Khrulkov A.V., Donetskiy K.I., Usacheva M.N., Goryansky A.N. Infusion methods for the manufacture of polymer composite materials (review). Part 2 // Proceedings of VIAM. 2022. No. 7 (113). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-7- 50-62.

Infusion methods for the manufacture of polymer composite materials (review)

Part 2
Khrulkov A.V., Donetskiy K.I., Usacheva M.N., Goryansky A.N.
Abstract

Polymer composite materials (PCM) are increasingly replacing traditional materials. New PCMs are constantly being developed, which are more economical and at the same time provide high-quality manufacturing of parts and structures from them. The infusion process has a well-established position among such processes as automated winding and automated prepreg lay-up followed by autoclaving. However, when using autoclave technology, there are restrictions on the dimensions of the molded parts, in addition, this method is quite expensive to operate. Therefore, the infusion process is increasingly used in the manufacture of parts in aircraft and shipbuilding, the construction industry, etc.

Keywords
infusion, vacuum infusion, polymer composite materials, autoclave molding, economic efficiency
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Kablov E.N. VIAM: New generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  5. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  6. Epoxy binder: pat. 2754399 Rus. Federation; filed 02.11.20; publ. 01.09.21.
  7. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: September 10, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  8. Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
  9. Timoshkov P.N., Khrulkov A.V., Yazvenko L.N. Composite materials in automotive industry (review). Trudy VIAM, 2017, no. 6 (54), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 10, 2021). DOI: 10.18577/2307-6046-2017-0-6-7-7.
  10. Borshchev A.V., Gusev Y.A. Development and implementation of PCM in automotive industry, varieties of HP-RTM processes. Aviacionnye materialy i tehnologii, 2014, no. 4, pp. 48–52. DOI: 10.18577/2071-9140-2014-0-4-48-52.
  11. Doriomedov M.S. Russian and world market of polymer composites (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 10, 2021). DOI: 10.18577/2307-6046-2020-67-29-37.
  12. Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 24–28. DOI: 10.18577/2071-9140-2014-0-s2-24-28.
  13. Heider D., Simacek P., Dominauskas A. et al. Infusion design methodology for thick-section, low-permeability preforms using inter-laminar flow media. Composites. Part A: Applied Science and Manufacturing, 2007, vol. 38 (2), pp. 525–534.
  14. Plastic transfer molding techniques for the production of fiber reinforced plastic structures: pat. US4902215A; filed 08.06.88; publ. 20.02.90.
  15. Vacuum-forming fibre reinforced resin composites: pat. GB2257938A; filed 08.06.88; publ. 27.01.93.
  16. Vacuum-forming method and apparatus for vacuum-forming fibre reinforced resin composites: pat. EP0525263B1; filed 01.08.91; publ. 27.03.96.
  17. Process for manufacturing resin-impregnated, reinforced articles without the presence of resin fumes: pat. US 4132755A; filed 22.07.77; publ. 02.01.79.
  18. High-performance infusion system for VARTM fabrication: pat. US6964561B2; filed 23.04.02; publ. 15.11.05.
  19. Takeda F., Hayashi K., Yasuo S. et al. Research in the application of the VaRTM technique to the fabrication of primary aircraft composite structures. Mitsubishi Heavy Industries Technical Review, 2005, no. 42. P. 1–6.
  20. Vacuum resin impregnation process: pat. US4942013A; filed 27.03.89; publ. 17.07.90.
  21. Jokhan O.M., Kostenko O.P. Methods for manufacturing parts from composite materials by impregnation in tooling. Part 2. Methods of vacuum impregnation. Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov, 2012, no. 1, pp. 80–92.
  22. Method of laminating reinforced plastics: pat. US3309450A; filed 05.07.61; publ. 14.03.67.
  23. Cole C. Guide for low cost design and manufacturing of composite general aviation aircraft, techreport. National Institute for Aviation Research, Wichita State University, 2001. 103 p.
  24. Loving D.A., Loving J., Sargent R., Sudduth R.D. Resin transfer molding involving center injection using a new production-oriented process for composites. ICCE6 Conference Proceedings. Orlando, 1999, pp. 513–514.
  25. Process for fiberglass molding using a vacuum: pat. US6508974B1; filed 15.02.96; publ. 21.03.03.
  26. Method of liquid resin infusion of a composite preform: pat. US20150102535A1; filed 11.10.13; publ. 16.04.15.
  27. Controlled atmospheric pressure resin infusion process: pat. EP1507647B1; filed 29.05.02; publ. 12.09.12.
  28. Plant molding fibre-reinforced plastic by injection under vacuum: pat. FR2771960A1; filed 09.12.97; publ. 11.06.99.
  29. Ricciardi M.R., Antonucci V., Durante M. et al. A new cost-saving vacuum infusion process for fiber-reinforced composites: pulsed infusion. Journal of Composite Materials, 2014, vol. 48 (11), pp. 365–373.
  30. A bagging blanket and method for forming a fibre reinforced resin composite component: pat. GB2316036A; filed 05.08.96; publ. 18.02.98.
  31. Alms J.B., Advani S.G., Glancey J.L. Liquid composite molding control methodologies using vacuum induced preform relaxation. Composites. Part A: Applied Science and Manufacturing, 2011, vol. 42 (1), pp. 57–65.
  32. Double bag vacuum infusion process: pat. US7413694B2; filed 07.12.99; publ. 19.08.08.
  33. How wings are made for the MS-21 aircraft. Available at: https://zen.yandex.ru/media/alexio_marziano/kak-delaiut-krylia-dlia-samoleta-ms21-5aa1849677d0e6cf2df9614a (accessed: April 10, 2022).
  34. A method for manufacturing fibrous composites by vacuum infusion and a device for implementing the method: pat. RU2480335C1. Rus. Federation; filed 07.02.12; publ. 27.04.13.