Sagomonova V.A., Syty Y.V. Basic concepts of creation damping materials for aviation // Proceedings of VIAM. 2013. No. 11. Ст. 03. URL: https://www.viam-works.ru.

Basic concepts of creation damping materials for aviation

Sagomonova V.A., Syty Y.V.
Abstract

This paper deals with basic principles of creating damping materials for aviation use, namely basic theoretic concepts, requirements to the materials, different kinds of materials and their comparative characteristics.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kudisova L.Ya., Kuznetsov V.B., Kaurova N.F. Problemy strukturnogo shuma i zvukoizolyatsii tonkostennyh konstruktsiy [Aspects of structural noise and noise insulation of thin-walled structures]. M.: TsAGI im. prof. N.E. Zhukovskogo. 1991. 174 s.
  3. Solomatov V.I., Cherkasov V.D., Fomin N.E. Vibropogloschayuschie kompozitsionnye materialy [Vibration-absorbing composite materials. Saransk]. Saransk: Izd-vo Mordovskogo universiteta. 2001. 95 s.
  4. Askadskiy A.A., Luchkina L.V., Nikiforova G.G. Vibropogloschayuschie gradientnye polimernye materialy [Vibroabsorbing gradient polymer materials] //Plasticheskie massy. 2007. №4. S. 30–33.
  5. Sytyj Yu.V., Kislyakova V.I., Sagomonova V.A., Antyufeeva N.V. Perspektivnyj vibropogloschayuschiy material VTP-3V [VTP-3V advanced vibration-absorbing material] //Aviatsionnye materialy i tehnologii. 2012. №3. S. 47–49.
  6. Rao M.D. Recent applications of viscoelastic damping for noise control in automobiles and commercial airplanes //Journal of Sound and Vibration. 2003. №262. R. 457–474.
  7. Damped structural panel and method of making the same: rat. 6266427 US; opubl. 2001.
  8. Vibration damped sandwich systems having interlayers of vinyl acetate-ethylene copolimers: rat. 3640836 US; opubl. 1972.
  9. Method of forming noise-damping material with ultra-thin viscoelastic layer: rat. 6202462 US; opubl. 2001.
  10. Sperling L.H. Sound and Vibration Damping with Polymers: Basic Viscoelastic Definitions and Concepts /In: American Chemical Society Symposium Series. 1990. R. 5–23.
  11. Rongong J.A., Goruppa AA., Buravalla V.R. Plasma deposition of constrained layer damping coatings //Journal of Mechanical Engineering Science. 2004. V. 218. Part C. Р. 669–679.
  12. Oosting N.J., Hennessy J., Hanner D.T. Application of a Constrained Layer Damping Treatment to a Cast Aluminum V6 Engine Front Cover /In: Society of automotive engineers. New York. 2005. P. 2286.
  13. Method for manufacturing compartment made of steel/thermoplastic damping material composite structural plates: pat. 102825859 CN; opubl. 2012.
  14. Constrained layer damper, and related methods: pat/ 8377553 US; opubl. 2013.
  15. Acoustic damping compositions: pat. 8028800 US; opubl. 2011.
  16. Structural composite material with improved acoustic and vibration damping properties: pat. 2010/170746 A1 US; opubl. 2010.
  17. Multilayer and composition gradient structures with improved damping properties: pat. 2012/164907 A1 US; opubl. 2012.
  18. Energy absorbing thermoplastic elastomer: pat. 8051947 US; opubl. 2011.
  19. Li Hui, Zhang Yong-Bing, Ma Yu-Pu. Recent Advance in Vibration Damping Property of Polyurethane Interpenetrating Polymer Networks //Development and Application of Materials. 2008 (elektronnaya versiya).
  20. Molding material having vibration damping property and molded article: pat. 2013/0012641 A1 US; opubl. 2013.
  21. Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bol'shakov V.A. Novye vibropogloschayuschie materialy [Novel Vibration-absorbing Materials] //Aviatsionnye materialy i tehnologii. 2012. №2. S. 51–54.
  22. Petrova G.N., Perfilova D.N., Gryaznov V.I., Beyder E.Ya. Termoplastichnye elastomery dlya zameny rezin [Thermoplastic elastomers for the substitution of rubbers] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 302–308.