Kozlov I.A., Volkov I.A., Fomina M.A., Zakharov К.Е. Features of chemical oxidation of semi-finished products obtained by selective laser melting from a metal powder composition of the alloy VAS1 // Proceedings of VIAM. 2023. No. 11 (129). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-11-90-98.
Features of chemical oxidation of semi-finished products obtained by selective laser melting from a metal powder composition of the alloy VAS1
Abstract
The work is devoted to the adaptation of the traditional technology of chemical oxidation of parts and workpieces made of aluminum alloys obtained by traditional methods for surface treatment of parts manufactured by selective laser fusion and metal powder composition of the VAC1 alloy. The work investigated the compatibility and influence of the main chemical components of electrolytes on the stability of solutions and the quality of the formed coating. The performance of electrolytes for oxidation and various options for chemical preparation of the surface of samples from the alloy VAC1 are considered.
Keywords
chemical oxidation, corrosion, coatings, additive technologies, aluminum alloys
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
- Kablov E.N. Innovative development is the most important priority of the state. Metally Evrazii, 2010, no. 2, pp. 6–11.
- Kablov E.N. What will the future be made of? New generation materials, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Aboulkhair N.T., Everitt N.M., Ashcroft I., Tuck C. Reducing porosity in AlSi10Mg parts processed by selective laser melting. Additive Manufacturing, 2014, vol. 1–4, pp. 77–86.
- Prashanth K.G., Scudino S., Klauss H.J. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment. Materials Science & Engineering: A, 2014, vol. 590, pp. 153–160.
- Weingarten С., Buchbinder D. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg. Journal of Materials Processing Technology, 2015, vol. 221, pp. 112–120.
- Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova L.B., Zaitsev D.V. Formation of metastable phases during the decomposition of a solid solution during the artificial aging of Al alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17.
- Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metalmatrix composite materials on the basis of Al–SiC. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 373–380.
- Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
- Sbitneva S.V., Lukina E.А., Benarieb I. Some structural features of aluminum alloys obtained by selective laser melting (review). Trudy VIAM, 2023, no. 1 (119), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 22, 2023). DOI: 10.18577/2307-6046-2023-0-1-69-83.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr IN additive manufacturing (review) Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 24, 2023). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Kravchenko D.V., Kozlov I.A., Nikiforov A.A. Methods for preparing the surface of aluminum alloys for electroplating (review). Trudy VIAM, 2021, no. 6 (100), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 04, 2023). DOI: 10.18577/2307-6046-2021-0-6-82-99.
- Zhelonkina S.I. Review of modern methods of preparing the surface of aluminum alloys for the application of metal coatings (part 1). Uprochnyayushchie tekhnologii i pokrytiya, 2021, vol. 17, no. 5 (197), pp. 227–231.
- Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.