Lomberg B.S., Akhmedzyanov M.V., Chabina E.B., Rastorgueva O.I. Heat-resistant wrought superalloy for high-pressure compressor blades of promising gas turbine engines // Proceedings of VIAM. 2022. No. 6 (112). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-6-5-14.

Heat-resistant wrought superalloy for high-pressure compressor blades of promising gas turbine engines

Lomberg B.S., Akhmedzyanov M.V., Chabina E.B., Rastorgueva O.I.
Abstract

A wrought heat-resistant superalloy VZh179-ID has been developed for blades of the last stages of a high-pressure compressor with an operating temperature up to 800 °С of high-thrust gas turbine engines. To achieve the required indicators for mechanical properties structural studies have been carried out, the results of which are used in determining the models of alloy’s heat treatment. According to the complex of mechanical properties the developed alloy has significant quotes of superiority both in comparison with EP718-ID alloy and the most heat-resistant wrought alloy for blades EP220.

Keywords
heat-resistant wrought superalloy, technology, bar, structure, thermal treatment, high-pressure compressor
Reference list
  1. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8. pp. 54–58.
  2. Inozemtsev A.A. Materials and technologies for the PD-14 engine. Proceedings of International Scientific and Technical Conference "New materials and technologies for deep processing of raw materials – the basis for the innovative development of the Russian economy". Moscow: VIAM, 2012, art. 16, 1 CD-ROM.
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  4. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577 / 2071-9140-2019-0-2-3-11.
  5. Lomberg B.S., Chudareva L.T., Seryogina N.I. Influence of the structure of the EP975-ID alloy on the properties of large-sized forgings. Aviatsionnye materialy, 1984, no. 3, pp. 9–17.
  6. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  7. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  8. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Heat-resistant wrought nickel-based alloy and product made from it: pat. 2737835 Rus. Federation, no. 2020118382; filed. 03.06.20; publ. 03.12.20.
  10. Gorbovets M.A., Slavin A.V. Proof of material compliance with the requirements to part No. 33 of JARs. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 89–94. DOI: 10.18577/2071-9140-2018-0-3-89-94.
  11. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DO1: 10.18577/2071-9140-2020-0-4-59-70.
  12. Gorelik S.S. Recrystallization of metals and alloys. Moscow: Metallurgiya, 1978, 568 p.
  13. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2018. Vol. 2: Deformable heat-resistant steels and alloys. Alloys based on refractory metals, 248 p.
  14. INCONEL® alloy 718. Available at: http://www.specialmetals.com/documents/technical-bulletins/inconel (accessed at: January 24, 2022).
  15. Khodinev I.A., Monin S.A., Ryzhkov P.V. Investigation of the growth rate of a fatigue crack in heat-resistant nickel alloys. Voprosy materialovedeniya, 2020, no. 4 (104), pp. 48–63. DOI: 10.22349/1994-6716-2020-104-4-48-63.