Visik E.M., Koljadov E.V., Kuzmina N.A. Influence of directional crystallization parameters on the structure of the intermetallic nickel alloy VIN4M-VI when casting single-crystal blanks of nozzle blades // Proceedings of VIAM. 2023. No. 9 (127). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-9-3-15.

Influence of directional crystallization parameters on the structure of the intermetallic nickel alloy VIN4M-VI when casting single-crystal blanks of nozzle blades

Visik E.M., Koljadov E.V., Kuzmina N.A.
Abstract

The directions of the development of casting blocks for casting small-sized blanks of nozzle blades at the UVNK-9A installation and the influence of the conditions of the technological process of directed crystallization on the formation of the single-crystal structure of the intermetallic alloy VIN4M-VI of KGO [001] are considered. The results of X-ray diffraction and metallographic studies of blanks of nozzle blades made of nickel alloy VIN4M-VI are presented, confirming the possibility of obtaining a single-crystal structure in them KGO [001], and the results of testing this alloy in pilot and serial production.

Keywords
intermetallic nickel alloys, directional crystallization, installations for single-crystal casting, single-crystal nozzle blades, microstructure
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Drozdov A.A., Povarova K.B., Morozov A.E., Antonova A.V., Bulakhina M.A., Aladieva N.A. Dandritic liquidation in single-zerolins of intermetallic alloys based on Ni3Al, alloyed Cr, Mo, W, Ti, Co, Re. Metally, 2015, no. 4, pp. 48–55.
  3. Buntushkin V.P., Bazileva O.A. Allocations based on nickel aluminides NiAl, Ni3Al for engineering. Aviatsionnaya promyshlennost, 1999, no. 2, pp. 47–50.
  4. Buntushkin V.P., Bazileva O.A. High-temperature foundry of the Ni3Al aluminum-resistant alloy. Aviacionnye materialy i tehnologii, 2000, no. 3, pp. 20–24.
  5. Kablov E.N., Povarova K.B., Buntushkin V.P., Kazan N.K., Bazilyov O.A. High-temperature alloys based on Ni3Al for neoclated nozzle and working blades of the gas turbine engine. Report Intersectoral Scientific and practical. Conf. "Problems of creating new materials for the air-cosmic industry". Moscow: VIAM, 2002, pp. 33–34.
  6. Gerasimov V.V., Petrushin N.V., Visik E.M. Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy. Trudy VIAM, 2015, no. 3, paper no. 01. Available at: http://www.viam-works.ru (accessed: May 10, 2023). DOI: 10.18577/2307-6046-2015-0-3-1-1.
  7. Kablov E.N., Ospennikova O.G., Petrushin N.V. New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades. Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
  8. Povarova K.B., Buntushkin V.P., Kazan N.K., Drozdov A.A. A comparative analysis of the principles of the creation of heat-resistant nickel super-payments and alloys based on Ni3Al (γ-phase). Perspektivnye materialy, 2005, no. 2, pp. 9–19.
  9. Kablov E.N., Petrushin N.V. Computer method for constructing casting heat-resistant nickel alloys. Foundry heat-resistant alloys. The effect of S.T. Kishkin. Moscow: Nauka, 2006, pp. 56–78.
  10. Petrushin N.V., Elyutin E.S., Korolev A.V. Monocrystalline heat-resistant alloys: composition, technology, structure and properties. Materials of All-Rus. Sci.-tech. Conf. “Fundamental and applied research in the field of creating cast-resistant nickel and intermetal alloys and highly effective technologies for the manufacture of GTD parts”. Moscow: VIAM, 2017, pp. 271–303.
  11. Visik E.M., Tikhomirova E.A., Petrushin N.V., Ospennikova O.G., Gerasimov V.V., Zhihushkin A.A. Technological testing of a new heat-resistant alloy with low density when casting turbine workers of monocrystalline blades. Metallurg, 2017, no. 2, рр. 34–40.
  12. Gerasimov V.V. From single-crystal uncooled blades to turbines blades with penetration (transpiration) cooling made by additive technologies (review on technology of single-crystal GTE bladescasting). Trudy VIAM, 2016, no. 10, paper no. 1. Available at: http://www.viam-works.ru (accessed: May 18, 2023). DOI: 10.18577/2307-6046-2016-0-10-1-1.
  13. Kablov E.N. Casting shoulder blades of gas turbine engines: alloys, technology, coating. Moscow: MISIS, 2006, 632 p.
  14. Kolyadov EV, Visik EM, Gerasimov VV, Arginbaeva E.G. The influence of directional solidification parameters on the structure and properties of the intermetallic alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 18, 2023). DOI: 10.18577/2307-6046-2019-0-3-14-26.
  15. Ma D., Wang F., Wu Q., Bogner S., Bührig A.S. Innovations in Casting Techniques for Single Crystal Turbine Blades of Superalloys. Superalloys 2016: Proceedings of the 13th International Symposium on Superalloys. Wiley, 2016, рр. 237–246. DOI: 10.1002/9781119075646.ch26.
  16. Elliot A.J., Karney G.B., Pollock T.M., Gigliotti M.F.X. Issue in Processing by the Liquid-Sn Assisted Directional Solidification Technique. Superalloys 2004. ТМS Minerals, Metals & Materials Society, 2004, pp. 421−445.
  17. Toloraya V.N., Demonis I.M., Ostroukhova G.A. The formation of a monocrystalline structure of alloy large-sized turbine blades of the GTD and GTU at the installations of high-gradient directed crystallization. Metallovedeniye i termicheskaya obrabotka metallov, 2011, no. 1, pp. 25–33.
  18. Kuzmina N.A., Petrushin N.V., Visik E.M., Eremin N.N., Naprienko S.A. Application of the Laue method to study the structure of a nickel heat-resistant alloy sample destroyed during mechanical processing. Trudy VIAM, 2020, no. 10 (92), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 18, 2023). DOI: 10.18577/2307-6046-2020-0-10-3-12.
  19. Tikhomirova E.A., Sidokhin E.F. Determination by the method of LAUE crystallographic orientation and devastating of the blocks of monocrystal products in the production of turbine shovels. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2011, no. 3 (27), pp. 43–49.
  20. Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 18, 2023). DOI: 10.18577/2307-6046-2019-0-12-11-19.
  21. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: May 22, 2023). DOI: 10.18577/2713-0193-2023-0-1-30-50.