbide banding in AISI 440C steel: a case study. Metallography, Microstructure, and Analysis, 2016, vol. 5, no. 2, pp. 108–115.
  4. Geller Yu.A. Tool steels. Moscow: Metallurgiya, 1983, 525 p.
  5. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: January 24, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  6. Bakradze M.M., Voznesenskaya N.M., Leonov A.V., Krylov S.A., Tonysheva O.A. Development and research of high-strength corrosion-resistant steel for bearing parts. Metallurg, 2019, no. 11, pp. 39–44.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Bannykh I.O., Ashmarin A.A., Betzofen S.Ya. et al. Optimization of chemical composition and parameters of thermomechanical processing of TRIP steels based on new methods of X-ray tensiometry, texture and phase analysis. Metally, 2022, no. 6, pp. 66–72.
  9. Lukin E.I., Blinov V.M., Bannykh I.O. et al. Effect of the Quenching Temperature on the Structure and Mechanical Properties of Martensitic–Ferritic Corrosion-Resistant Nitrogen-Bearing 08Kh17N2AF Steel. Russian Metallurgy (Metally), 2023, no. 6, pp. 629–637.
  10. Blinov V.M., Antsyferova M.V., Bannykh I.O. et al. Structure and Properties of High-Strength Low-Alloy Martensitic Steels with an Overequilibrium Nitrogen Content. Russian Metallurgy (Metally), 2023, no. 6, pp. 649–656.
  11. Lukin E.I., Ashmarin A.A., Bannykh I.O. et al. Effect of the Reduction during Cold Rolling on the Phase Composition, Texture, and Residual Stresses in 20Kh15AN3MD2 Steel. Russian Metallurgy (Metally), 2023, vol. 2023, no. 11, pp. 1598–1605.
  12. Kuksenova L.I., Gerasimov S.A., Lapteva V.G. Wear resistance of structural materials. Moscow: Publ. house of Bauman Moscow State Technical Univ., 2011, 240 p.
  13. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.A. Study of the tribo-technical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening. Trudy VIAM, 2021, no. 10 (104), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 16, 2024). DOI: 10.18577/2307-6046-2021-0-10-3-11.
  14. Pokrovskaya N.G., Markova E.S., Shalkevich A.B. High-strength structural martensitic aging steels in aircraft construction. Aviatsionnaya promyshlennost, 2014, no. 1, pp. 24–28.
  15. Stephen W. Martensitic aging steels. High-strength steels. Moscow: Metallurgiya, 1969, pp. 235–257.
  16. Edneral A.F., Kardonsky V.M., Perkas M.D. Structural changes during aging of carbon-free iron-nickel martensite. Imperfections of the crystal structure and martensitic transformations. Moscow: Nauka, 1972, pp. 63–79.
  17. Perkas M.D., Kardonsky V.M. High-strength maraging steels. Moscow: Metallurgy, 1970, 223 p.
  18. Sevalnev G.S., Druzhinina M.E., Dulnev K.V., Mosolov A.N., Fomina L.Р., Chirkov I.A. Improvement of the tribotechnical characteristics of beryllium-containing steel VNS32-VI by surface modification. Trudy VIAM, 2022, no. 11 (117), paper no. 01. Available at: http://www.viam-works.ru (accessed: January 05, 2024). DOI: 10.18577/2307-6046-2022-0-11-3-14.
  19. Gorokhov A.Yu. Effect of VKS-210 steel structure on the defect of elastic modulus under fatigue impact. Aktualnye problemy gumanitarnykh i yestestvennykh nauk, 2015, no. 3-1, pp. 52–54.
  20. Perkas M.D., Strug M.D., Rusanenko V.V. Elinvar martensitic-aging steels with a high elastic limit. Metallovedenie i termicheskaya obrabotka metallov, 1991, no. 8, pp. 40–41.
  21. Markova E.S., Yakusheva N.A., Pokrovskaja N.G., Shalkevich A.B. Technological features of the production of maraging steel VKS-180. Trudy VIAM, 2013, no. 7, paper no. 01. Available at: http://www.viam-works.ru (accessed: February 10, 2024).
  22. Structural materials: reference book. Ed. B.N. Arzamasov. Moscow: Mashinostroenie, 1990, 688 p.
  23. Sadovsky V. D. Structural heredity in steel. Moscow: Metallurgiya, 1973, 208 p.
  24. Oshurina L.A. Analysis of the application of parameter sensors based on 21NKMT elinvar alloy. Innovatsii i investitsii, 2021, no. 3, pp. 169–171.
  25. García-León R.A., Martínez-Trinidad J., Campos-Silva I. et al. Wear maps of borided AISI 316L steel under ball-on-flat dry sliding conditions. Materials Letters, 2021, vol. 282, p. 128842.
  26. Kuksenova L.I., Alekseeva M.S. Effect of Preliminary Treatment on Tribotechnical Characteristics of Nitrided Structural Steels. Metal Science and Heat Treatment, 2023, vol. 65, no. 1-2, pp. 34–41.
  27. Kuksenova L.I., Savenko V.I. Physicochemical Tribomechanics of Antifriction Materials Operating in Heavy-Loaded Friction Pairs in Active Lubricating Media. Journal of Friction and Wear, 2023, vol. 44, no. 6, pp. 333–345.