Makushina M.A., Kochetkov A.S., Vinogradov I.D. Statistical evaluation of the homogeneity of the chemical composition of vacuum-arc remelting ingots from economic alloy titanium VT40L // Proceedings of VIAM. 2022. No. 11 (117). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-11-27-36.

Statistical evaluation of the homogeneity of the chemical composition of vacuum-arc remelting ingots from economic alloy titanium VT40L

Makushina M.A., Kochetkov A.S., Vinogradov I.D.
Abstract

Presents the results of studies of the uniformity of the distribution of alloying elements in ingots from economically alloyed casting titanium alloy VT40L. Experimental ingots obtained by double vacuum-arc remelting, for which the main technological parameters of melting calculated. Statistical processing of the results of chemical analysis was carried out using Shewhart control charts, and indicators of process capabilities were also evaluated. Suggestions are made about methods for achieving the best stability indicators.

Keywords
titanium, cast alloys, ingot, chemical composition, vacuum-arc melting, quality indicators
Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Putyrskiy S.V., Yakovlev A.L., Nochovnaya N.A., Krokhina V.A. Research of different heat treatment modes influence on properties of semi-finished products and welded joints from titanium alloy ВТ22М. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 3–10. DOI: 10.18577/2071-9140-2019-0-1-3-10.
  3. Krokhina V.A., Putyrskiy S.V., Gribkov M.S. Analysis of structure and mechanical properties of welded joint from titanium alloy VT22M. Aviation materials and technologies, 2022, no. 2 (67), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 16, 2022). DOI: 10.18577/2713-0193-2022-0-2-52-62.
  4. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  5. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  6. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: a reference book. Moscow: VILS; MATI, 2009, 520 p.
  7. Aviation materials: a reference book in 12 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2010, vol. 6: Titanium alloys, 96 p.
  8. Tarasenko E.N., Prokhodtseva L.V., Rudakov A.G. High-strength economically alloyed titanium alloy with increased durability for precision shaped casting. Aviacionnye materialy i tehnologii, 2005, no. 2, pp. 37–42.
  9. Yasinsky K.K., Tarasenko E.N. New high-strength cast titanium alloy VT40L. Aviacionnye materialy i tehnologii, 2007, no. 1, pp. 58–60.
  10. Kochetkov A.S., Nochovnaya N.A., Bokov K.A. Specifics of production process of VT40 titanium alloy castings. Trudy VIAM, 2016, no. 3, paper no. 04. Available at: http://www.viam-works.ru (accessed: September 14, 2022). DOI: 10.18577/2307-6046-2016-0-3-4-4.
  11. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  12. Shiryaev A.A., Nochovnaya N.A. Study of structure and chemical composition of pilot high-alloyed titanium alloy ingots. Trudy VIAM, 2015, paper no. 9, no. 06. Available at: http://www.viam-works.ru (accessed: September 23, 2022). DOI: 10.18577/2307-6046-2015-0-9-6-6.
  13. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  14. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  15. Kochetkov A.S., Panin P.V., Nochovnaya N.A., Makushina M.A. Investigation of the chemical inhomogeneity of ingots of a beta-hardening TiAl-alloy of variable composition. Metallurg, 2020, no. 9, pp. 93–100.
  16. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: September 15, 2022). DOI: 10.18577/2071-9140-2022-0-1-30-40.
  17. Dobatkin V.I., Anoshkin N.F., Andreev A.L., Bochvar G.A., Musatov M.I., Tetyukhin V.V., Chistyakov E.P. Ingots of titanium alloys. Moscow: Metallurgiya, 1966, 287 p.
  18. Sergeev V.V., Galitsky N.V., Kiselev V.P., Kozlov V.M. Titanium metallurgy. Moscow: Metallurgiya, 1971, 320 p.
  19. State Standard R 50779.42–99. Statistical methods. Shewhart control charts. Moscow: Publishing house of standards, 1999, 32 p.
  20. State Standard R 50779.44–2001. Statistical methods. Process capability indicators. Basic methods of calculation. Moscow: Publishing house of standards, 2001, 16 p.