Gulyaev I.N., Pavlovsky K.A. High modulus carbon plastics for civil aviation equipment (review) // Proceedings of VIAM. 2023. No. 3 (121). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-3-95-106.

High modulus carbon plastics for civil aviation equipment (review)

Gulyaev I.N., Pavlovsky K.A.
Abstract

The review of carbon fiber reinforced plastics based on high–modulus carbon fiber and woven reinforcing fillers developed at the National Research Center «Kurchatov Institute» – VIAM is presented. The difference between high-modulus reinforcing fillers and high-strength fillers is shown. The main domestic and foreign fiber brands are presented, as well as information on the elastic-strength characteristics of the developed high-modulus carbon fiber plastics, including at various temperatures. The comparison of domestic carbon fiber plastics with foreign materials of similar composition and structure is carried out.

Keywords
polymer composite material (PCM), high-modulus carbon fiber, carbon fiber, graphitized fiber, structural properties of PCM, aviation materials
Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  2. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. New materials are needed for space exploration. Nauchnaya Rossiya. Available at: https://scientificrussia.ru/interviews/akademik-e-n-kablov-dlya-osvoeniya-kosmosa-nuzhny-novye-
  4. materialy (accessed: June 10, 2022).
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer composite materials: structure, properties, technology: textbook. Ed. A.A. Berlin. 3rd ed., rev. and add. St. Petersburg: Profession, 2011, 556 p.
  7. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 10, 2022). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  8. Sidorina A.I., Gunyaeva A.G. Carbon fiber market. Khimicheskie volokna, 2016, no. 4, pp. 48–53.
  9. Startsev O.V., Khristoforov D.A., Kolyushnichenko A.B., Fizulov B.G., Rumyantsev A.F., Gunyaev G.M., Raskutin A.E. Dimensional stability of high-modulus carbon fibers and carbon plastics based on them. Reports of intersectoral scientific-practical. conf. "Problems of creating new materials for the aerospace industry in the XXI century". Moscow: VIAM, 2002, p. 87.
  10. Carbon fiber: high-tech carbon fiber based on PAN precursor. Available at: https://umatex.com/production/fiber/ (accessed: July 20, 2022).
  11. Aviation materials: a reference book in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, vol. 7: Polymer composite materials, 2010, 210 p.
  12. TenaxTM Filament Yarn. Available at: https://www.teijincarbon.com/products/tenaxr-carbon-fiber/tenaxr-filament-yarn (accessed: February 03, 2023).
  13. Valueva M.I., Evdokimov A.A., Nacharkina A.V., Gubin A.M. Polymer composite materials and technologies in the automotive industry (rеview). Trudy VIAM, 2022, no. 1 (107), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2022-0-1-53-65.
  14. Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 15, 2022). DOI: 10.18577/2307-6046-2022-0-5-87-95.
  15. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  16. Raskutin A.E. Polymer composite materials of a new generation for aviation and space technology. Report conf. "Modern achievements in the field of creating promising non-metallic composite materials and coatings for aviation and space technology". Moscow: VIAM, 2015. Available at: https://conf.viam.ru/conf/172/proceedings (accessed: May 25, 2022).
  17. Raskutin A.E. Structural carbon plastics based on new melt-type binders and Porcher fabrics. Novosti materialovedeniya. Nauka i tekhnika, 2013, no. 5. URL: http://materialsnews.ru (date of access: 04.06.2022).
  18. Mishurov K.S., Mishkin S.I., Gunyaeva A.G. Polymer composite materials for advanced aircraft engines. Materials of II All-Rus. sci.-tech. conf. "Polymer composite materials and production technologies of a new generation". Moscow: VIAM, 2017, pp. 131–145.
  19. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  20. Gunyaeva A.G. Developments of FSUE "VIAM" in the field of polymer composite materials for aviation and other industries. Reports of IV Interdisciplinary scientific forum with International participation "New materials and promising technologies": in 3 vols. Moscow: Buki Vedi, 2018, vol. 3, рр. 71–72.
  21. Valueva M.I., Zelenina I.V., Mishurov K.S., Gulyaev I.N. Review of publications on the development of blades made of polymer composite materials for an aircraft engine fan. Vestnik mashinostroeniya, 2019, no. 2, pp. 34–41.
  22. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  23. Gunyaeva A.G., Raskutin A.E., Gulyaev I.N., Sidorina A.I., Mishkin S.I. Polymer composite materials of a new generation for the aviation, electrical and construction industry. Reports of II Intern. sci.-tech. conf. "New materials and technologies for deep processing of raw materials – the basis for the innovative development of the Russian economy". Moscow: VIAM, 2017. Available at: http://conf.viam.ru/conf/254/proceedings (accessed: May 25, 2022).
  24. High temperature plastics market by type (polysulfones, polyimides, polyphenylene sulfide, fluoropolymers, and others), by end-use industries (electrical & electronic, transportation, industrial, medical, and others) – Global trends & forecast to 2019. Available at: https://www.marketsandmarkets.com/Market-Reports/high-temperature-plastics-market-1192.html (accessed: November 17, 2021).
  25. Shimkin A.A., Ponomarenko S.A., Mukhametov R.R. Study of the curing process of a diphthalonitrile binder. Zhurnal prikladnoy khimii, 2016, vol. 89, no. 2, pp. 256–264.
  26. Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 15, 2022). DOI: 10.18577/2307-6046-2016-0-2-8-8.
  27. Raskutin A.E. Heat-resistant carbon plastics for aircraft structures operating at temperatures up to 400 °C: Cand. Sc. (Tech.). Moscow, 2007, 166 p.
  28. Valevin E.O., Zelenina I.V., Marakhovsky P.S., Gulyaev A.I., Bukharov S.V. Investigation of the effect of heat and moisture exposure on the phthalonitrile matrix. Materialovedenie, 2015, no. 9, pp. 15–19.