UDC
620.1:669.245
DOI
10.18577/2307-6046-2022-0-5-123-137
Article PDF (Russian)
(1.03 MB)
How to cite
Gorbovets M.A., Khodinev I.A., Karashaev M.M., Ryzhkov P.V. Low cycle dwell fatigue testing of heat resistant metallic materials (review) // Proceedings of VIAM. 2022. No. 5 (111). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-5-123-137.
Low cycle dwell fatigue testing of heat resistant metallic materials (review)
Abstract
A review of the methods for testing dwell low-cycle fatigue is carried out and the results of tests of nickel heat-resistant alloys and steels are presented. The description of models for calculating damage in the interaction of fatigue and creep is presented. The requirements for specimens, equipment and test results for metallic materials are analyzed. The fractographic features of fracture due to high-temperature dwell fatigue of heat-resistant nickel alloys and steels are considered.
Keywords
mechanical properties, fatigue, high-temperature nickel alloys, irregular loading, damage accumulation, cyclic durability
Reference list
- Kablov E.N., Golubovsky E.R. Heat resistance of nickel alloys. Moscow: Mashinostroenie, 1998, 464 p.
- Inozemtsev A.A., Nikhhamkin M.A., Sandratsky V.L. Gas turbine engines. Moscow: Mashinostroenie, 2007, 204 p.
- Kogaev V.P. Calculations for strength at stresses that are variable in time. Moscow: Mashinostroenie, 1993, 364 p.
- Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14). pp. 16–21.
- Makhutov N.A. Strength and safety. Fundamental and applied research. Novosibirsk: Nauka, 2008, 528 p.
- Sulak I., Obrtlík K. Effect of tensile dwell on high-temperature low-cycle fatigue and fracture behavior of cast superalloy MAR-M247. Engineering Fracture Mechanics, 2017, vol. 185, pp. 92–100. DOI: 10.1016/j.engfracmech.2017.04.002.
- Sun L., Bao X.-G., Guo S.-G. et al. The creep-fatigue behavior of a nickel-based superalloy: Experiments study and cyclic plastic analysis. International Journal of Fatigue, 2021, vol. 147. DOI: 10.1016/j.ijfatigue.2021.106187.
- Goswami T., Hanninen H. Dwell effects on high temperature fatigue behavior. Part I. Materials and Design, 2001, vol. 22, is. 3, pp. 199–215.
- Bukaty S.A., Okrugin A.A. Study of the cyclic durability of the material under conditions of low-cycle fatigue and long-term strength. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2014, no. 5 (47), part 4, pp. 142–150.
- Manson S.S., Halford G.R., Hirschberg M.H. Creep-fatigue analysis by strain-range partitioning. Technical paper. National Pressure Vessel and Piping Conference. San Francisco, 1971, pp. 1–17.
- Inozemtsev A.A., Ratchiev A.M., Nikhamkin M.Sh. Low-cycle fatigue and cyclic crack resistance of a nickel alloy under loading characteristic of turbine disks. Tyazheloe mashinostroenie, 2011, no. 4, pp. 30–33.
- ASTM E2714-13. Standard Test Method for Creep-Fatigue Testing. ASTM International, 2020. DOI: 10.15.20/E2714-13R13.
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Elsevier Publishing Resource Database. Available at: https://www.sciencedirect.com (accessed: October 20, 2021).
- National Aeronautics and Space Administration (NASA) Technical Reports Database. Available at: https://ntrs.nasa.gov (accessed: October 20, 2021).
- Database of RSCI resources. Available at: https://www.elibrary.ru (accessed: October 20, 2021).
- Manson S.S., Halford G.R. Fatigue and Durability of Structural Materials. ASM International, 2006. 456 p.
- Morishita M., Asada Y., Ispikawa A. An Evaluation of Creep-Fatigue of 304 Stainless Steel in Very Vacuum Environment. Bulletin of ASME, 1985, vol. 6, no. 235, pp. 7–12.
- Miller D.A., Priest R.H., Ellison E.G. A Review of Material response and life prediction techniques under fatigue creep loading conditions. Journal of High Temperature and Process, 1984, vol. 6, no. 3, 4, pp. 155–194.
- Belyaev M.S., Khvatskiy K.K., Gorbovets M.A. Comparative analysis of national standards of RF and the USA on methods of metals fatigue testing. Trudy VIAM, 2014, no. 9, paper no. 11. Available at: http://www.viam-works.ru (accessed: November 21, 2021). DOI: 10.18577/2307-6046-2014-0-9-11-11.
- Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DO1: 10.18577/2071-9140-2020-0-4-59-70.
- Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021. no. 1 (62). paper no. 08. Available at: http://www.journal.viam.ru (accessed: December 12, 2021). DOI: 10.18577/2071-9140-2021-0-1-80-94.
- Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: November 3, 2020). DOI: 10.18577/2307-6046-2018-0-9-51-60.
- Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Strength tests and researches of aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
- Carroll L.J., Cabet C., Carroll M.C., Wright R.N. The development of microstructural damage during high temperature creep – fatigue of a nickel alloy. International Journal of Fatigue, 2013, vol. 47, pp. 115–125. DOI: 10.1016/j.ijfatigue.2012.07.016.