Alekseev A.V., Yakimovitch P.V. Analysis of praseodyme by the ICP-MS method // Proceedings of VIAM. 2022. No. 7 (113). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-7- 116-124.
Analysis of praseodyme by the ICP-MS method
Abstract
The content of impurities of 33 elements (Li, Be, B, Na, Mg, Al, P, K, Ca, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ga, As, Se, Rb , Sr, Zr, Mo, Cd, Cs, Ba, Re, Tl, Pb, Bi, Th, U) in a praseodymium sample by inductively coupled plasma mass spectrometry (ICP-MS). The technique of sample dissolution and its preparation for analysis is given. Spectral interferences are eliminated by applying mathematical correction equations, a reaction-collision cell, and by adjusting the plasma power.
Keywords
inductively coupled plasma mass spectrometry, ICP-MS, rare earth metals, determination of harmful impurities, analysis of rare earth metals, microwave sample preparation
Reference list
- Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
- Korolev D.V., Stolyankov Yu.V., Piskorsky V.P., Valeev R.A., Bahmetiev M.V., Dvorezkaya E.V., Koplak O.V., Morgunov R.B. Magnetic properties and magnetic strip domains in micro stripes PrDyFeCoB. Aviation materials and technologies, 2021, no. 3 (64), paper no. 08. Available at: http://www.journal.viam.ru (accessed: June 06, 2021). DOI: 10.18577/2713-0193-2021-0-3-86-93.
- Cherednichenko I.V., Ospennikova O.G., Piskorsky V.P., Valeev R.A., Buzenkov A.V. Economic aspects of the production of permanent magnets. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 4 (22). Art. 06. Available at: http://www.materialsnews.ru (accessed: June 06, 2021).
- Korolev D.V., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Morgunov R.B. The method of hot deformation for the manufacture of the permanent magnets of REM–Fe–B by the spark plasma sintering (review). Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 11–18. DOI: 10.18577/2071-9140-2017-0-4-11-18.
- Kablov E.N., Ospennikova O.G., Cherednichenko I.V., Rezchikova I.I., Valeev R.A., Piskorskij V.P. Influence of Cu content to phase structure and magnetic properties of thermostable sintered magnets of Nd–Dy–Fe–Co–B and Pr–Dy–Fe–Co–B systems. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 11–19. DOI: 10.18577/2071-9140-2015-0-S2-11-19.
- Kablov E.N., Ospennikova O.G., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Korolev D.V. Properties dependence of the Nd–Dy–Fe–Co–B sintered materials on technological parameters. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 24–29. DOI: 10.18577/2071-9140-2015-0-S2-24-29.
- Lutsenko A.N., Perov N.S., Chabina E.B. The new stages of development of Testing Center. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level RM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- State Standard 23862.20–79. Rare earth metals and their oxides. Methods for the determination of vanadium. Moscow: Gosstandart of the USSR, 1979, pp. 1–3.
- State Standard 23862.21–79. Rare earth metals and their oxides. Methods for the determination of chromium. Moscow: Gosstandart of the USSR, 1979, pp. 1–2.
- State Standard 23862.4–79. Rare earth metals and their oxides. Spectral method for the determination of vanadium, iron, cobalt, silicon, manganese, copper, nickel, lead, titanium, chromium. Moscow: Gosstandart of the USSR, 1979, pp. 1–4.
- Zhernokleeva K.V., Baranovskaya V.B. Analysis of Pure Scandium, Yttrium, and Their Oxides Using Methods of Inductively Coupled Plasma Atomic Emission Spectrometry and Inductively Coupled Plasma Mass Spectrometry. Inorganic Materials, 2011, vol. 47, no. 15, pp. 1627–1634.
- Shu-Xiu Z., Murachi S., Imasaka T., Watanabe M. Determination of Rare Earth Impurities in Ultrapure Europium Oxide by Inductively-Coupled Plasma Mass Spectrometry. Analytica Chimica Acta, 1995, vol. 314, no. 4, pp. 193–201.
- Pupyshev A.A., Epova E.N. Spectral noise of polyatomic ions in the method of mass spectrometry with inductively coupled plasma. Analytics and control, 2001, vol. 5, no. 4, pp. 335–369.
- Leikin A.Yu., Karandashev V.K., Lisovsky S.V., Volkov I.A. The use of a reaction-collision cell for the determination of impurity elements in rare earth metals using the ICP-MS method. Zavodskaya laboratoriya. Diagnostika materialov, 2014, vol. 80, no. 5, pp. 6–9.
- Yakimovich P.V., Alekseev A.V., Min P.G. Determination of low phosphorus content in heat-resistant nickel alloys by ICP-MS method. Trudy VIAM, 2014, no. 10, paper no. 02. Available at: http://viam-works.ru (accessed: June 06, 2021). DOI: 10.18577/2307-6046-2014-0-10-2-2.
- Karandashev V.K., Zhernokleeva K.V., Karpov Yu.A. The use of doubly charged ions in the determination of some rare earth elements in neodymium, samarium, europium and their compounds by inductively coupled plasma mass spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2012, vol. 78, no. 12, pp. 5–10.