Chaykun A.М., Yumashev O.B. Features of the development of the formula of frost-resistant ozone-resistant rubber based on EPDM rubber // Proceedings of VIAM. 2022. No. 9 (115). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-9-58-67.

Features of the development of the formula of frost-resistant ozone-resistant rubber based on EPDM rubber

Chaykun A.М., Yumashev O.B.
Abstract

The article shows the main directions for the development of a formulation for frost-resistant ozone-resistant rubber for sealing purposes. Currently, there are problems with the durability of the operation of parts made of rubber grade NO-68-1 due to the instability of the raw material base of rubbers. A comprehensive analysis of rubbers of various composition and structure was carried out. Based on the results of the analysis, ethylene-propylene, ethylene-propylene diene, and propylene oxide rubbers were selected as the polymer base. Mixtures of various compositions are made from these rubbers. According to the test results, the optimal composition of frost-resistant ozone-resistant rubber was selected.

Keywords
rubber, ethylenepropilene rubber, propileneoxide rubber, sulphur, peroxide, cold resistance, ozone-resistance
Reference list
  1. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  2. Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  3. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  4. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Fedyukin D.L., Makhlis F.A. Technical and technological properties of rubbers. Moscow: Khimiya, 1985, 240 p.
  7. Seals and sealing technology: reference book. Ed. A.I. Golubev, L.A. Kondakov. Moscow: Mashinostroenie, 1986, 464 p.
  8. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review). Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  9. Mikhailin Yu.A. Structural polymeric composite materials. 2nd ed. St. Petersburg: Nauchnye osnovy i tekhnologii, 2016, 820 p.
  10. Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Features of old-resistant rubbers on the basis on different unvulcanized rubbers. Trudy VIAM, no. 12, paper no. 04. Available at: http://www.viam-works.ru (accessed: April 13, 2022).
  11. Nurmukhametova A.N., Zenitova L.A. Methods for obtaining nanodispersed fillers. Proceedings of XII Int. conf. young scientists, students and graduate students "Synthesis, study of properties, modification and processing of macromolecular compounds – IV Kirpichnikov Readings". Kazan: Institute of Catalysis Boreskov SB RAS, 2008, p. 120.
  12. Thr big reference book for specialists in rubbers: at 2 parts. Moscow: Tekhinform, 2012, 1385 p.
  13. Naumov I.S., Chaikun A.M., Eliseev O.A. Russian and International Standards for Test Methods for Rubbers, Raw Rubber Compounds and High Molecular Weight Rubbers. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 11, pp. 4–13.
  14. Rubber technology: compounding and testing. Trans. from Engl. St. Petersburg: Nauchnye osnovy i tekhnologii, 2010, 632 p.
  15. Semenova S.N., Chaykun A.M., Suleymanov R.R. Ethylene-propylenediene rubber and its use in rubber materials for special purposes (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 23–30. DOI: 10.18577/2071-9140-2019-0-3-23-30.
  16. Kablov E.N., Semenova S.N., Suleymanov R.R., Chaykun A.M. Prospects for the use of ethylene-propylenediene rubber as part of cold resistant rubber. Trudy VIAM, 2019, no. 12 (84), paper no. 4. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2019-0-12-29-36.
  17. Semenova S.N., Chaikun A.M., Suleimanov R.R. Influence of the vulcanizing system on the temperature properties of rubber based on ethylene propylene rubber. Kauchuk i rezina, 2020, vol. 79, no. 4, pp. 210–213.
  18. Hoffmann V. Vulcanization and vulcanizing agents. Leningrad: Khimiya, 1968, 464 p.
  19. Govorova O.A., Kanauzova A.A., Saveliev A.L. Modification of ethylene-propylene rubbers and rubbers based on them. Moscow: TsNIITENeftekhim, 1990, p. 69.
  20. Kamenev Yu.G., Mironyuk V.P., Greshanovsky V.A. Influence of MVR of SKEP rubbers on their plastoelastic and technological properties. Kauchuk i rezina, 1973, no. 6, pp. 13–16.
  21. Kisin K.V., Lovchikov V.A., Mironyuk V.P., Romanikhin V.B. Study of the microstructure of ethylene-propylene rubbers by 13C NMR. Kauchuk i rezina, 1981, no. 6, pp. 13–16.
  22. Stereoregular rubbers. Ed. W. Saltman; trans. from English. Z.Z. Vysotsky. Moscow, 1981, vol. 1, 492 p.
  23. Synthetic rubber. Ed. I.V. Garmonov. 2nd ed. Leningrad: Khimiya, 1983, 559 p.
  24. Mironyuk V.P. Dependence of the vulcanization activity of SCEP on the nature of the third monomers. Kauchuk i rezina, 1991, no. 2, pp. 13–16.
  25. Mironyuk V.P., Kurlyand S.K., Vasileva M.A., Afanasiev I.D. Influence of the degree of crystallinity of the copolymer of ethylene, propylene and ethylidenenorbornene (EPDM-E) on their mechanical properties. Kauchuk i rezina, 1977, no. 7, pp. 14–17.
  26. Mironyuk V.P., Reikh V.N., Livshits I.A., Sukhotina T.M. Properties of ternary copolymers of ethylene, propylene and ethylidenenorbornene. Kauchuk i rezina, 1973, no. 1, pp. 7–10.
  27. Mironyuk V.P., Sidorovich V.A. Influence of the molecular structure of ethylene-propylene rubbers on their elastic properties. Kauchuk i rezina, 1981, no. 3, pp. 8–10.
  28. Shershnev V.A., Yulovskaya V.D. Problems of vulcanization in connection with the formation of network and phase structures in mixtures of elastomers. Kauchuk i rezina, 2000, no. 6, p. 16.
  29. Bukhina M.F., Kurlyand S.K. Frost resistance of elastomers. Moscow: Khimiya, 1989, 176 p.
  30. Zuev Yu.S., Degteva T.G. Service life of elastomers conditions. Moscow: Khimiya, 1986, 264 p.
  31. Dick J.S. Rubber and resin: compounding, structure and testing. Trans. from Engl. Ed. V.A. Shershnev. St. Petersburg: Nauchnye osnovy i tekhnologii, 2010, 620 p.
  32. Rubber and resin. Science and technology. Ed. J. Mark, B. Erman, F. Eyrich; trans from Engl. Ed. A.A. Berlin, Yu.L. Morozov. Dolgoprudny: Intellekt, 2011, 768 p.
  33. Kuleznev V.N., Shershnev V.A. Chemistry and physics of polymers. Moscow: KolosS, 2007, 367 p.
  34. Shuldeshov E.M. Sound-proof properties of aviation heatsound-proof materials. Trudy VIAM, 2019, no. 12 (84), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 20, 2022). DOI: 10.18577/2307-6046-2019-0-12-37-45.
  35. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
  36. Komissarzhevsky V.K., Kerber M.L. Polymer composite materials: structure, properties, application. St. Petersburg: Professiya, 2008, 560 p.
  37. Kuznetsova V.A., Kozlova A.A., Zheleznyak V.G., Shapovalov G.G. Influence of elastomeric modifiers on properties of metal-polymeric compositions. Trudy VIAM, 2019, no. 8 (80), paper no. 06. URL: http://www.viam-works.ru (accessed: June 20, 2022). DOI: 10.18577/2307-6046-2019-0-8-46-55.
  38. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  39. Oreshko E.I., Erasov V.S., Grinevich D.V., Sershak P.V. Review of criteria of durability of materials. Trudy VIAM, 2019, no. 9 (81), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 20, 2022). DOI: 10.18577/2307-6046-2019-0-9-108-126.