Morozova L.V. Investigation of the causes of loss of elastic properties of a 30H13 steel membrane // Proceedings of VIAM. 2023. No. 7 (125). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-7-15-22.

Investigation of the causes of loss of elastic properties of a 30H13 steel membrane

Morozova L.V.
Abstract

A comprehensive study of a membrane made of corrosion-resistant heat-resistant steel 30H13 was carried out in order to identify the causes of loss of elastic properties. The structure was evaluated, the chemical composition, the structure of the surface and the fracture of the part were studied using optical and electron microscopy, chemical analysis and non-destructive testing. It was found that during the production process, the membrane was subjected to high-temperature heating, causing grain growth (normalization), as well as prolonged electropolishing, leading to the identification of grain boundaries and the development of corrosion processes.

Keywords
fractography, crack, steel, corrosion, membrane, damage
Reference list
  1. Corrosion-resistant, heat-resistant and high-strength steels and alloys. Moscow: Intermet Engineering, 2000, 232 p.
  2. Grader of steels and alloys. 4th ed., rev. and add. Ed. Yu.G. Dragunov, A.S. Zubchenko Moscow: Mashinostroenie, 2014, 491 p.
  3. State Standard 5949–2018. Metal products from stainless steels and iron-nickel alloys, corrosion-resistant, heat-resistant and heat-resistant. Specifications. Moscow: Standartinform, 2018, 32 p.
  4. Andreeva L.E. Elastic elements of devices. Moscow: Mashgiz, 1962, 456 p.
  5. Rannev G.G. Intelligent measuring instruments. Moscow: Academy, 2010, 272 p.
  6. Friden J. Modern sensors. Moscow: Technosfera, 2006, 592 p.
  7. Krasnoyarsky V.V., Frenkel G.V., Nosov R.P. Corrosion and protection of metals. Moscow: Metallurgiya, 1969, 299 p.
  8. Protection against corrosion, aging and biodamage of machines, equipment and structures: a reference book in 2 vols. Ed. A.A. Gerasimenko. Moscow: Mashinostroenie, 1987, vol. 1, 688 p.
  9. State Standard 9.908–85. Unified system of protection against corrosion and aging. Metals and alloys. Methods for determining the indicators of corrosion and corrosion resistance. Moscow: Gosstandart SSSR, 1985, 79 p.
  10. State Standard 9.106–2021. Unified system of protection against corrosion and aging. Corrosion of metals. Terms and Definitions. Moscow: RST, 2021, 12 p.
  11. ISO 8044:2020. Corrosion of metals and alloys. ISO copyright office, 2020, 29 p.
  12. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  13. Kablov E.N. The key problem is materials // Trends and guidelines for Russia's innovative development. Moscow: VIAM, 2015, pp. 458–464.
  14. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  15. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DO1: 10.18577/2071-9140-2020-0-4-59-70.
  16. Erasov V.S., Oreshko E.I., Lutsenko A.N. Multilevel large-scale complex research of deformation of metal materials. Aviation materials and technologies, 2022, no. 1 (66), paper no. 11. Available at: http://www.journal.viam.ru (accessed: February 28, 2023). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  17. Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.
  18. Klevtsov G.V., Botvina L.R., Klevtsova N.A., Limar L.V. Fractodiagnostics of destruction of metallic materials and structures. Moscow: MISIS, 2007, 259 p.