Terekhin A.L., Leonov A.A., Trofimov N.V., Grinevich A.V. Features of fatigue failure of magnesium based alloy samples // Proceedings of VIAM. 2023. No. 12 (130). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-12-38-52.

Features of fatigue failure of magnesium based alloy samples

Terekhin A.L., Leonov A.A., Trofimov N.V., Grinevich A.V.
Abstract

Data on the cyclic durability of magnesium alloy samples of the Mg–REM–Zr system are presented. The fatigue characteristics of corset samples and notched samples were assessed at loading cycle asymmetry coefficients R = 0,1 and R = –1. For corset samples, the factors determining cyclic durability are the size of the inclusions; for samples with a notch, the location of the defect relative to the plane of the notch. Fractograms of specimen fractures are presented. The possibility of increasing the fatigue resistance of an alloy of the Mg–REM–Zr system by improving the quality of casting has been established.

Keywords
magnesium alloy, cyclic durability, cycle asymmetry, stress concentration factor, defects, fractography
Reference list
  1. Trofimov N.V., Leonov A.A. Study of the influence of alloying elements (Nb and Ti) on the impurity content and mechanical properties of a high-strength magnesium alloy of the Mg–Zn–Zr system. Metally, 2020, no. 3, pp. 14–19.
  2. Mukhina I.Yu., Duyunova V.A., Uridiya Z.P. Promising cast magnesium alloys. Liteynoe proizvodstvo, 2013, no. 5, pp. 2–5.
  3. Magnesium Alloys. Design, Processing and Properties. Ed. Frank Czerwinski. IntechOpen, 2011. 540 p. DOI: 10.5772/560.
  4. Luo A.A. Magnesium casting technology for structural applications. Journal of Magnesium and Alloys, 2013, vol. 1, pp. 2–22. DOI: 10.1016/j.jma.2013.02.002.
  5. Mukhina I.Yu., Leonov A.A. Fluxes in the metallurgy of magnesium alloys. Vse materialy. Entsiklopedicheskiy spravochnik, 2017, no. 8, pp. 19–25.
  6. Rycerz L. Practical remarks concerning phase diagrams determination on the basis of differential scanning calorimetry measurements. Journal of Thermal Analysis and Calorimetry, 2013, vol. 113, pp. 231–238. DOI: 10.1007/s10973-013-3097-0.
  7. Duyunova V.A., Uridiya Z.P. Study of the flammability of cast magnesium alloys of the Mg–Zn–Zr system. Liteyshchik Russii, 2012, no. 11, pp. 21–23.
  8. Leonov A.A., Trofimov N.V., Duyunova V.A., Uridia Z.P. Trends in the development of cast magnesium alloys with an increased ignition temperature (review). Trudy VIAM, 2021, no. 2 (96), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 25, 2023). DOI: 10.18577/2307-6046-2021-0-2-3-9.
  9. Mukhina I.Yu. Research of metal systems based on magnesium and development of principles for creating corrosion-resistant magnesium alloys. Metallovedenie i termicheskaya obrabotka metallov, 2014, no. 1, pp. 8–12.
  10. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  11. Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
  12. Duyunova V.A., Leonov A.A., Trofimov N.V. Study of the influence of rare earth elements and heat treatment on the structure and properties of a heat-resistant cast magnesium alloy of the Mg–REM–Zr system. Metally, 2020, no. 5, pp. 58–63.
  13. Kablov E.N. Modern materials are the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  14. Belyaev M.S., Gorbovec M.A. About discontinuity of LCF diagram in S-N coordinates for Ni-based superalloy. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 103–108. DOI: 10.18577/2071-9140-2014-s4-103-108.
  15. Grinevich A.V., Rumyancev Yu.S., Morozova L.V., Terehin A.L. Study of fatigue life of 1163-T and V95o.ch.-T2 aluminum alloys after surface hardening. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 93–102. DOI: 10.18577/2071-9140-2014-s4-93-102.
  16. Belyaev M.S., Terentev V.F., Gorbovec M.A., Bakradze M.M., Goldberg M.A. Low-cycle fatigue for a given deformation and parameters of elastic-plastic deformation of superalloy VZh175. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 87–92. DOI: 10.18577/2071-9140-2014-0-s4-87-92.
  17. Grinevich D.V., Gulina I.V., Yakovlev N.O., Dzandarov D.-S.V., Glagovsky A.A., Ermakova Yu.V. Study of the influence of fatigue loading parameters on the durability of aircraft slat diaphragm lugs. Zavodskaya laboratoriya. Diagnostika materialov, 2023, no. 6, vol. 89, pp. 76–82.
  18. Iakovlev N.O., Selivanov A.A., Gulina I.V., Grinevich A.V. Revisiting the durability of hinged-bolt connections. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-4-79-85.
  19. Erasov V.S., Avtaev V.V., Oreshko E.I., Yakovlev N.O. Strain-controlled testing advantages at static tension and repeated-static tension. Trudy VIAM, 2018, no. 10 (70), paper no. 10. Available at: http://www.viam-works.ru (accessed: August 25, 2023). DOI: 10.18577/2307-6046-2018-0-9-92-104.
  20. Oreshko E.I., Erasov V.S., Grinevich D.V., Sershak P.V. Review of criteria of durability of materials. Trudy VIAM, 2019, no. 9 (81), paper no. 12. Available at: http://www.viam-works.ru (accessed: August 25, 2023). DOI: 10.18577/2307-6046-2019-0-9-108-126.
  21. Yakovlev N.O., Grinevich D.V., Mazalov P.B. Mathematical modeling of the stress-strain state during compression of a mesh structure synthesized by selective laser melting. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Natural Sciences, 2018, no. 6 (81), pp. 113–127.
  22. Mitrakov O.V., Yakovlev N.O., Yakusheva N.A., Grinevich A.V. Destruction features of steel 20ХГСН2МФА-ВД during the fracture toughness test. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 49–56. DOI: 10.18577/2071-9140-2019-0-1-49-56.
  23. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Qualification tests and researches of durability of aviation materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 440–448.