Khudnev A.A., Batienkov R.V., Bolshakova A.N., Dvoretskov R.M. Study of the features of compaction of powder composite materials based on molybdenum using spark plasma sintering // Proceedings of VIAM. 2022. No. 3 (109). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-3-64-74.

Study of the features of compaction of powder composite materials based on molybdenum using spark plasma sintering

Khudnev A.A., Batienkov R.V., Bolshakova A.N., Dvoretskov R.M.
Abstract

Composite dispersion-strengthened materials of the Mo–Ti–Zr–C and Mo–Hf–C systems were investigated in this work. Samples were obtained by powder metallurgy methods using mechanical alloying with subsequent compaction of as-received powder by a spark plasma sintering. It was found that the main strengthening phase in the obtained material of the Mo–Ti–Zr–C system is molybdenum oxide with titanium, zirconium and molybdenum dissolved in it. The material of the Mo–Hf–C system contains two types of reinforcing phase: molybdenum oxides and hafnium oxides. An increase in the sintering temperature by 200 °C did not lead to an increase in the density of materials, but led to the growth of grains and a carbide layer on the surface of the samples.

Keywords
spark plasma sintering, mechanical alloying, molybdenum, dispersion-strengthened composite material, powder metallurgy, microstructural analysis
Reference list
  1. Kablov E.N., Svetlov I.L., Neiman A.V., Min P.G., Karachevtsev F.N., Karpov M.I. High-temperature composites based on the Nb–Si system reinforced with niobium silicides. Inorganic Materials: Applied Research, 2017, vol. 8, no. 4, pp. 609–617.
  2. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  3. Kablov E.N., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A., Narsky A.R. Prospects for the creation of high-temperature heat-resistant alloys based on refractory matrices and natural composites. Voprosy materialovedeniya, 2020, no. 4, pp. 64–78.
  4. Lebedeva Yu.E., Afanasev-Hodikin A.N., Prokopchenko G.M., Shavnev A.A., Serebryakov D.I. Obtaining of experimental constructionally similar sample of the nozzle assembly sector and carrying out its tests at temperature of 1500 °С. Trudy VIAM, 2020, no. 10 (92), paper no. 06. Available at: http://www.viam-works.ru (accessed: September 10, 2021). DOI: 10.18577/2307-6046-2020-0-10-51-62.
  5. Fan J., Lu M., Cheng H. et al. Effect of alloying elements Ti, Zr on the property and microstructure of molybdenum. International Journal of Refractory Metals and Hard Materials, 2009, vol. 27, no. 1, pp. 78–82. DOI: 10.1016/j.ijrmhm.2008.03.006.
  6. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Refractory alloys for innovative equipment. Trudy VIAM, 2016, no. 10, paper no. 5. Available at: http://www.viam-works.ru (accessed: August 25, 2021). DOI: 10.18577/2307-6046-2016-0-10-5-5.
  7. Kucher A.M. Metal technology. 4th ed., rev. and add. Leningrad: Mashinostroenie, 1987, 214 p.
  8. Kapustin V.I., Korzhaviy A.P. Drift spectrometry: traditional methods and development prospects. Rossiyskiy tekhnologicheskiy zhurnal, 2016, vol. 4, no. 2, pp. 3–24.
  9. Ohser-Wiedemann R., Weck C., Martin U. et al. Spark plasma sintering of TiC particlereinforced molybdenum composites. International Journal of Refractory Metals and Hard Material, 2012, vol. 32, pp. 1–6. DOI:10.1016/j.ijrmhm.2011.12.001.
  10. Yavas B., Goller G. Investigation the effect of B4C addition on properties of TZM alloy prepared by spark plasma sintering. International Journal of Refractory Metals and Hard Materials, 2016, vol. 58, pp. 182–188. DOI: 10.1016/j.ijrmhm.2016.04.020.
  11. Majumdar S., Sharma I.G., Raveendra S. et al. In situ chemical vapour co-deposition of Al and Si to form diffusion coatings on TZM. Materials Science and Engineering: A, 2008, vol. 492, no. 1–2, pp. 211–217. DOI: 10.1016/j.msea.2008.03.020.
  12. Nagae M., Yoshio T., Takada J., Hiraoka Y. Improvement in recrystallization temperature and mechanical properties of a commercial TZM alloy through microstructure control by multi-step internal nitriding. Materials transactions, 2005, vol. 46, no. 10, pp. 2129–2134. DOI: 10.2320/matertrans.46.2129.
  13. Mazalov I.S., Mazalov P.B., Suhov D.I., Sulyanova E.A. Influence of hot isostatic pressing parameters on structure and properties of cobalt-based alloys obtained by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 01. Available at: http://www.journal.viam.ru (accessed: August 25, 2021). DOI: 10.18577/2713-0193-2021-0-2-3-14.
  14. Majumdar S., Sharma I.G. Development of Mo base TZM (Mo–0.5Ti–0.1Zr–0.02C) alloy and its shapes. BARC Newsletter, 2010, vol. 312, pp. 21–27.
  15. Sharma I.G., Chakraborty S.P., Suri A.K. Preparation of TZM alloy by aluminothermic smelting and its characterization. Journal of Alloys and Compounds, 2005, vol. 393, no. 1–2, pp. 122–127.
  16. Yavas B., Sahin F., Yucel O., Goller G. Preparation of Pre-Alloyed TZM Alloy with Addition of B4C by Using Spark Plasma Sintering. 6th International Conference on Materials Science and Technologies, 2016, pp. 75–76.
  17. Efimochkin I.Yu., Kuzmina N.A., Grashchenkov D.V., Svetlov I.L., Bobrovsky A.P. Niobium silicide synthesis by spark plasma sintering of composite powders. Trudy VIAM, 2018, no. 11 (71), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 25, 2021). DOI: 10.18577/2307-6046-2018-0-11-35-44.
  18. Torrecillas S.M.R., Solis P.N., Okunkova A.A., Peretyagin P.Yu. Fundamentals of spark plasma sintering of nanopowders. Moscow: Technosfera, 2014, 96 p.
  19. Akin I., Hotta M., Sahin F.C. et al. Microstructure and densification of ZrB2–SiC composites prepared by spark plasma sintering. Journal of the European Ceramic Society, 2009, vol. 29, no. 11, pp. 2379–2385.
  20. Morgunova N.N., Klypin B.A., Boyarshinov V.A. еt al. Alloys of molybdenum. Moscow: Metallurgy, 1975. 392 p.
  21. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu. Development of powder metallurgy of heat-resistant materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 6, pp. 10–22.
  22. Batienkov R.V., Bolshakova A.N., Khudnev A.A., Kuznetsov B.Yu. Investigation of mechanical alloying of powder materials of the Mo–Ti–Zr–C and Mo–Hf–C systems. Metallurg, 2020, no. 11, pp. 93–99.
  23. Dudina D.V. Electrospark sintering of mixtures of metal powders and composites with metal matrices: peculiarities of structure formation and properties of sintered materials. Obrabotka metallov (tekhnologiya, oborudovaniye, instrumenty), 2017, no. 2, pp. 45–54. DOI: 10.17212/1994-6309-2017-2-45-54.