UDC
543.51; 669.1
DOI
10.18577/2307-6046-2021-0-7-103-111
Article PDF (Russian)
(706.57 KB)
How to cite
Alekseev A.V., Orlov G.V., Petrov P.S. Analysis of cobalt and nickel bases cathodes by X-ray fluorescence spectroscopy // Proceedings of VIAM. 2021. No. 7 (101). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-7-103-111.
Analysis of cobalt and nickel bases cathodes by X-ray fluorescence spectroscopy
Abstract
In this work, Al, Cr, Cu, Fe, Ni, Si and Y were determined in SDP-6 cathodes based on cobalt and SDP-1 and AZh8 nickel-based cathodes by x-ray fluorescence spectroscopy. The calibration dependences are corrected taking into account the superposition of signals from interfering elements on the analytical signal and changes in intensity caused by inter-element influences in the matrix. A standard-free analysis was carried out using the method of fundamental parameters. The correctness of the results obtained was confirmed by a comparative analysis by atomic emission spectroscopy and high-resolution mass spectrometry with a glow discharge.
Keywords
x-ray fluorescence analysis, nickel alloys, cathodes, nickel analysis, cobalt analysis.
Reference list
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
- Budinovskiy S.A., Muboyadzhyan S.A., Kosmin A.A. Ion-plasma coatings for the protection of industrial turbine blades from sulfide-oxide corrosion. Nauka i tekhnika v gazovoy promyshlennosti, 2010, no. 3, pp. 61–68.
- Farafonov D.P., Leshchev N.E., Afanasiev-Khody- kin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- State Standard 13047.10–2014. Nickel. Cobalt. Methods for the determination of copper. Moscow: Standartinform, 2015, pp. 2–4.
- State Standard 13047.8–2014. Nickel. Cobalt. Methods for the determination of silicon. Moscow: Standartinform, 2015, pp. 1–4.
- State Standard 13047.17–2014. Nickel. Cobalt. Methods for the determination of iron. Moscow: Standartinform, 2015, pp. 4–6.
- State Standard 13047.5–2014. Nickel. Cobalt. Methods for the determination of nickel in cobalt. Moscow: Standartinform, 2015, pp. 4–6.
- State Standard 8776–2010. Cobalt. Methods of chemical-atomic-emission spectral analysis. Moscow: Standartinform, 2011, pp. 12–18.
- Blokhin M.A. X-ray spectral research methods. Moscow State Publ. House of Phys.-Math. Literature, 1959, 388 p.
- Handbook of x-ray spectrometry. Ed. R.E. Van Grieken, A.A. Marcowicz. 2nd ed., rev. and expanded. New York: Marcel Dekker, Inc., 2001, pp. 14–56.
- Criss J.W., Birks L.S. Calculation methods for fluorescent X-ray spectrometry. Empirical coefficients vs. fundamental parameters. Analytical Chemistry, 1968, vol. 40, pp. 1080–1086.
- Mashin N.I., Lebedeva R.V., Tumanova A.N. X-ray fluorescence analysis of Ni – Fe – Mn – Cr systems. Analitika i kontrol, 2004, vol. 8, no. 2, pp. 160–164.