Karachevtsev F.N., Eroshkin S.G., Mostyaev I.V., Akinina M.V., Slavin A.V. Development of standard samples of magnesium alloys VML20 and VMD16 // Proceedings of VIAM. 2021. No. 5 (99). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-5-39-47.

Development of standard samples of magnesium alloys VML20 and VMD16

Karachevtsev F.N., Eroshkin S.G., Mostyaev I.V., Akinina M.V., Slavin A.V.
Abstract

A technology for the manufacture and production of reference material (CRM) of the composition of magnesium alloys of the VML20 and VMD16 grades has been developed. In FSUE «VNIIOFI» tests of CRM material were carried out in order to approve their type, as well as metrological examination. Conclusions were drawn up on checking the results of CRM testing for the composition of the indicated alloys and certificates of type approval of reference materials were issued. CRM sets of the approved type of state standard samples of high-strength magnesium alloys of VML20 and VMD16 grades have a relative error of the certified values of the mass fraction of elements in the range from 0.5 to 5% (by weight) no more than 5% rel.

Keywords
standard sample, magnesium alloys, spectroscopy, manufacturing technology, type approval of reference materials, uncertainty.
Reference list
  1. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  2. Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
  3. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dynamics of the development of magnesium and cast aluminum alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  4. Mukhina I.Yu., Uridiya Z.P., Trofimov N.V. Сorrosion-resistant casting magnesium alloys. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 15–23. DOI: 10.18577/2071-9140-2017-0-2-15-23.
  5. Leonov A.A., Trofimov N.V., Duyunova V.A., Uritia Z.P. Trends in the development of cast magnesium alloys with an increased ignition temperature (review). Trudy VIAM, 2021, no. 2 (96), paper no. 01. Available at: http://www.viam-works.ru (accessed: March 19, 2021). DOI: 10.18577/2307-6046-2021-0-2-3-9.
  6. Volkova E.F., Duyunova V.A. Effect of unconventional deformation technology applicable to some commercial magnesium–based alloys. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 17–23. DOI: 10.18577/2071-9140-2016-03-17-23.
  7. Volkova E.F., Mostyaev I.V., Akinina M.V. Comparative analysis of mechanical properties anisotropy and microstructure of semi-finished products from high-strength magnesium alloys with REE. Trudy VIAM, 2018, no. 5 (65), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 9, 2021). DOI: 10.18577/2307-6046-2018-0-5-24-33.
  8. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Assessment of the compliance of new materials using CO and high levels. Kompetentnost, 2017, no. 2. C. 40-46.
  9. Lutsenko A.N., Perov N.S., Chabina E.B. The new stages of development of Testing Center. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
  10. Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of the diagnosis of materials. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
  11. Karpov Yu.A. Analytical control of metallurgical production. Moscow: Metallurgiya, 1995, pp. 97–107.
  12. Otto M. Modern methods of analytical chemistry: at 2 vols. Moscow: Technosfera, 2003, vol. 1, 416 p.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Fariñas J.C., Rucandio I., Pomares-Alfonso M.S. et al. Determination of Rare Earth and Concomitant Elements in Magnesium Alloys by Inductively Coupled Plasma Optical Emission Spectrometry. Talanta, 2016, no. 154, pp. 53–62. DOI: 10.1016/J.Talanta.2016.03.047.
  15. Palekov R.M., Baranovskaya V.B., Karachevtsev F.N., Letov A.F. Determination of rare-earth metals in magnesium alloys by atomic-emission spectrometry with inductively-bound plasma. Izmeritelnaya tekhnika, 2019, no 4, pp. 62–66.