Kuzmina N.A., Ostroukhova G.A. Blockiness and substructure in single-crystal castings of nickel heat-resistant alloys // Proceedings of VIAM. 2022. No. 7 (113). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-7-13-26.

Blockiness and substructure in single-crystal castings of nickel heat-resistant alloys

Kuzmina N.A., Ostroukhova G.A.
Abstract

The paper defines two groups of defects characteristic of single crystals of NGC: substructure and blockiness. The most common causes of their occurrence are considered. The comparison of the main methods of substructure control: visual, swing and Laue and the results of determining the disorientation of the substructure by the method of swing relative to the longitudinal axis of the casting and the complete disorientation of the substructure determined by lauegrams is given. Based on the comparison, a conclusion is made about the limits of sensitivity during visual inspection of the structure.

Keywords
single crystal, crystallographic orientation, disorientation of subgrains, lauegram, x-ray diffraction, production technology of single crystal casting
Reference list
  1. Gerasimov V.V., Petrushin N.V., Visik E.M. Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy. Trudy VIAM, 2015, no. 3, paper no. 01. Available at: http://www.viam-works.ru (accessed: May 16, 2022). DOI: 10.18577/2307-6046-2015-0-3-1-1.
  2. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  3. Visik E.M., Tikhomirova E.A., Petrushin N.V., Ospennikova O.G., Gerasimov V.V., Zhivushkin A.A. Technological testing of a new heat-resistant alloy with low density during casting of single-crystal GTE blades. Metallurg, 2017, no. 2, pp. 80–86.
  4. Petrushin N.V., Elyutin E.S., Visik E.M., Golynets S.A. Development of single-crystal heat-resistant nickel alloy of the 5th generation. Metally, 2017, no. 6, pp. 38–51.
  5. Visik E.M., Gerasimov V.V., Petrushin N.V., Kolyadov E.V., Filonova E.V. Technological testing of casting of single-crystal blades from heat-resistant nickel alloy VZhL20 of low density. Liteyshchik Rossii, 2018, no. 5, pp. 17–21.
  6. Kablov E.N., Petrushin N.V., Sidorov V.V., Demonis I.M. Development of single-crystal high-rhenium heat-resistant nickel alloys by computer design. Aviacionnye materialy i tekhnologii, 2004, no. 1, pp. 22–36.
  7. Kolyadov EV, Visik EM, Gerasimov VV, Arginbaeva E.G. The influence of directional solidification parameters on the structure and properties of the intermetallic alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 16, 2022). DOI: 10.18577/2307-6046-2019-0-3-14-26.
  8. Petrushin N.V., Visik E.M., Gorbovets M.A., Nazarkin R.M. Structural-phase characteristics and mechanical properties of single crystals of heat-resistant nickel-rhenium-containing alloys with intermetallic-carbide hardening. Metally, 2016, no. 4, pp. 57–70.
  9. Ospennikova O.G., Rassokhina L.I., Bityutskaya O.N., Gamazina M.V. Optimization of technology for the manufacture of ceramic rods to improve the quality of cast blades of gas turbine engines. Novosti materialovedeniya. Nauka i tekhnika, 2017, no. 3–4 (27), paper no. 04. Available at: https://materialsnews.ru (accessed: May 13, 2022).
  10. Bondarenko Yu.A., Kablov E.N., Surova V.A., Echin A.B. Influence of high-gradient directional crystallization on the structure and properties of a rhenium-containing single-crystal alloy. Metallovedeniye i termicheskaya obrabotka metallov, 2006, no. 8 (614), pp. 33–35.
  11. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  12. Shalin R.E., Svetlov I.L., Kachanov E.B., Tolorayya V.N., Gavrilin O.S. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.
  13. Echin A.B., Bondarenko Yu.A. Structural features and properties of single-crystal Ni-based superalloy produced under conditions of variable temperature gradient on the solidification front. Trudy VIAM, 2015, no. 8, paper no. 01. Available at: http://www.viam-works.ru (accessed: May 13, 2022). DOI: 10.18577/2307-6046-2015-0-8-1-1.
  14. Bakradze M.M., Echin A.B. Calculation of temperature fields inside the casting by numerical method and using computer simulation. Tekhnologiya metallov, 2021, no. 6, pp. 31–38.
  15. Visik E.M., Kolyadov E.V., Ospennikova O.G., Gerasimov V.V., Filonova E.V. Influence of technological modes of casting on the structure of single-crystal blades from a carbon-free heat-resistant nickel alloy. Tekhnologiya metallov, 2018, no. 1, pp. 19–26.
  16. Kolyadov E.V., Gerasimov V.V., Visik E.M., Mezhin Yu.A. Casting by the method of directional crystallization with a controlled temperature gradient at the crystallization front. Liteynoe proizvodstvo, 2016, no. 8, pp. 24–26.
  17. Toloraya V.N., Nekrasov S.N., Ostroukhova G.A. Comparative analysis of the structure and properties of castings from heat-resistant alloys obtained on installations such as UVNK and PMP. Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 5–6 (31). paper no. 01. Available at: https://materialsnews.ru (accessed: May 13, 2022).
  18. Kolyadov E.V., Gerasimov V.V., Visik E.M. Influence of axial and radial temperature gradients at the crystallization front on the macro- and microstructure of ZhS32 alloy. Liteynoe proizvodstvo, 2014, no. 6, pp. 28–31.
  19. Visik E.M., Gerasimov V.V., Kolyadov E.V., Kuzmina N.A. Influence of technological modes of casting on the structure parameters of monocrystals of new heat-resistant alloys. Metallurgiya mashinostroeniya, 2016, no. 5, pp. 27–31.
  20. Kuzmina N.A., Petrushin N.V., Visik E.M., Eremin N.N., Naprienko S.A. Application of the Laue method to study the structure of a nickel heat-resistant alloy sample destroyed during mechanical processing. Trudy VIAM, 2020, no. 10 (92), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 13, 2022). DOI: 10.18577/2307-6046-2020-0-10-3-12.
  21. Tolorajya V.N., Filonova E.V., Chubarova E.N. i dr. Research of influence of HIP on microporosity in single-crystal casting of carbon-free hot strength alloys. Aviacionnye materialy i tehnologii, 2011, no. 1, pp. 20–26.
  22. Kablov E.N., Tolorayya V.N., Ostroukhova G.A., Aleshin I.N. Investigation of growth defects of the banding type in single-crystal castings from carbon-free heat-resistant alloys. Dvigatel, 2010, no. 6 (72). pp. 14–16.
  23. Kolyadov E.V., Gerasimov V.V., Visik E.M. About specific defects of castings after directional crystallization. Liteynoe proizvodstvo, 2015, no. 7, pp. 11–13.
  24. Sinichkina T.S., Belikov A.V., Visik E.M. The problem of burn formation on castings from ZhS-32 alloy. Liteynoe proizvodstvo, 2015, no. 2, pp. 18–20.
  25. Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 12, 2022). DOI: 10.18577/2307-6046-2019-0-12-11-19.
  26. Khayutin S.G. On misorientation of grains during directional crystallization. Metallovedeniye i termicheskaya obrabotka metallov, 2007, no. 6, pp. 42–43.
  27. Sidokhin E.F., Sidokhin F.A., Khayutin S.G. On the substructure of single-crystal GTE blades. Aviatsionnaya promyshlennost, 2009, no. 1, pp. 34–36.
  28. Sidokhin F.A., Sidokhin A.F., Sidokhin E.F. On the determination of the crystallographic orientation of single crystals by the Laue method. Zavodskaya laboratoriya. Diagnostika materialov, 2009, vol. 75, no. 1, pp. 35–37.
  29. Potrakhov N.N., Khayutin S.G., Lifshits V.A., Oses R. PRDU-KROS setup for express determination of the crystallographic orientation of cubic single crystals from inverse Laue patterns. Zavodskaya laboratoriya. Diagnostika materialov, 2015, vol. 81, no. 8, pp. 27–30.
  30. Oses R., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. The program for deciphering the inverse Laue patterns of FCC single crystals to determine the crystallographic orientation of samples (CGO analysis): certificate. about State Reg. Computer programs, no. 201164448. 2011.
  31. Kuzmina N.A., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Comparative structure control of single-crystal castings of nickel superalloys x-ray diffraction methods of oscillation and Laue. Trudy VIAM, 2019, no. 9 (81), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 13, 2022). DOI: 10.18577/2307-6046-2019-0-9-15-25.