Kuznetsova V.A., Silaeva A.A., Zheleznyak V.G., Marchenko S.A. Modification of epoxy film-forming and the hardeners for coatings (review) // Proceedings of VIAM. 2022. No. 5 (111). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-5-96-111.

Modification of epoxy film-forming and the hardeners for coatings (review)

Kuznetsova V.A., Silaeva A.A., Zheleznyak V.G., Marchenko S.A.
Abstract

In this work the analysis of experience of application of different approaches for achievement of necessary characteristics of coatings on the basis of epoxy film-forming at the expense of component modification of film-forming system is carried out. Ways of modification of hardeners for epoxy film-forming and epoxy resins are considered, influence of modifying agents on properties of coatings is described. The great attention is given in particular to amine hardeners, as to the most widespread hardeners of epoxies. Among modifiers of epoxy oligomers for receiving coatings uretan-containing, organic silicon oligomer products and rubbers are allocated.

Keywords
epoxy top coat, hardener, modifying agent, coating system, adhesion, physical mechanical properties, electroisolating coatings, chemical resistant
Reference list
  1. Chebotarevsky V.V., Kondrashov E.K. Technology of paints and varnishes in mechanical engineering. Moscow: Mashinostroenie, 1978, 295 p.
  2. Yakovlev A.D. Chemistry and technology of paint coatings. St. Petersburg: Khimizdat, 2010, 445 p.
  3. Kondrashov E.K. Paint and varnish materials and coatings based on them in mechanical engineering. Moscow: Paint-Media, 2021, 255 p.
  4. Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  5. Kablov E.N. Chemistry in Aviation Materials Science. Russian Journal of General Chemistry, 2011, vol. 81, no. 5, pp. 967–969.
  6. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. The main directions of improving the operational properties, technological and environmental characteristics of paint coatings for aviation equipment. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96–102.
  7. Eselev A.D., Bobylev V.A. Epoxy resins and hardeners for the production of paints and varnishes. Paints and varnishes and their application, 2005, no. 10, pp. 16–25.
  8. Moshinsky L.Ya. Epoxy resins and hardeners. Tel Aviv: Arkadia Press Ltd, 1995, pp. 40–142.
  9. Filichkina V.N. Modern state and trends in the development of production and consumption of epoxy resins. Chemical industry abroad. Moscow: NIITEKhIM, 1988, is. 8, 18 p.
  10. Kochnova Z.A., Zhavoronok E.S., Chalykh A.E. Epoxy resins and hardeners: industrial products. Moscow: Paint media, 2006, 200 p.
  11. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  12. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: October 17, 2021). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  13. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Paint and varnish materials and coatings. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 315–327.
  14. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  15. Problems of protective paints and varnish coatings. Review of materials of the European conference "Protective coatings" (Protective coating), Düsseldorf. Lakokrasochnye materialy i ikh primenenie, 2013, no. 9, pp. 33–35.
  16. Eselev A.D., Bobylev V.A. Epoxy resins: yesterday, today, tomorrow. Lakokrasochnaya promyshlennost, 2009, no. 9, pp. 15–17.
  17. Shakhmaliev A.M., Ying Shen Kang, Bilalov Ya.M. et al. Modification of an epoxy oligomer with a reactive oligomer. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 7–9.
  18. Amosova Z.V. Synthesis and study of epoxy oligomers and polymers. Moscow: NIITEKhIM, 1979, 97 p.
  19. Moshinsky L.Ya., Belaya E.S. Epoxy resin hardeners. Moscow: NIITEKhIM, 1983, 62 p.
  20. Katnov V.E., Stepin S.N. Influence of the hardener on the properties of epoxy coatings. Proceedings of the scientific session of Kazan State Technical University. Kazan, 2009, p. 25.
  21. Smekhov F.M., Kardash N.S., Shode L.V. et al. Properties of epoxy coatings with various amine-type hardeners. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 9–11.
  22. Finkelstein M.I. Industrial application of epoxy paints and varnishes. Leningrad: Khimiya, 1983, 120 p.
  23. Epoxy resin hardeners: review inform. Moscow: NIITEKHIM, 1976, 47 p.
  24. Sorokin M.V., Kochnova Z.A., Shode L.G. Chemistry and technology of film-forming substances. Moscow: Khimiya, 1989, 477 p.
  25. Mirer E.V., Shode L.G., Tartakovskaya A.M., Kuzina S.I. Heterophase hydrolysis of ketimine adducts of epoxy oligomers. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 9–11.
  26. Smekhov F.M., Kardash N.S., Shode L.G. et al. Properties of epoxy coatings with various amine-type hardeners. Lakokrasochnye materialy i ikh primenenie, 1989, no. 5, pp. 36–39.
  27. Sorokin M.F., Onosova L.A., Tarasov A.V., Shode L.G. Epoxy materials based on modified amine hardeners. Lakokrasochnye materialy i ikh primeneniye, 1988, no. 3, pp. 4–6.
  28. Vedyakin S.V., Shode L.G., Smekhov G.M., Zeitlin G.M. Modification of epoxyamine systems with organosilicon epoxyurethanes. Lakokrasochnye materialy i ikh primenenie, 1991, no. 2, pp. 1–3.
  29. Aleksashina O.F., Molotov I.Yu., Shigorin V.G. et al. Properties of epoxy-ketimine coatings and experience with the use of KI-1 hardener. Lakokrasochnye materialy i ikh primenenie, 1990, no. 5, pp. 13–16.
  30. Shode L.G., Sinitsina O.V., Voloshchuk K.A. Peculiarities of curing epoxy coatings with blocked hardeners (ketimines). Lakokrasochnye materialy i ikh primenenie, 1989, no. 6, pp. 9–12.
  31. Shode L.G., Dudina L.V., Miroshnik V.M. Hardeners for epoxy oligomers of the EPAM type. Lakokrasochnye materialy i ikh primenenie, 1989, no. 5, pp. 16–19.
  32. Sorokin M.F., Shode L.G., Dudina L.V. etc. New hardeners of epoxy oligomers based on epoxy oligomers and ammonia. Lakokrasochnye materialy i ikh primenenie, 1989, no. 2, pp. 13–15.
  33. Shode L.G., Smekhov F.M., Kuzina S.I. Modified polyethylenepolyamines as hardeners for epoxy oligomers. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 4–6.
  34. Sorokin M.F., Kochnova Z.A., Zakharova A.A., Golova N.A. Curing of epoxy oligomers with aminoalkoxysilanes. Lakokrasochnye materialy i ikh primenenie, 1986, no. 5, pp. 19–20.
  35. Kochnova Z.A., Belyaev A.V., Zeitlin G.M. Curing of epoxy oligomers with the participation of aminopropyltriethoxysilanes. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 24–27.
  36. Akopova T.A., Ponomarenko O.P., Olikhova Yu.V., Osipchik V.S. Study of the effect of organosilicon modifiers on the properties of epoxy-containing binders. Uspekhi khimii i khimicheskoy tekhnologii, 2012, vol. XXVI, no. 3 (32), pp. 70–72.
  37. Arvan A.S., Kovalenko V.M., Sheshukov A.V., Shreiner S.A. Improving the properties of epoxy coatings by curing them with amino esters. Lakokrasochnye materialy i ikh primenenie, 1974, no. 4, pp. 53–54.
  38. Sukhareva L.A., Mironova T.A., Fedyakova N.V. et al. Properties and structure of modified epoxy-polyamine coatings. Lakokrasochnye materialy i ikh primenenie, 1989, no. 5, pp. 50–52.
  39. Zhavoronok E.S., Senchikhin I.N., Kolesnikova E.F. Peculiarities of curing mixtures of dianoic and aliphatic epoxy oligomers with different reactivity. Vysokomolekulyarnye soyedineniya. Series B, 2010, vol. 52, no. 4, pp. 706–714.
  40. Petrova I.A., Kobozeva I.A., Savrasova E.M. The mechanism of curing epoxy oligomers by aluminum chelates in thin films. Lakokrasochnye materialy i ikh primenenie, 1990, no. 1, pp. 30–33.
  41. Kirillov A.N., Garipov R.M., Deberdeev R.Ya. Application of organoelement epoxyurethane oligomers for modification of epoxyamine coatings. VIII Intern. conf. on chemistry and physicochemistry of oligomers "Oligomers-2002". Chernogolovka, 2002, p. 248.
  42. Kochnova Z.A., Shode L.G. Hardeners for epoxy film formers. Lakokrasochnye materialy i ikh primenenie, 1995, no. 3–4, pp. 42–47.
  43. Mostovoy A.S., Panova L.G. Investigation of the possibility of using low molecular weight polyamide grade PO-300 as a "cold" curing hardener for epoxy oligomers. Plasticheskiye massy, 2016, no. 1–2, pp. 16–18.
  44. Kondrashov E.K., Vladimirsky V.N., Beider E.Ya. Erosion resistant coatings. Moscow: Khimiya, 1989, 135 p.
  45. Shibalovich V.V., Yakovlev A.D. The use of amino acid hardeners in epoxy paint and varnish compositions. Lakokrasochnye materialy i ikh primenenie, 1979, no. 5, pp. 30–32.
  46. Mikheev V.V., Ivanova R.R. Curing of epoxy oligomers by urethane-containing polyamines. Lakokrasochnye materialy i ikh primenenie, 2003, no. 12, pp. 8–11.
  47. Logunov G.I., Nikolaev V.N. Epoxy oligomers cured with oligourethane acrylate and oligouretananallylate. Lakokrasochnye materialy i ikh primenenie, 1982, no. 3, pp. 19–20.
  48. Kirillov A.N., Sof’ina S.Yu., Garipov R.M., Deberdeev R.Ya. Modification of epoxyamine compositions with epoxyurethane oligomers. Lakokrasochnye materialy i ikh primenenie, 2003, no. 4, pp. 25–28.
  49. Kirillov A.N., Garipov R.M., Deberdeev R.Ya. Influence of epoxyurethane modifiers on the properties of epoxy lacquer coatings. IX All-Rus. conf. "Structure and dynamics of molecular systems". Yoshkar-Ola, 2002, pp. 236–239.
  50. Prilutskaya N.V., Smekhov F.M., Shuster S.V. Modification of epoxy compositions with epoxy esters for coatings. Lakokrasochnye materialy i ikh primenenie, 1985, no. 1, pp. 30–32.
  51. Lipson G.Ya. Colloidal-chemical properties of heterogeneous systems based on epoxy oligomer and reactive modifiers: thesis abstract, Cand. Sc. (Tech.). Moscow, 1985, pp. 13–18.
  52. Mochalova E.N. Formation of the structure and properties of epoxyamine compositions in the presence of reactive and inert modifiers: thesis abstract, Cand Sc. (Tech.). Moscow, 1999, 15 p.
  53. Parshina M.S., Soldatov M.A., Makarova V.A. Influence of the chemical structure of organofluorine copolymer modifiers on the moisture resistance of amine-cured epoxy resin. Lakokrasochnye materialy i ikh primenenie, 2018, no. 3, pp. 15–19.
  54. Kurbatov V.G., Ilyin A.A., Indeikin E.A. Influence of polyaniline additive on the physical and mechanical properties of epoxy coatings. Lakokrasochnye materialy i ikh primenenie, 2011, no. 1–2, pp. 49–51.
  55. Snopkov A.Yu., Glezer E.A., Yakovlev A.D. Coatings based on epoxy resins modified with rubber. Lakokrasochnye materialy i ikh primenenie, 1989, no. 3, pp. 66–71.
  56. Ternovykh A.M. Development and study of protective polymer coatings based on epoxy and rubber oligomers with increased adhesive resistance: thesis abstract, Cand. Sc. (Tech.). Moscow, 1985, pp. 3–15.
  57. Kablov V.F. System technology rubber-oligomeric compositions. X Int. conf. on chemistry and physicochemistry of polymers. Volgograd: Volgograd State Tech. University, 2009, pp. 162–19.
  58. Chalykh A.E., Zhavoronok E.S., Kochnova Z.A., Kiselev M.R. Structure formation in binary mixtures of carboxyl-containing rubber–epoxy oligomer. Khimicheskaya fizika, 2009, vol. 28, no. 6, pp. 91–96.
  59. Kochnova Z.A., Zhavoronok E.S., Kotova A.V. Features of obtaining epoxy-rubber compositions based on liquid butadiene-nitrile rubbers and epoxy oligomers. Lakokrasochnye materialy i ikh primenenie, 1998, no. 11, pp. 27–28.
  60. Kuznetsova V.А., Zheleznyak V.G., Kurshev E.V., Yemelyanov V.V. Research of fuel- and water resistance of coatings based on the filled epoxy-thiokol polymeric compositions. Aviation materials and technologies, 2021, no. 2 (63), paper no. 10. Available at: http://www.journal.viam.ru (accessed: June 24, 2021). DOI: 10.18577/2713-0193-2021-0-2-93-102.
  61. Zhavoronok E.S. Multicomponent polymer networks based on epoxy oligomers with active polyfunctional groups: thesis abstract, Dr. Sc. (Chem.). Moscow, 2019, pp. 35–39.
  62. Composition for protective coating: pat. 2290421 Rus. Federation, no. 2005124341/04; filed 01.08.05; publ. 27.12.06.
  63. Composition for protective coating of polymer composite materials: pat. 2480499 Rus. Federation, no. 2011127312/05; filed 04.07.11; publ. 27.04.13.
  64. Storozhuk I.P., Pavlyukovich N.G. Modified thiokol compositions and their use as waterproofing and protective paintwork materials. Lakokrasochnye materialy i ikh primenenie, 2017, no. 5, pp. 29–33.
  65. Chalykh A.E., Kochnova Z.A., Zhavoronok E.S. Compatibility and diffusion in the systems epoxy oligomers–liquid carboxylate rubbers. Vysokomolekulyarnye soyedineniya. Ser. A. 2001, vol. 43, no. 12, pp. 1–9.
  66. Van Ngan N., Kostromina N.V., Osipchik V.S. et al. Polysiloxane-containing epoxyurethane oligomers and coatings based on them. Plasticheskiye massy, 2019, no. 3–4, pp. 3–6.
  67. Kuznetsova V.A. Erosion-resistant composition based on the three-phase polymer system "epoxy oligomer-rubber-reinforcing filler": thesis abstract, Cand. Sc. (Tech.). Moscow, 1999, 24 p.
  68. Strekachinskaya L.S., Verkholantsev V.V., Grozinskaya Z.P. Patterns of stratification of solutions of polymer mixtures. Lakokrasochnye materialy i ikh primenenie, 1980, no. 4, pp. 13–15.
  69. Grozinskaya Z.P., Strekachinskaya L.S., Verkholantsev V.V. Improvement of some characteristics of coatings due to delamination of the film former. Lakokrasochnye materialy i ikh primenenie, 1979, no. 5, pp. 30–32.
  70. Shleomenzon Yu.B., Morozova I.I., Pavlova V.P. et al. Structure of epoxy-rubber composition. Lakokrasochnye materialy i ikh primenenie, 1979, no. 2, pp. 8–10.
  71. Kuznetsova V.А. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.
  72. Kuznetsova V.A., Deev I.S., Semenova L.V. Influence of modification of epoxy film-forming compositions on their phase microstructure and adgesion to aluminium alloy. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 72–78. DOI: 10.18577/2071-9140-2016-0-1-72-78.
  73. Yakovlev A.D., Yakovlev S.A. Paint and varnish functional coatings. St. Petersburg: Khimizdat, 2016, 265 p.