Karachevtsev F.N., Titov V.I. Development of standard samples of the composition of heat-resistant nickel-based alloys for spectral analysis of cathodes used for ion-plasma coatings of GTE working and nozzle blades // Proceedings of VIAM. 2021. No. 5 (99). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-5-14-22.
Development of standard samples of the composition of heat-resistant nickel-based alloys for spectral analysis of cathodes used for ion-plasma coatings of GTE working and nozzle blades
Abstract
In the work, the development of technologies for the manufacture and production of standard samples of heat-resistant nickel-based alloys: SDP-1, SDP-2, VSPD-9, VZhL-2, AZh-8. Developed and certified by MI 1.2.027–2011 «Method of measuring alloying elements by x-ray fluorescence method in heat-resistant alloys» establishes the measurement of the dimensions of alloying elements in heat-resistant nickel-based alloys by x-ray fluorescence method. The registration of the RSA of heat-resistant nickel-based alloys SDP-1, SDP-2, VSPD-9, VZhL-2, AZh-8 in the System of voluntary certification of standard samples of materials and materials.
Keywords
nickel alloys, reference materials, manufacturing technology, measurement technique, x-ray fluorescence method, ion-plasma coatings.
Reference list
- Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
- Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
- Kosmin A.A., Budinovskiy S.A., Muboyadzhyan S.A. Heat and corrosion resistant coating for working turbine blades from promising high-temperature alloy VZhL21. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 17–24. DOI: 10.18577/2071-9140-2017-0-1-17-24.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Competence. Kompetentnost, 2017, no. 2, pp. 40–46.
- Dvoretskov R.M., Petrov PS, Orlov G.V., Karachevtsev F.N., Letov A.F. Standard samples of new grades of heat-resistant nickel alloys and their application for spectral analysis. Zavodskaya laboratoriya. Diagnostika materialov, 2018, vol. 84, no. 11, pp. 15–22.
- Handbook of x-ray spectrometry. Ed. R.E. Van Grieken, A.A. Marcowicz. 2nd ed. New York: Marcel Dekker, 2001, pp. 14–56.
- Criss J.W., Birks L.S. Calculation methods for fluorescent X-ray spectrometry. Empirical coeffi-cients vs. fundamental parameters. Analytical Chemistry, 1968, vol. 40, pp. 1080–1086.
- Mashin N.I., Lebedeva R.V., Tumanova A.N. X-ray fluorescence analysis of systems Ni–Fe–Mn–Cr. Analitika i kontrol, 2004, vol. 8, no. 2, pp. 160–164.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plasma methods of nickel alloys elemental chemical composition analysis. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.
- Dvoretskov R.M., Baranovskaya V.B., Mazalov I.S., Karachevtsev F.N. Application of atomic emission spectrometry with inductively coupled plasma for the analysis of electrolytes during electrolytic extraction of the phases of nickel alloys. Trudy VIAM, 2018, no. 12 (72), paper no. 12. Available at: http://viam-works.ru (accessed: March 17, 2021). DOI: 18577/2307-6046-2018-0-12-107-120.
- Dvoretskov R.M., Volkova O.S., Radzikovskaya V.N., Burova V.N. Determination of beryllium in modern aviation materials by atomic emission spectrometry with inductively coupled plasma. Trudy VIAM, 2016, no. 4, paper no. 5. Available at: http://www.viam-works.ru (accessed: March 17, 2021). DOI: 10.18577/2307-6046-2016-0-4-5-5.
- Chernikova I.I., Tyumneva K.V., Bakaldina T.V., Ermolaeva T.N. Improvement of sample preparation in the analysis of ferroalloys by atomic emission spectrometry with inductively coupled plasma. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 5, pp. 11–17.