Kuznetcova P.A., Tkachuk A.I., Lyubimova A.S., Eldjaeva G.B. Characteristics of the molten epoxy resin system VSE-62, processed by the injection methods, for the manufacture of highly loaded structural polymer composite materials // Proceedings of VIAM. 2023. No. 5 (123). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-5-43-53.

Characteristics of the molten epoxy resin system VSE-62, processed by the injection methods, for the manufacture of highly loaded structural polymer composite materials

Kuznetcova P.A., Tkachuk A.I., Lyubimova A.S., Eldjaeva G.B.
Abstract

In the present work, the thermophysical and physicomechanical characteristics of a molten epoxy resin system VSE-62, developed in SIC «Kurchatov Institute» – VIAM, are considered. The value of the glass transition temperature of the system, the kinetic parameters of the curing process with a different speed of the heating, the plot of the gelation time and flexural strength are given. The results of rheological tests in isothermal and dynamical modes are shown. The low viscosity of the system and long-term viability at high temperatures allows it to be used for the manufacture of various polymer composite materials by resin transfer moulding and vacuum assisted resin transfer moulding.

Keywords
epoxy resin system, one component epoxy resin system VSE-62, vacuum assisted resin transfer moulding, polymer composite material, gelation time
Reference list
  1. Kablov E.N. New generation Materials and technologies for their digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  2. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 10, 2022). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  3. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  4. Timoshkov P.N. Modern polymer composite materials for use in aviation technology. III All-Rus. sci.-tech. conf. "Polymer composite materials and production technologies of a new generation". Moscow: VIAM, 2018, pp. 40–56.
  5. Mikhailin Yu.A. Structural polymeric composite materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2008, 822 p.
  6. Kogan D.I. Technology for the manufacture of polymer composite materials by the method of impregnation with film binders: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2011, 139 p.
  7. Kudryavtseva A.N., Tkachuk A.I., Grigorieva K.N., Gurevich Ya.M. The use of epoxy resin system VSE-30, processed by the infusion technology, for the manufacture of low and medium loaded structural polymer composite materials. Trudy VIAM, 2019, no. 1 (73), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 12, 2022). DOI: 10.18577/2307-6046-2019-0-1-31-39.
  8. Kryzhanovsky V.K., Kerber M.L., Burlov V.V. Manufacture of products from polymeric materials. St. Petersburg: Professionya, 2004, 464 p.
  9. Vlasov S.V., Kandyrin L.B., Kuleznev A.V. et al. Fundamentals of plastics processing technology. Moscow: Khimiya, 2004, 600 p.
  10. Kholodnikov Yu.V. Methods for manufacturing products from composites. Mezhdunarodnyj zhurnal prikladnykh i fundamentalnykh issledovaniy, 2016, no. 6, pp. 214–221.
  11. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  12. Bratukhin A.G., Bogolyubov V.S., Sirotkin O.S. Technology for the production of products and integral structures from composite materials in mechanical engineering. Moscow: Gotika, 2003, 516 p
  13. Dushin M.I., Hrulkov A.V., Muhametov R.R. A choice of technological parameters of autoclave formation of details from polymeric composite materials. Aviacionnye materialy i tehnologii, 2011, no. 3, pp. 20–26.
  14. Leshukova I.V. Principal technologies for the manufacture of aircraft structures from composite materials: RTM and autoclave molding. Innovatsionnaya nauka, 2018, no. 1, pp. 14–16.
  15. Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review). Trudy VIAM, 2019, no. 11 (83), paper no. 03. Available at: http://www.viam-works.ru (accessed: October 20, 2022). DOI: 10.18577/2307-6046-2019-0-11-22-36.
  16. Arulappan C., Duraisamy A., Adhikari D., Gururaja S. Investigations on pressure and thickness profiles in carbon fiber-reinforced polymers during vacuum assisted resin transfer molding. Journal of Reinforced Plastics and Composites, 2015, vol. 34, pp. 3–18.
  17. Ricciardi M.R., Antonucci V., Durante M. et al. A new cost-saving vacuum infusion process for fiber-reinforced composites: Pulsed infusion. Journal of Composite Materials, 2014, vol. 48 (11), pp. 1365–1373.
  18. Marques A.T. Fibrous materials reinforced composites production techniques. Fibrous and Composite Materials for Civil Engineering Applications. Woodhead Publishing, 2011, pp. 191–215. DOI: 10.1533/9780857095583.3.191.
  19. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 15, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  20. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  21. Terekhov I.V., Tkachuk A.I., Donetsky K.I., Karavaev R.Yu. Technological and operational characteristics of the VSE-62 low-viscosity epoxy resin with increased pot life and its application. Aviation materials and technologies, 2021, no. 2 (63), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 15, 2022). DOI: 10.18577/2713-0193-2021-0-2-43-50.
  22. Kladovshchikova O.I., Tikhonov N.N., Zhdanov I.A., Sutyagina A.K., Nakhaeva A.V. Composite materials based on ultra-high molecular weight polyethylene. Uspekhi v khimii i khimicheskoy tekhnologii, 2019, vol. 3, no. 6, pp. 30–32.
  23. Lubin. J. Handbook of composite materials. Moscow: Mashinostroenie, 1988, 348 p.