Vlasova O.V., Denisova V.S., Zakalashnyy A.V., Solntsev St.S. Electrical insulating heat-resistant lead-free enamel for the protection of electronic equipment // Proceedings of VIAM. 2022. No. 1 (107). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-1-88-96.

Electrical insulating heat-resistant lead-free enamel for the protection of electronic equipment

Vlasova O.V., Denisova V.S., Zakalashnyy A.V., Solntsev St.S.
Abstract

In present work electrical insulating coatings based on BaO–B2O3–SiO2 glass-forming system for use in electronic circuits on a metal substrate were investigated. The synthesized compositions in terms of chemical resistance belong to the class of stabilized glasses. The tests were showed that the experimental compositions significantly exceed the known coatings in terms of dielectric properties. Positive data on the stability of dielectric properties and on the quality of the defect-free coating layer were obtained.

Keywords
enamel, electrical insulating coating, glass, dielectric properties, electrical resistance, dielectric
Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Abstracts of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technical development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences. 2020, vol. 90, no. 2, pp. 225–228.
  4. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 65, no. 6, pp. 846–855.
  5. Nemilov S.V. Optical materials science. Optical glasses: textbook. St. Petersburg: SPbGU ITMO, 2011, 175 p.
  6. Appen A.A. Glass chemistry. Leningrad: Khimiya, 1974, 352 p.
  7. Denisova V.S., Vlasova O.V., Malinina G.A. Effect of the addition of silicon tetraboride on the thermal stability of reaction cured coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 50–55. DOI: 10.18577 / 2071-9140-2020-0-2-50-55.
  8. Belyachenkov I.O., Schegoleva N.E., Chainikova A.S., Vaganova M.L., Shavnev A.A. The influ-ence of sintering and modifying additives on the sintering process and the properties of silicon nitride ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 70–78. DOI: 10.18577/2071-9140-2020-0-1-70-78.
  9. Barinov D.Ya., Marahovskiy P.S., Maltceva E.Yu., Besprozvanniy E.D., Aliasova E.E. Research of thermal conductivity of printed circuit boards based on aluminum substrate and alumina dielectric. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 43–48. DOI: 10.18577/2071-9140-2019-0-1-43-48.
  10. Loshchinin Yu.V., Budinovskiy S.A., Razmakhov M.G. Heat conductivity of heat-protective coatings ZrO2–Y2O3 alloyed by REM oxides obtained by magnetronny application. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 42–49. DOI: 10.18577/2071-9140-2018-0-3-42-49.
  11. Shilova O.A., Polyakova I.G., Petrova I.V. et al. Synthesis and study of film-forming compositions based on silica sols and dispersed oxides for obtaining glass-ceramic electrical insulating coatings. Fizika i khimiya stekla, 2015, vol. 41, no. 6, pp. 819–829.
  12. Efimova L.N., Ivanov N.V., Shilova O.A. Electrical insulating glass-ceramic coating on a small-section nichrome wire. Collection of materials II scientific-technical. conf. with int. participation "Nanoindustry and technologies of the future" for students, graduate students and young scientists. St. Petersburg, 2014, pp. 74–76.
  13. Structural transformations in glasses at elevated temperatures. Ed. N.A.. Toropova, E.A. Porai-Kosice. Moscow; Leningrad: Nauka, 1965, 514 p.
  14. Shelby J. Structure, properties and technology of glass: trans. from English Moscow: Mir, 2006, 288 p.
  15. Krishnan A.T., Bae S., Fonash S.J. Low temperature microcrystalline silicon thin film resistors on glass substrates. Solid-State Electronics, 2000, vol. 44, no. 7, pp. 1163–1168.
  16. Bao R., Busta C. M., Su X. et al. Microstructures, phases, and properties of low melting BaO–B2O3–ZnO glass films prepared by pulsed laser deposition. Journal of Non-Crystalline Solids, 2013, vol. 371, pp. 28–32.
  17. Technology of enamel and protective coatings: textbook. Ed. L.L. Bragina, A.P. Zubekhin. Kharkov: NTU KhPI; Novocherkassk: YURSTU (NPI), 2003, 484 p.