Antipov V.V., Stepanova E.V., Babashov V.G., Ivakhnenko Yu.A., Butakov V.V. Influence of reinforcement with oxide refractory fibers on the flexibility of thermal insulation materials // Proceedings of VIAM. 2023. No. 5 (123). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-5-75-84.

Influence of reinforcement with oxide refractory fibers on the flexibility of thermal insulation materials

Antipov V.V., Stepanova E.V., Babashov V.G., Ivakhnenko Yu.A., Butakov V.V.
Abstract

In this work, we investigated the possibility of improving the flexibility of sealing heat-insulating materials by introducing a reinforcing component into the composition of the material in the form of chopped oxide ceramic refractory fibers. The effect of a reinforcing component on the change in the critical bending radius of samples of fibrous material based on ceramic refractory fibers has been studied. Sample tests showed an improvement in flexibility by 12–25 %, depending on the thickness and bulk density of heat-insulating materials.

Keywords
oxide ceramic fibers, fibrous heat-insulating material, critical bending radius, stapled roving, material density, roving length
Reference list
  1. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  3. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovacii, 2020, no. 6 (260), pp. 3–16.
  4. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  5. Chentsov I.V., Klibansky I.B., Mashchensky A.A., Kapitanov A.F. Technology of the most important industries. Minsk: Vysheyshaya shkola, 1980, part 1, 324 p.
  6. Polezhaev Yu.V., Yurevich F.B. Thermal protection. Ed. A.B. Lykov. Moscow: Energy, 1976, 391 p.
  7. Varrik N.M., Maksimov V.G. Features of obtaining high-temperature oxide fiber. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 6, paper no. 06. Available at: http://www.materialsnews.ru (accessed: November 23, 2022).
  8. Afanasov I.M., Lazoryak B.I. High temperature ceramic fibers. Moscow: Lomonosov Moscow State Univ., 2010, 51 p.
  9. Fibers from oxide ceramics: pat. 2396388 Rus. Federation; filed 10.02.10; publ. 10.08.10.
  10. Grashchenkov D.V., Balinova Yu.A., Tinyakova E.V. Ceramic fibers of aluminum oxide and materials based on them. Steklo i keramika, 2012, no. 4, pp. 32–35.
  11. Babashov V.G., Varrik N.M., Maksimov V.G., Samorodova O.N. Oxide fiber coated with silicon carbide for producing composite materials. Aviation materials and technologies, 2021, no. 3 (64), paper no. 09. Available at: http://www.journal.viam.ru (accessed: October 26, 2022). DOI: 10.18577/2713-0193-2021-0-3-94-104.
  12. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), paper no. 11. Available at: http://www.journal.viam.ru (accessed: October 31, 2022). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  13. Katz S.M. High temperature thermal insulation materials. Moscow: Metallurgiya, 1981, 231 p.
  14. Shirokorodyuk V.K. Effective thermal insulation materials. Krasnodar: KSAU, 2005, 130 p.
  15. Aksenov S.E. Modern thermal insulation materials. Arkhangelsk: AGTU, 2009, 119 p.
  16. Rakhimov R.Z., Shelikhov N.S. Modern thermal insulation materials. Kazan: KGASU, 2006, 392 p.
  17. Ermolenko I.N., Ulyanova T.M., Vityaz P.A., Fedorova I.L. Fibrous high temperature materials. Minsk: Nauka i tekhnologii, 1991, 255 p.
  18. Refractory fibrous ceramic insulation and process of making same: pat. US 6183852; filed 05.06.95; publ. 09.07.02.
  19. Perepelkin K.E. Reinforcing fibers and fibrous polymer composites. St. Petersburg: Nauchnye osnovy i tekhnologii, 2009, 380 p.
  20. Method for obtaining fibrous oxide material: pat. SU 1730233 A1; filed 28.03.89; publ. 30.04.92.
  21. Zhitnyuk S.V., Medvedev P.N., Sorokin O.Yu., Kachaev A.A. Formation of crystallographic texture in polycryctalline ceramics as a way to enhance properties (review). Trudy VIAM, 2022, no. 5 (111), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 11, 2022). DOI: 10.18577/2307-6046-2022-0-5-74-86.
  22. Stepanova E.V., Maksimov V.G., Ivakhnenko Yu.A. Internal defects of complex threads from oxide refractory fibers. Novye ogneupory, 2022, no. 2, pp. 56–60.
  23. Butakov V.V., Basargin O.V., Babashov V.G., Ivakhnenko Yu.A. A behavioral model of the fibrous material during bending tests. Trudy VIAM, 2014, no. 12, paper no. 6. Available at: http://www.viam-works.ru (accessed: November 14, 2022). DOI: 10.18577/2307-6046-2014-0-12-6-6.
  24. Kolyshev S.G., Basargin O.V., Butakov V.V. Experiments to determine the tensile strength of samples from lightweight flexible fibrous materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 5, pp. 8–11.
  25. Duka A.V. Development of technology for improved quartz HSM based on the development of the principles of structure formation of fibrous pulps: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 1989, 22 p.
  26. Khodakovsky M.D. Manufacture of glass fibers and fabrics. Moscow: Khimiya, 1973, 312 p.
  27. Chernyak M.G. Continuous glass fiber. Moscow: Khimiya, 1965, 322 p.
  28. Zhabin A.N., Sidorov D.V., Nyafkin A.N. Fibrous composite materials with a metal matrix (review). Trudy VIAM, 2021, no. 6 (100), paper no. 03. Available at: http://www.viam-works.ru (accessed: October 04, 2022). DOI: 10.18577/2307-6046-2021-0-6-27-35