Veligodsky I.M., Koval T.V., Kurnosov A.O., Marachovskiy P.C. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions // Proceedings of VIAM. 2022. No. 11 (117). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-11-134-148.

Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions

Veligodsky I.M., Koval T.V., Kurnosov A.O., Marachovskiy P.C.
Abstract

Because of limited resistance of glass fiber reinforced plastic (GFRP) to influence of climatic factors it is interesting to make natural weathering tests in different climatic conditions. The study of strength and thermomechanical properties changing of GFRP VPS-48/7781 (with or without coating) after 3 year environmental exposure in different climatic zones. It was shown that applying of coating based on VE-69 provides saving strength and thermomechanical properties on the initial level.

Keywords
natural climatic tests, GFRP VPS-48/7781, flexural strength, compressive strength, dynamic mechanical analysis
Reference list
  1. Doriomedov M.S. Russian and world market of polymer composites (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 04. Available at: http://www.viam-works.ru (accessed: June 29, 2022). DOI: 10.18577/2307-6046-2020-67-29-37.
  2. Tkachuk A.I., Gurevich Ya.M., Guseva M.A., Mishurov K.S. Technological and operational characteristics and applications of the epoxy binder VSE-1212, processed by prepreg technology. Klei. Germetiki. Tekhnologii, 2018, no. 4, pp. 29–34.
  3. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
  4. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: June 29, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  5. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes.
  6. I. Evaluation of the influence of significant factors of influence. Deformatsiya i razrushenie materialov, 2019, no. 12, pp. 7–16. DOI: 10.31044/1814-4632-2019-12-7-16.
  7. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of methods for studying the early stages of aging. Deformatsiya i razrushenie materialov, 2020, no. 1, pp. 15–21. DOI: 10.31044/1814-4632-2020-1-15-21.
  8. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016. no. 6, paper no. 11. Available at: http://www.viam-works.ru (accessed: June 29, 2022). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  9. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  10. Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Investigation of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9. DOI: 10.31044/1994-6260-2020-0-3-2-9.
  11. Osadchiy N.V., Malyshev V.A., Shepel V.T. Investigation of the deformation of a five-layer beam with a shear-compliant filler under concentrated force loading. Deformatsiya i razrusheniye materialov, 2018, no. 7, pp. 11–16.
  12. Raskutin A.E. Structural carbon plastics based on new melt-type binders and Porcher fabrics. Novosti materialovedeniya. Nauka i tekhnika, 2013, no. 5, art. 01. Available at: http://materialsnews.ru (date of access: 07/08/2022).
  13. Gulyaev A.I., Yakovlev N.O., Krylov V.D., Shurtakov S.V. Fracture micromechanics of glass-reinforced plastics during delamination by modes I and II. Materialovedenie, 2016, no. 2, pp. 13–22.
  14. Gulyaev A.I., Yakovlev N.O., Krylov V.D., Lashov O.A. Application of fractographic analysis in the study of interlayer fracture of PCM. Aviaсionnye materialy i tehnologii, 2017, no. 3 (48), pp. 65–73. DOI: 10.18577/2071-9140-2017-0-3-65-73.
  15. Semyonova L.V., Nefyodov N.I. Recovery technology for PWC systems with polyurethane enamel for the operating aviation articles after wornout PLC removal. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 47–50. DOI: 10.18577/2071-9140-2014-0-s3-47-50.
  16. Nefedov N.I. Issues of import substitution in the paint and varnish industry. All materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2015, no. 8, pp. 25–28.
  17. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solvent-free binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 29, 2022). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  18. Vavilova M.I., Sokolov I.I., Akhmadieva K.R., Yamschikova G.A. Polymer composite materials with low porosity obtained by the technology of impregnation with a film binder. Voprosy materialovedeniya, 2017, no. 1 (89), pp. 140–146. DOI: 10.22349/1994-6716-2017-89-1-140-146.
  19. Lobanov D.S., Zubova E.M. Influence of temperature aging on the mechanical behavior of structural fiberglass during interlaminar shear.Works of XXXI Intern. innovative conf. young scientists and students on problems of mechanical engineering. Moscow: Blagonravov Institute of Mechanical Engineering of RAS, 2020, pp. 779–782.
  20. Nikolaev E.V., Pavlov M.R., Andreeva N.P., Slavin A.V., Skirta A.A. Investigation of the aging processes of polymer composite materials in natural conditions of the tropical climate of North America. Novosti materialovedeniya. Science and technology, 2018, no. 3–4 (30), art. 8. Available at: http://materialsnews.ru (accessed: July 08, 2022).
  21. Startsev O.V., Lebedev M.P., Kychkin A.K. Aging of polymeric composite materials in conditions of extremely cold climate. Izvestiya Altayskogo gosudarstvennogo universiteta, 2020, no. 1 (111). pp. 41–51. DOI: 10.14258/izvasu(2020)1-06.