Abstract

Reducing warpage and residual stresses during hardening is an urgent problem in the production of parts and semi-finished products from aluminum alloys. Water is usually used as a cooling medium during quenching, and, for volumetric forgings, hot or boiling water, depending on the composition of the alloy. However, water as a quenching medium has significant drawbacks: uneven (three-stage) cooling due to a change in the state of aggregation, sharpness of cooling and, accordingly, the creation of large warpage and residual stresses in the case of using cold water, an insufficient degree of reduction in warpage and residual stresses during cooling in hot water, low speed cooling and, accordingly, the deterioration of the properties of most alloys during quenching in boiling water. Discusses in detail various methods for reducing warping and residual stresses during hardening in parts made of high-strength aluminum alloys.

Keywords
aluminium alloy, low-distortion quenching, polymer medium, uphill quenching, residual stress, distortion, mechanical properties
Reference list
  1. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  2. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Aluminum alloys in aerospace engineering. Ed. E.N. Kablov. Moscow: Nauka, 2001, 192 p.
  3. Oglodkov M.S., Shchetinina N.D., Rudchenko A.S., Panteleev M.D. Directions of the development of promising aluminum-lithium alloys for aerospace engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
  4. Benarieb I., Ber L.B., Antipov K.V., Sbitneva S.V. Trends in development of wrought alloys of Al–Mg–Si–(Cu) system. Part 1 (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 14–22. DOI: 10.18577/2071-9140-2019-0-3-14-22.
  5. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  6. Antipov V.V., Grigoryev M.V., Konovalov A.N., Meshkov A.A., Serebrennikova N.Yu. Research of the influence of riveting on the low-cycle fatigue of riveted connection sheets of aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 3–8. DOI: 10.18577/2071-9140-2019-0-3-3-8.
  7. Koptyug V.A., Fridlyander I.N., Mikhailova I.F. et al. Cooling media with polymer additives for low-deformation hardening of aluminum alloys. Metallurgy of aluminum alloys. Moscow: Nauka, 1985, pp. 55–60.
  8. Moazam M.A., Honarpisheh M. Residual stress formation and distribution due to precipitation hardening and stress relieving of AA7075. Materials Research Express, 2019, no. 6. DOI: 10.1088/2053-1591/ab59b6.
  9. Koc M., Culp J., Altan T. Prediction of residual stresses in quenched aluminum blocks and their reduction through cold working processes. Journal of Materials Processing Technology, 2006, no. 174, pp. 342–354. DOI: 10.1016/j.jmatprotec.2006.02.007.
  10. Lin G.Y., Zhang H., Zhu W. et al. Residual stress in quenched 7075 aluminum alloy thick plates. Transactions of Nonferrous Metals Society of China, 2003, no. 13, pp. 641–644. DOI: 10.4236/msce.2021.94002.
  11. Robinson J.S., Hossain S., Truman C.E. et al. Residual stress in 7449 aluminium alloy forgings. Materials Science and Engineering: A, 2010, no. 527, pp. 2603–2612. DOI: 10.1016/J.MSEA.2009.12.022.
  12. Robinson J.S., Tanner D.A. Residual stress development and relief in high strength aluminium alloys using standard and retrogression thermal treatments. Materials Science and Technology, 2003, no. 19, pp. 512–518. DOI: 10.1179/026708303225001939.
  13. Sun Y.S., Jiang F.L., Zhang H., Su J., Yuan W.H. Residual stress relief in Al‒Zn‒Mg‒Cu alloy by a new multistage interrupted artificial aging treatment. Materials and Design, 2016, no. 92, pp. 281–287. DOI: 10.1016/j.matdes.2015.12.004.
  14. Bates C.E., Totten G.E. Procedure for quenching media selection to maximize tensile properties and minimise distortion in aluminium-alloy parts. Heat Treatment of Metals, 1988, no. 15, pp. 89–97. DOI: 10.1007/BF02831618.
  15. Hilder N. Polymer quenchants – a review. Heat Treatment of Metals, 1986, no. 13, pp. 15–26.
  16. Hilder N. The behavior of polymer quenchants. University of Aston in Birmingham, 1988, 404 р.
  17. Zhang J., Deng Y.L., Yang W. et al. Design of the multi-stage quenching process for 7050 aluminum alloy. Materials and Design, 2014, no. 56, pp. 334‒344. DOI: 10.1016/j.matdes.2013.09.029.
  18. Tanner D.A., Robinson J.S. Reducing residual stress in 2014 aluminum alloy die forgings. Materials and Design, 2008, no. 29, pp. 1489–1496. DOI: 10.1016/j.matdes.2007.07.002.
  19. Kolobnev N.I., Senatorova O.G. Patterns of changes in properties during hardening. Metallurgy of aluminum and its alloys: a reference book. Moscow: Metallurgiya, 1983, pp. 143–180.
  20. Schimanski K. Heat Treatment and Distortion – Challenge for Aircraft Industries. Proceedings of ICAA-12. Bremen, 2012, pp. 68–73.
  21. Ivanov A.L., Sidelnikov V.V., Nechaikina T.A., Kozlova O.Yu. Influence of low-deformation hardening on the complex of properties of sheet parts from aluminum alloys. Metallovedenie i termicheskaya obrabotka metallov, 2021, no. 10, pp. 9–15.
  22. Ivanov A.L., Senatorova O.G., Mitasov M.M., Antipov V.V., Straupenek M.E., Tormysheva N.Yu. Kinetics of cooling of sheet parts made of aluminum alloys during low-deformation hardening in a polymeric medium. Metallovedenie i termicheskaya obrabotka metallov, 2017, no. 11 (749), pp. 31–36.
  23. Masoudi S., Amirian Gh., Saeedi Eh., Ahmadi M. The effect of quench-induced residual stresses on the distortion of machined thin-walled parts. Journal of materials Engineering and performance, 2015, no. 24, pp. 3933–3941. DOI: 10.1007/s11665-015-1695-7.
  24. Robinson J.S., Donovan A.O., Wimpory R.C. Uphill quenching to reduce residual stress in aluminium alloy 7449 hollow structures. Experimental mechanics, 2022, no. 62, pp. 1411–1420. DOI: 10.1007/s11340-022-00836-8.
  25. Liu J., Jiang F., Tang M. et al. Reduced residual stress and retained properties in Al–Zn–Mg–Cu alloys using a novel cladding quenching process. Journal of materials research and technology, 2020, no. 9, pp. 7201–7209. DOI: 10.1016/j.jmrt.2020.04.080.